Application Status and Research Progress of Doping Modification of W-Cu Composites AITranslate

School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology;School of Materials Science&Engineering,Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

W-Cu composites are widely used in various industrial fields due to their excellent comprehensive properties, including high hardness, wear resistance, ablation resistance, electrical and thermal conductivity, and low thermal expansion coefficient.This paper introduces the latest research progress of W-Cu compo-sites and their current applications in electrical contacts, microelectronics, military use, and functionally graded materials.In addtion, the paper emphatically summarizes and analyzes the classification and principles of doping modification for W-Cu composites, as well as the influence of doping modification on material properties.Finally, the potential problems and research directions of W-Cu composites in the future are put forward.

KeyWords AITranslate

W-Cu composite doping modification miscibility of W and Cu application status property

1宋鹏,李达,弓艳飞,熊宁,韩蕊蕊,姚惠龙.镀镍厚度对钨铜封装材料气密性及耐腐蚀性的影响[J].中国钨业,2023,38(3):80-86.

2郭凌翔,唐颖,黄世伟,肖博澜,夏东浩,孙佳.C/C复合材料高熵氧化物涂层抗烧蚀性能[J].无机材料学报,2024,39(1):61-70.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.11[金属学及工艺—金属材料]

Citation Information:

W-Cu composites are widely used in various industrial fields due to their excellent comprehensive properties, including high hardness, wear resistance, ablation resistance, electrical and thermal conductivity, and low thermal expansion coefficient.This paper introduces the latest research progress of W-Cu compo-sites and their current applications in electrical contacts, microelectronics, military use, and functionally graded materials.In addtion, the paper emphatically summarizes and analyzes the classification and principles of doping modification for W-Cu composites, as well as the influence of doping modification on material properties.Finally, the potential problems and research directions of W-Cu composites in the future are put forward.

quote

GB/T 7714-2015 [1] LOU Wen-peng, LI Xiu-qing, WEI Shi-zhong, et al. Application Status and Research Progress of Doping Modification of W-Cu Composites[J]. Rare Metals and Cemented Carbides, 2024(1): 6-16.
MLA [1] LOU Wen-peng, et al., "Application Status and Research Progress of Doping Modification of W-Cu Composites." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 6-16.
APA [1] LOU Wen-peng, LI Xiu-qing, WEI Shi-zhong, WAN GQi, LIANG Jing-kun, CHEN Liang-dong, & XU Liu-jie. (2024). Application Status and Research Progress of Doping Modification of W-Cu Composites. Rare Metals and Cemented Carbides(1), 6-16.
IEEE [1] LOU Wen-peng, LI Xiu-qing, WEI Shi-zhong, WAN GQi, LIANG Jing-kun, CHEN Liang-dong, and XU Liu-jie, "Application Status and Research Progress of Doping Modification of W-Cu Composites," Rare Metals and Cemented Carbides, no. 1, pp. 6-16, 2024. keywords: {W-Cu composite;doping modification;miscibility of W and Cu;application status;property}