The Latest Development of Zone Melting Technology AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The basic principles of zone melting technology are explained, its latest development and applica- tion are reviewed focusing on the progress of its critical process steps. Description is made of the current applications of zone melting in high-pure materials like semiconductors, refractory metals and rare earth el- ements. Current limitation and future development direction of zone melting technology are also analyzed and pointed out.

KeyWords AITranslate

zone melting high-pure material technical principle technological progress current application

1吕毓松,周勇坤,刘佐权.用剩余电阻率比评定高纯锡的纯度[J].云南大学学报:自然科学版,1996,18(3):261-266. 被引量:1

2Minoru, Isshiki, Minoru, etal. Preparation of high pu- rity metals for advanced devices[J]. Thin Solid Films, 2011, 519(24): 8 451-8 455.

3Pfann W G. Principles of zone melting[J]. AIME Tra- nsactions, 1952, 194: 747-754.

4李玉春.区域熔炼制备高纯金属的理论及过程分析[EB/OL].http://www.paper.edu.cn,2005-06-09.

5吴洪.区域熔炼的理论分析及实际应用[J].佳木斯工学院学报,1995,13(1):14-17. 被引量:4

6Reiss Howard. Mathematical methods for zone-melting processes[J]. AIME Transactions, 1964, 200: 1 053- 1 059.

7Lord N W. Analysis of molten-zone refining[J]. AIME Transactions, 1953, 197:1 531-1 533.

8石洁,罗超,王怀胜,刘勇,李鱼飞.感应区域熔炼法制备高纯铜[J].稀有金属材料与工程,2010,39(A01):418-421. 被引量:6

9翟秀静,符岩,张晓明,孙中祺,范立志.原铝中Fe、Si杂质分配系数的计算与测定[J].轻金属,2000(12):37-39. 被引量:3

10Cheung No e, Bertazzoli Rodnei, Garcia Amauri. Nu merieal and experimental analysis of an approach based on variable solute distribution coefficients during purifi- cation by zone refining[J]. Separation and Purification Technology, 2007, 52(3): 504-511.

1田丽森,尹延西,胡志方,李忠岐,王力军.高纯金属铪制备技术研究进展[J].矿冶,2014,23(2):49-54. 被引量:11

2杜怡霖,张昆华,管伟明,李艳,刘洪江.过渡金属硼化物的实验研究现状与趋势[J].贵金属,2014,35(2):82-88. 被引量:2

3高文龙,张建刚,曹旭.金属钠提纯研究进展[J].广州化工,2014,42(14):13-14. 被引量:2

4吴钢,戎舟.小型有机固体熔炼装置运动控制系统设计[J].计算机技术与发展,2014,24(9):176-178.

5李沐春,刘斯琦,屈华,刘海平,刘伟东.真空区域熔炼炉的设计及碲提纯研究[J].金属材料研究,2014,40(3):6-9.

6姜民浩,宋建勋,张龙,刘勇,焦树强.CaCl_2–TiCl_2熔盐体系中制备高纯钛[J].电镀与涂饰,2014,33(23):1008-1011. 被引量:1

7刘斯琦,屈华,刘海平,李沐春,高闻远,刘伟东.稀散金属材料Te的区域熔炼提纯[J].特种铸造及有色合金,2014,0(12):1253-1255.

8田晓根,张亚莉,李少英,黄志鹏,王茹.传热过程中固体形状对温度分布的影响分析[J].稀有金属,2017,41(4):377-383. 被引量:3

9夏兴莉,李琦,魏远隆,张维冰.低温富集液液萃取分析苦瓜挥发性成分[J].生命科学仪器,2018,16(3):60-65. 被引量:3

10何几文,刘欢,胡智东,张福元,华中胜.铜阳极泥中碲的回收研究进展[J].稀有金属与硬质合金,2018,46(4):20-28. 被引量:11

1贾雷,严红燕,李慧,刘畅,张帅.金属铪的制备和精炼[J].热加工工艺,2020,0(1):10-15. 被引量:1

2董雪平,郭树军,徐欣.锆铪萃取分离机理的研究进展[J].广州化工,2015,43(23):42-44. 被引量:3

3邵建达,戴亚平,许乔.惯性约束聚变激光驱动装置用光学元器件的研究进展[J].光学精密工程,2016,24(12):2889-2895. 被引量:17

4谢珊珊,李慧,梁精龙,霍东兴.金属铪的制备工艺[J].热加工工艺,2017,46(6):36-38. 被引量:5

5郭咏,李世长.硼化铑晶格动力学性质的第一性原理计算[J].山西师范大学学报:自然科学版,2017,31(4):29-32.

6赵飞,李娟.惰气熔融-红外法测定铪中氢含量[J].有色金属科学与工程,2017,8(6):117-120. 被引量:1

7邹灿辉,龙莹,郑鑫,张锦阳,林华泰.三元过渡金属硼化物Os_(1-x)Ru_xB_2的制备及其结构和性能研究[J].无机材料学报,2018,33(7):787-792. 被引量:1

8宁瑞,余珊,房孟钊,李伟,李飞燕.提高分金工序中碲浸出率的试验研究[J].湖南有色金属,2019,35(2):39-41. 被引量:2

9曲世联,陈婉琦,黄正兴,刘翔,刘伟.He注入对W在瞬态热负荷条件下熔化行为的影响[J].稀有金属,2019,43(3):290-295. 被引量:2

10邓孝纯,李慧,张汉鑫,张立生.铪的应用及金属铪的制备工艺[J].稀有金属与硬质合金,2019,47(3):62-65. 被引量:3

1秦丽娟,赵景富,孙镇,郑鹏.镍红土矿RKEF法工艺进展[J].有色矿冶,2012,28(2):34-36. 被引量:14

2李尚隆,姜朋忠.金属镁生产工艺进展[J].化工管理,2016(23). 被引量:2

3及亚娜,孙体昌,蒋曼.红土镍矿提镍工艺进展[J].矿产保护与利用,2011,31(2):43-49. 被引量:27

4韩继龙,孙庆国.金属镁生产工艺进展[J].盐湖研究,2008,16(4):59-65. 被引量:23

5高玉来.不锈钢冶炼工艺进展及LF优化应用[J].商品与质量:学术观察,2012(5):66-66.

6张长理.电解法再生废硬质合金工艺进展[J].有色金属:冶炼部分,1990(2):40-42. 被引量:1

7陈隆玉.生物湿法冶金工艺进展[J].铀矿冶,2008,27(4):177-177.

8杨玮娇,马保中.红土镍矿加压酸浸工艺进展[J].矿冶,2011,20(3):61-67. 被引量:17

9汪珂,马慧娟.原苏联钛氯化冶金工艺进展[J].钒钛,1992(6):49-53. 被引量:1

10邹序枚.粗晶碳化钨粉生产工艺进展及其工艺原理探讨[J].硬质合金,1995,12(1):23-29. 被引量:14

Basic Information:

DOI:

Chinese Library Classification Number:TF114.31[冶金工程—冶金物理化学]

Citation Information:

The basic principles of zone melting technology are explained, its latest development and applica- tion are reviewed focusing on the progress of its critical process steps. Description is made of the current applications of zone melting in high-pure materials like semiconductors, refractory metals and rare earth el- ements. Current limitation and future development direction of zone melting technology are also analyzed and pointed out.

quote

GB/T 7714-2015 [1] LIU Wen-sheng, LIU Shu-hua, MA Yun-zhu, et al. The Latest Development of Zone Melting Technology[J]. Rare Metals and Cemented Carbides, 2013(1): 66-71.
MLA [1] LIU Wen-sheng, et al., "The Latest Development of Zone Melting Technology." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 66-71.
APA [1] LIU Wen-sheng, LIU Shu-hua, MA Yun-zhu, & LONG Lu-ping. (2013). The Latest Development of Zone Melting Technology. Rare Metals and Cemented Carbides(1), 66-71.
IEEE [1] LIU Wen-sheng, LIU Shu-hua, MA Yun-zhu, and LONG Lu-ping, "The Latest Development of Zone Melting Technology," Rare Metals and Cemented Carbides, no. 1, pp. 66-71, 2013. keywords: {zone melting;high-pure material;technical principle;technological progress;current application}