Development of Noncarbonaceous Anode Material of Li-ion Secondary Battery AITranslate

Institute of Chemistry and Chemical Engineering, Anqing Teachers College;Institute of Chemistry and Chemical Engineering, Anqing Teachers College;Institute of Chemistry and Chemical Engineering, Anqing Teachers College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Four main types of anode material of modern Li-ion secondary battery-Li-containing transition metal nitride, tin oxide, transition metal oxide and V-based composite oxide are reviewed. And their intercalation and de-intercalation mechanism,performance characteristic and latest development are systematically introduced.

KeyWords AITranslate

Li-ion secondary battery noncarbonaceous anode material intercalation and de-intercalation mechanism intermetallic compound

1Shodai T,Sakurai Y,Suzuk T.Electrochemical study of Li4Ti5O12 as negative electrode for Li-ion polymer rechargeable batteries[J].Solid State Ionics,2005,128(3):85-88.

2Takeda Y,Yang J.Electrochemical impedance spectroscopy study of SnO and nano-SnO anodes in lithium rechargeable batteries[J].J Power Sources,2001,97-98(2):244-249.

3Yang J,Takeda Y,Imanishi N,et al.Dispersion of Sn and SnO on carbon anodes[J].Electrochim Acta,2007,52(6):2 659-2 663.

4Li N,Martin C.Electrochemical characterization of tin based composite oxides as negative electrodes for lithium batteries[J].J Electrochem Soc,2001,148(3):164-168.

5Mohamedi M,Lee S,Takahashi D,et al.Amorphous tin oxide films:preparation and characterization as anode active material for lithium ion batteries[J].Electrochim Acta,2005,20(4):1 161-1 165.

6Courtney I A,McKinnon W R,Dahn J R.Key factors controlling the reversibility of the reaction of lithium with SnO2 and Sn2BP6 glass[J].J Electrochem Soc,2004,151(1):59-65.

7Gejke C,Zanghellini E,Fransson L,et al.Use of amorphous tin-oxide films obtained by spray pyrolysis as electrode in lithium batteries[J].J Power Sources,2001,97-98(2):226-229.

8Courtney I A,Dahn J R.Electrochemical and in site X-ray diffraction studies of the reaction of lithium with tin oxide composites[J].J Electrochem Soc,2007,154(6):2 045-2 049.

9Brousse T,Retoux R.Thin-film crystalline SnO2-lithium electrodes[J].J Electrochem Soc,2008,155(1):1-6.

10Liu W,Huang X,Wang Z,et al.Synthesis and characterization of amorphous nanosized MnSnO3as a high capacity anode material for lithium ion battery[J].J Electrochem Soc.2008,155(1):59-63.

1张加艳,沈建兴,魏长宝.锂离子电池负极材料研究进展[J].山东陶瓷,2015,38(1):7-10. 被引量:3

1李涛,罗驹华,颜祝,申盼.NiFe2O4-石墨烯纳米复合材料的制备及其电化学性能[J].合成材料老化与应用,2016,0(4):46-53.

2林信勇,李求忠.锂离子电池Ni包裹Sn负极材料的制备和性能研究[J].宁德师范学院学报:自然科学版,2018,30(1):54-58. 被引量:1

3黄启高,欧阳海波,刘长青,张晨鸽.MOF衍生钴氧化物材料的制备及其电化学性能[J].陕西科技大学学报,2020,38(5):126-131.

1殷金玲,陈猛,李胜军.锂离子电池非碳负极材料的研究进展[J].应用科技,2002,29(10):52-55. 被引量:4

2邓敏超.锂离子电池负极材料研究进展[J].娄底师专学报,2003(2):26-28. 被引量:4

3颜剑,苏玉长,苏继桃,卢普涛.锂离子电池负极材料的研究进展[J].电池工业,2006,11(4):277-281. 被引量:13

4吴宇平,万春荣,姜长印,李建军,李阳兴.锂离子二次电池锡的氧化物负极材料的研究[J].化学通报,1998(10):24-26. 被引量:12

5杜远东,任尚坤,马兴科.锂离子二次电池负极材料及电解质研究[J].周口师范高等专科学校学报,2002,19(2):27-31. 被引量:1

6孙兴川,崔朝军,张妩娜.钒基电极材料的研究进展[J].科技视界,2015(32):183-183.

7颜剑,苏玉长,卢普涛,苏继桃.Li^+嵌Al反应的热力学分析及实验研究[J].电池,2006,36(2):135-136.

8陈汝文,涂新满,陈德志.过渡金属氮化物在锂离子电池中的应用[J].化学进展,2015,27(4):416-423. 被引量:5

9王波.含新能源的电力系统经济调度探讨[J].低碳世界,2015,0(27):68-69.

10贾旭平.美国PNNL开发出新型低成本液流电池[J].电源技术,2016,40(1):6-7.

Basic Information:

DOI:

Chinese Library Classification Number:TM911[电气工程—电力电子与电力传动]

Citation Information:

Four main types of anode material of modern Li-ion secondary battery-Li-containing transition metal nitride, tin oxide, transition metal oxide and V-based composite oxide are reviewed. And their intercalation and de-intercalation mechanism,performance characteristic and latest development are systematically introduced.

quote

GB/T 7714-2015 [1] LIU Tao, DU Rong-bin, KONG Xue-jun. Development of Noncarbonaceous Anode Material of Li-ion Secondary Battery[J]. Rare Metals and Cemented Carbides, 2009(3): 59-64.
MLA [1] LIU Tao, et al., "Development of Noncarbonaceous Anode Material of Li-ion Secondary Battery." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 59-64.
APA [1] LIU Tao, DU Rong-bin, & KONG Xue-jun. (2009). Development of Noncarbonaceous Anode Material of Li-ion Secondary Battery. Rare Metals and Cemented Carbides(3), 59-64.
IEEE [1] LIU Tao, DU Rong-bin, and KONG Xue-jun, "Development of Noncarbonaceous Anode Material of Li-ion Secondary Battery," Rare Metals and Cemented Carbides, no. 3, pp. 59-64, 2009. keywords: {Li-ion secondary battery;noncarbonaceous anode material;intercalation and de-intercalation mechanism;intermetallic compound}