daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Dissolution Characteristics of Sc2O3 in ScF3-LiF Molten Salt AITranslate

School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The liquidus temperature of ScF3-LiF molten salt was measured by step cooling curve method.The solubility of Sc2O3in ScF3-LiF molten salt was measured by the isothermal saturation method,and the effects of temperature and ScF3content were studied.The dissolution mechanism of Sc2O3in ScF3-LiF molten salt was analyzed by X-ray diffraction.The results show that the liquidus temperature of ScF3-LiF molten salt rises with the increase of ScF3content,while it decreases with the addition of Sc2O3.The dissolution of Sc2O3in ScF3-LiF molten salt is mainly chemical dissolution,the dissolution equilibrium time is about 2 h,and its solubility increases with the increase of temperature and ScF3content.

KeyWords AITranslate

Sc2O3 ScF3-LiF molten salt electrolysis liquidus temperature solubility

1王新宇,潘青林,周昌荣,梁文杰,尹志民.含钪铝锂合金的研究与发展[J].稀土,2005,26(6):70-75. 被引量:11

2刘翘楚,薛济来,朱骏.钾冰晶石—氧化钪体系中铝热还原反应过程的研究[J].有色金属:冶炼部分,2013(3):24-27. 被引量:7

3李广宇,杨少华,李继东,胡宪伟,王兆文,张明杰,邱竹贤.熔盐电解法制备铝钪合金的研究[J].轻金属,2007(5):54-57. 被引量:8

4孙本良,翟玉春,田彦文.氟盐体系中电解制取铝钪合金的研究[J].稀有金属,1998,22(3):191-194. 被引量:23

5路贵民,刘学山.氧化钪在nNaF·AlF_3ScF_3熔盐体系中的溶解[J].中国有色金属学报,1999,9(3):624-626. 被引量:24

6张立生,李慧,张汉鑫,梁精龙.NaCl-KCl-NaF-Fe3O4熔盐体系初晶温度的研究[J].有色金属:冶炼部分,2018,0(6):13-15. 被引量:1

7胡宪伟,王兆文,高炳亮,石忠宁,刘凤国,包莫日根高娃.Identification of structural entities in NdF_3-LiF melts with cryoscopic method[J].中国有色金属学报:英文版,2010,20(12):2387-2391. 被引量:2

8Xiaoping Zhu,Shuchen Sun,Chuan Liu,Ganfeng Tu.Solubility of RE_2O_3(RE=La and Nd) in light rare earth fluoride molten salts[J].稀土学报:英文版,2018,36(7):765-771. 被引量:5

1编辑部.“碳”“炭”二词的用法[J].柳钢科技,2022(4):52-54.

2杨亦林.聚乳酸纤维的性能及鉴别特征浅析[J].中文科技期刊数据库(全文版)工程技术,2020(10):0143-0144.

3熊祖江.聚己二酸对苯二甲酸丁二酯泡沫泡孔结构和性能研究[J].中国皮革,2023,52(1):98-104.

4肖力光,朱晨阳.纳米碳酸钙改性三元无机水合盐相变材料的研究[J].化工新型材料,2022,50(12):117-120. 被引量:1

5钟振亚,林如山,洪业,张磊,陈永利,唐洪彬,叶国安.金属乏燃料干法后处理熔盐电解槽电场分析[J].原子能科学技术,2023,57(3):457-468.

6何坚,王帅星,王春霞,田继红,康佳,杜楠.铝合金在HEDP电解液中的阳极氧化行为及膜层结构[J].中国有色金属学报,2023,33(1):180-190.

7史月欣,陈留勤,杜丁丁,柴乐,王子涵.丹霞山陡坡上风化洞穴的基本特征及成因探讨[J].热带地理,2023,43(1):103-114.

8蒋达华,杨昊天,刘景滔,徐玉珍.正癸酸/十八醇二元相变材料的热性能研究[J].中国材料进展,2023,42(2):168-173.

9张万鑫,孙志高.TDA-HDA/膨胀石墨复合相变材料的制备及性能研究[J].功能材料,2023,54(3):3106-3112.

10施斌卿,聂宝华,陈东初.物理化学相图实验教学中FactSage热力学计算软件的应用[J].广东化工,2022,49(24):255-259.

Basic Information:

DOI:

Chinese Library Classification Number:O645.4[理学—物理化学]

Citation Information:

The liquidus temperature of ScF3-LiF molten salt was measured by step cooling curve method.The solubility of Sc2O3in ScF3-LiF molten salt was measured by the isothermal saturation method,and the effects of temperature and ScF3content were studied.The dissolution mechanism of Sc2O3in ScF3-LiF molten salt was analyzed by X-ray diffraction.The results show that the liquidus temperature of ScF3-LiF molten salt rises with the increase of ScF3content,while it decreases with the addition of Sc2O3.The dissolution of Sc2O3in ScF3-LiF molten salt is mainly chemical dissolution,the dissolution equilibrium time is about 2 h,and its solubility increases with the increase of temperature and ScF3content.

quote

GB/T 7714-2015 [1] ZHAO Hang, CHEN Jian-she, WANG Chun-xin, et al. Dissolution Characteristics of Sc2O3 in ScF3-LiF Molten Salt[J]. Rare Metals and Cemented Carbides, 2023(1): 47-51.
MLA [1] ZHAO Hang, et al., "Dissolution Characteristics of Sc2O3 in ScF3-LiF Molten Salt." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 47-51.
APA [1] ZHAO Hang, CHEN Jian-she, WANG Chun-xin, LI Bin-chuan, HAN Qing, & LIU Kui-ren. (2023). Dissolution Characteristics of Sc2O3 in ScF3-LiF Molten Salt. Rare Metals and Cemented Carbides(1), 47-51.
IEEE [1] ZHAO Hang, CHEN Jian-she, WANG Chun-xin, LI Bin-chuan, HAN Qing, and LIU Kui-ren, "Dissolution Characteristics of Sc2O3 in ScF3-LiF Molten Salt," Rare Metals and Cemented Carbides, no. 1, pp. 47-51, 2023. keywords: {ScO;ScF-LiF;molten salt electrolysis;liquidus temperature;solubility}