Abstract AITranslate

This paper aims to design bio-based polyester as a viscosity modifier for lubricant properties. Bio-based polyricinoleate (PRic) and its saturated homologous polyhydroxystearate (PHS) have been synthesized from fatty acid methyl esters. The polycondensation performed in bulk in a one-step reaction without any purification leads to two series of polyesters within a large range of molecular weights, with Mw between 3 and 130 kg·mol–1. Their thermal properties were investigated. Good thermal stability was observed with degradation temperatures above 300 °C. As expected, PRic appeared to be amorphous with a particularly low glass-transition temperature, while PHS is semicrystalline. A rheological study determined that polyricinoleate entangled when its molecular weight was above 25 kg·mol–1. These two bio-based and biodegradable polymers were then evaluated as viscosity modifiers in both organic and mineral oils. PHS with high molecular weights appeared to be an excellent thickener as well as a good viscosity index improver with a viscosity index (VI) increase above +50 in organic lubricant oil and +64 in mineral oil.

KeyWords AITranslate

polyricinoleate polyhydroxystearate lubricant viscosity modifiers thickeners viscosity index
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01153

Chinese Library Classification Number:

Citation Information:

This paper aims to design bio-based polyester as a viscosity modifier for lubricant properties. Bio-based polyricinoleate (PRic) and its saturated homologous polyhydroxystearate (PHS) have been synthesized from fatty acid methyl esters. The polycondensation performed in bulk in a one-step reaction without any purification leads to two series of polyesters within a large range of molecular weights, with Mw between 3 and 130 kg·mol–1. Their thermal properties were investigated. Good thermal stability was observed with degradation temperatures above 300 °C. As expected, PRic appeared to be amorphous with a particularly low glass-transition temperature, while PHS is semicrystalline. A rheological study determined that polyricinoleate entangled when its molecular weight was above 25 kg·mol–1. These two bio-based and biodegradable polymers were then evaluated as viscosity modifiers in both organic and mineral oils. PHS with high molecular weights appeared to be an excellent thickener as well as a good viscosity index improver with a viscosity index (VI) increase above +50 in organic lubricant oil and +64 in mineral oil.

quote

GB/T 7714-2015 [1] Hélène Méheust, JeanFrançois Le Meins, Etienne Grau, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01153.
MLA [1] Hélène Méheust, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01153.
APA [1] Hélène Méheust, JeanFrançois Le Meins, Etienne Grau, & Henri Cramail. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01153
IEEE [1] Hélène Méheust, JeanFrançois Le Meins, Etienne Grau, and Henri Cramail, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01153. keywords: {polyricinoleate;polyhydroxystearate;lubricant;viscosity modifiers;thickeners;viscosity index}