The W-6Ni-4Co-2X alloys(X=Nb,Ta,Hf,Mo and Ti)were prepared by powder metallurgy technology,and the effects of adding Nb,Ta,Hf,Mo,and Ti elements on the microstructure and mechanical properties of W-6Ni-4Co alloy were investigated.The results show that the microstructure of the W-6Ni-4Co-2X alloys mainly includes base phase(W phase)and binder phase,and the type and content of the binder phase are related to the precipitation of dissolved W phase in the binder phase(Ni,Co)during sintering.The W grains of W-6Ni-4Co-2Ta alloy and W-6Ni-4Co-2Hf alloy are in the form of irregular polygon,while the W grains of W-6Ni-4Co-2Nb alloy and W-6Ni-4Co-2Ti alloy are ellipsoidal and dispersedly distributed in the binder phase.The uniform microstructure,finer grains,and good interfacial bonding of the W/binder phase in W-6Ni-4Co-2Ta alloy contribute to its superior hardness,bending strength,and yield strength.In W-6Ni-4Co-2Mo alloy,W grains are arranged in network structure,and the continuous W ske-leton structure,in synergy with the ductile binder phase,reduces the strain hardening of the alloy,contributing to its excellent strain hardening resistance.Therefore,adding suitable transition metal elements to W-6Ni-4Co alloy provides an effective way for improving its mechanical properties.
KeyWords AITranslate
1毕广利,满宏生,姜静,李元东,蒋春宏,陈体军.挤压Mg-Y-Ni-Co合金的显微组织和力学性能[J].中国有色金属学报,2023,33(4):1011-1023.
2Wei Fan,Yan Zhuge,Xing Ma,Christopher W.K.Chow,Yue Liu,Guangtong Huang,Nima Gorjian.Effects of carbonation on mechanical properties of CAC‑GGBFS blended strain hardening cementitious composites[J].Low-carbon Materials and Green Construction,2023,1(1):3-20.
3范凯,葛宁,赵和明.材料应变硬化性能对隔膜锥段翻转行为的影响研究[J].载人航天,2023,29(4):434-441.
4吕邦成,郭丽萍,丁聪,吴建东,曹园章,陈波.高延性地质聚合物复合材料性能及微结构研究进展[J].材料导报,2023,37(10):226-236.
5朱利敏,李全安,陈晓亚,张清.Mg-8Gd-(0,3)Sm-0.5Zr合金的动态再结晶生长动力学[J].材料热处理学报,2024,45(1):166-174.
6章政文,顾津锦,赵俊华,黄建伟,吴海峰,文福拴.基于碳卫星与电力排放数据的碳计量[J].电力系统自动化,2024,48(1):2-9.
7常雪婷,宋嘉琪,王冰,王东胜,陈文聪,王海丰.微合金化对高锰奥氏体钢在酸性盐雾环境下的耐蚀性能影响研究[J].中国腐蚀与防护学报,2024,44(1):47-58.
8段方俊,肖绪培,余明娟,姚静.国家级传统村落空间分异及影响因素研究——以河南省为例[J].安徽农业科学,2024,52(4):184-188.
9邱玉新,张爱军,辛本斌,孟军虎,吴有智.Al_(0.2)Co_(1.5)CrNi_(1.5)Ti_(0.5)Mox高温耐磨高熵合金的组织结构、力学性能和摩擦学性能[J].摩擦学学报,2023,43(12):1381-1392.
10李文东,李进,陈亮.国产核电用大直径P91无缝钢管的研发[J].中国核电,2023,16(4):544-550.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]
Citation Information:
The W-6Ni-4Co-2X alloys(X=Nb,Ta,Hf,Mo and Ti)were prepared by powder metallurgy technology,and the effects of adding Nb,Ta,Hf,Mo,and Ti elements on the microstructure and mechanical properties of W-6Ni-4Co alloy were investigated.The results show that the microstructure of the W-6Ni-4Co-2X alloys mainly includes base phase(W phase)and binder phase,and the type and content of the binder phase are related to the precipitation of dissolved W phase in the binder phase(Ni,Co)during sintering.The W grains of W-6Ni-4Co-2Ta alloy and W-6Ni-4Co-2Hf alloy are in the form of irregular polygon,while the W grains of W-6Ni-4Co-2Nb alloy and W-6Ni-4Co-2Ti alloy are ellipsoidal and dispersedly distributed in the binder phase.The uniform microstructure,finer grains,and good interfacial bonding of the W/binder phase in W-6Ni-4Co-2Ta alloy contribute to its superior hardness,bending strength,and yield strength.In W-6Ni-4Co-2Mo alloy,W grains are arranged in network structure,and the continuous W ske-leton structure,in synergy with the ductile binder phase,reduces the strain hardening of the alloy,contributing to its excellent strain hardening resistance.Therefore,adding suitable transition metal elements to W-6Ni-4Co alloy provides an effective way for improving its mechanical properties.
quote
| GB/T 7714-2015 | [1] HU Xiao-nan, DONG Hong-feng, LI Pei-you. Effect of Element Addition on the Microstructure and Mechanical Properties of Two-Step Sintered W-6Ni-4Co Alloy[J]. Rare Metals and Cemented Carbides, 2024(1): 17-23. |
| MLA | [1] HU Xiao-nan, et al., "Effect of Element Addition on the Microstructure and Mechanical Properties of Two-Step Sintered W-6Ni-4Co Alloy." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 17-23. |
| APA | [1] HU Xiao-nan, DONG Hong-feng, & LI Pei-you. (2024). Effect of Element Addition on the Microstructure and Mechanical Properties of Two-Step Sintered W-6Ni-4Co Alloy. Rare Metals and Cemented Carbides(1), 17-23. |
| IEEE | [1] HU Xiao-nan, DONG Hong-feng, and LI Pei-you, "Effect of Element Addition on the Microstructure and Mechanical Properties of Two-Step Sintered W-6Ni-4Co Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 17-23, 2024. keywords: {W-Ni-Co alloy;metal element addition;two-step sintering;microstructure;mechanical property} |