The Latest Development of One-dimensional SiC Nanoscale Materials AITranslate

School of Materials Science and Engineering, Anhui University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of one-dimensional SiC nanoscale materials, such as SiC nanorods, nanowires, nanotubes and nanobelts,is reviewed. The important research directions of these one-dimension- al SiC nanoscale materials are also indicated.

KeyWords AITranslate

SiC nanorod nanowire nanotube the latest development

1Yang T H,Chen C H,Chatterjee A,et al.Controlled growth of silicon carbide nanorods by rapid thermal process and their field emission properties[J].Chem Phys Lett,2003,379(1-2):155-161.

2吴艳军,蔡炳初,张亚非,吴建生.碳化硅纳米晶须的制备研究进展[J].电子元件与材料,2003,22(9):41-44. 被引量:3

3Dai H J,Wong E W,Lu Y Z,et al.Synthesis and characterization of carbide nanorods[J].Nature,1995,375(6 534):769-771.

4Mo Y H,Shajahan M D,Lee Y S,et al.Structural transformation of carbon nanotubes to silicon carbide nanorods or microcrystals by the reaction with different silicon sources in rf induced CVD reactor[J].Synthetic Metals,2004,140(2-3):309-315.

5吴旭峰,凌一鸣.电弧放电制备碳化硅纳米棒[J].硅酸盐学报,2006,34(10):1283-1286. 被引量:5

6Meng G W,Zhang L D,Mo C M,et al.Preparation of β-SiC nanorods with and without amorphous SiO2wrapping layers[J].J Mater Res,1998,13(9):2 533-2 537.

7Zhou X T,Lai H L,Peng H Y,et al.Thin β-SiC nanorods and their field emission properties[J].Chem Phys Lett,2000,318(1-3):58-62.

8Yang W Y,Miao H Z,Xie Z P,et al.Synthesis of silicon carbide nanorods by catalyst-assisted pyrolysis of polymeric precursor[J].Chem Phys Lett,2004,383(5-6):441-444.

9徐武军,徐耀,孙先勇,刘亚琴,吴东,孙予罕.溶胶-凝胶和碳热还原法制备塔状SiC纳米棒[J].新型炭材料,2006,21(2):167-170. 被引量:8

10Sharma N K,Williams W S,Zangvil A.Formation and structure of silicon carbide whiskers[J].J Am Ceram Soc,1984,67(11):715-720.

1齐晓霞,许并社,翟光美,梁建,马淑芳.Ag作催化剂制备的SiC纳米材料的形貌及其发光性能[J].材料热处理学报,2016,37(7):1-5. 被引量:1

2张树霖.一维纳米材料的拉曼光谱学研究[J].光散射学报,2000,12(2):63-65.

3阎研,黄福敏,张树霖,朱邦芬,尚尔轶,范守善.随激发波长改变的SiC纳米棒的Raman光谱[J].科学通报,2001,46(15):1256-1257.

4徐武军,徐耀,孙先勇,刘亚琴,吴东,孙予罕.溶胶-凝胶和碳热还原法制备塔状SiC纳米棒[J].新型炭材料,2006,21(2):167-170. 被引量:8

5吴旭峰,凌一鸣.电弧放电制备碳化硅纳米棒[J].硅酸盐学报,2006,34(10):1283-1286. 被引量:5

6张爱霞,蔡克峰.一维碳化硅纳米材料的研究进展[J].材料导报,2006,20(F05):106-108. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]

Citation Information:

The latest development of one-dimensional SiC nanoscale materials, such as SiC nanorods, nanowires, nanotubes and nanobelts,is reviewed. The important research directions of these one-dimension- al SiC nanoscale materials are also indicated.

quote

GB/T 7714-2015 [1] PEI Li-zhai. The Latest Development of One-dimensional SiC Nanoscale Materials[J]. Rare Metals and Cemented Carbides, 2009(3): 52-58.
MLA [1] PEI Li-zhai. "The Latest Development of One-dimensional SiC Nanoscale Materials." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 52-58.
APA [1] PEI Li-zhai. (2009). The Latest Development of One-dimensional SiC Nanoscale Materials. Rare Metals and Cemented Carbides(3), 52-58.
IEEE [1] PEI Li-zhai, "The Latest Development of One-dimensional SiC Nanoscale Materials," Rare Metals and Cemented Carbides, no. 3, pp. 52-58, 2009. keywords: {SiC;nanorod;nanowire;nanotube;the latest development}