Abstract AITranslate

The choice of materials used in the chip fabrication is crucial in microfluidics. They are selected and adapted depending on the available production techniques and associated processes, the involved characterization and measurement methods, the physical and chemical experimental conditions, and the cost. Here, we propose a versatile approach using a combination of epoxy materials to fabricate manually resealable and reusable (>40 times) microfluidic chips which demonstrate numerous potentialities: good chemical resistance, optical (visible and X-ray) transparency, biocompatibility, capability to undergo in average 2.9 bar of liquid pressure, or integration of high aspect ratio (>1500) channels. It thus represents a promising alternative for prototyping in a large panel of applications and fundamental studies.

KeyWords AITranslate

epoxy microfluidics microfluidic chips microfabrication reversible sealing prototyping
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01112

Chinese Library Classification Number:

Citation Information:

The choice of materials used in the chip fabrication is crucial in microfluidics. They are selected and adapted depending on the available production techniques and associated processes, the involved characterization and measurement methods, the physical and chemical experimental conditions, and the cost. Here, we propose a versatile approach using a combination of epoxy materials to fabricate manually resealable and reusable (>40 times) microfluidic chips which demonstrate numerous potentialities: good chemical resistance, optical (visible and X-ray) transparency, biocompatibility, capability to undergo in average 2.9 bar of liquid pressure, or integration of high aspect ratio (>1500) channels. It thus represents a promising alternative for prototyping in a large panel of applications and fundamental studies.

quote

GB/T 7714-2015 [1] Simon Raffy, Etienne Palleau, Brice Calvignac, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01112.
MLA [1] Simon Raffy, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01112.
APA [1] Simon Raffy, Etienne Palleau, Brice Calvignac, Guillaume Brotons, Guillaume Lefebvre, Nicolas Rolley, Sébastien Teychene, Bernard Viguier, Sara Castaño Cerezo, Gilles Truan, & Laurence Ressier. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01112
IEEE [1] Simon Raffy, Etienne Palleau, Brice Calvignac, Guillaume Brotons, Guillaume Lefebvre, Nicolas Rolley, Sébastien Teychene, Bernard Viguier, Sara Castaño Cerezo, Gilles Truan, and Laurence Ressier, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01112. keywords: {epoxy;microfluidics;microfluidic chips;microfabrication;reversible sealing;prototyping}