Study on Preparation and NH3-SCR Denitration Performance of Molybdenum Oxide-Loaded Monazite Catalytic Materials AITranslate

School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The catalyst of molybdenum oxide-loaded monazite was prepared by impregnation method,and tests for its characterization and NH3-SCR denitration performance were carried out.The results show that the NO conversion rate of the composite catalyst with Mo/Ce molar ratio of 0.3 reaches 75%at the denitration reaction temperature of 400℃.Monazite increases the specific surface area of the catalyst.The loaded metal oxides are uniformly dispersed on the monazite surface,resulting in the coexistence of Ce3+/Ce4+and Mo5+/Mo6+and promoting electron transfer to generate oxygen vacancy and unsaturated chemical bonds,which is in favor of the increase of the active site on the monazite surface.Compared with pure monazite,the redox property and the adsorption and activation capacity of NH3of the composite catalyst have been improved mainly in the high temperature range,with a relatively small improvement in the denitration efficiency in the low temperature section.

KeyWords AITranslate

composite catalyst monazite molybdenum oxide denitration performance Mo5+/Mo6+coexistence Ce3+/Ce4+coexistence

1梁晶,郑健,韩苗苗,马龙信,石岩.氮氧化物危害及其处理技术[J].科技创新与应用,2021,11(24):120-122. 被引量:13

2耿冠楠,肖清扬,郑逸璇,同丹,张玉璇,张小曳,张强,贺克斌,刘阳.实施《大气污染防治行动计划》对中国东部地区PM2.5化学成分的影响[J].中国科学:地球科学,2020,50(4):469-482. 被引量:22

3杨培刚.大气中氮氧化物的危害因素及其防治措施[J].皮革制作与环保科技,2021,2(15):38-39. 被引量:5

4杨洁,李侠,杜红伟,柳召刚.低温La/Ce掺杂锰基脱硝催化剂的制备及表征[J].稀有金属与硬质合金,2021,49(3):41-45. 被引量:2

5赵欣,黄垒,李红蕊,扈航,韩瑾,施利毅,张登松.过渡金属(Cu,Fe,Mn,Co)改性高分散V_2O_5/TiO_2作为高效NH_3-SCR脱硝催化剂(英文)[J].催化学报(英文),2015,36(11):1886-1899. 被引量:28

6王献忠,吴彦霞,梁海龙,陈鑫,陈琛,晏根平,戴长友,陈玉峰.V2O5-MoO3TiO2催化剂脱硝性能的研究[J].石油炼制与化工,2021,52(1):79-85. 被引量:3

7程建忠,车丽萍.中国稀土资源开采现状及发展趋势[J].稀土,2010,31(2):65-69. 被引量:237

8余永富.白云鄂博矿稀土、铌资源综合利用研究意义重大[J].稀土信息,2007,13(8):8-9. 被引量:28

9张信莉,王栋,彭建升,路春美,徐丽婷.煅烧温度对Mn改性γ-Fe_2O_3催化剂结构及低温SCR脱硝活性的影响[J].燃料化学学报,2015,43(2):243-250. 被引量:12

10梁辉,查贤斌,归柯庭.γFe_2O_3的选择性催化还原脱硝性能及其对NH_3和NO的表面吸附行为研究[J].中国电机工程学报,2014,34(32):5734-5740. 被引量:10

1宋丽云,邓世林,周宜芸,李双叶,展宗城,李坚,何洪.V_(2)O_(5)-MoO_(3)/TiO_(2)催化剂的NH_(3)-SCR性能:载体的影响[J].材料导报,2023,37(6):67-72.

2黄鹏,王欣媛,郝芹,周济,徐彩霞.多级纳米花球状聚多巴胺-钼氧化物复合材料用于宽电压窗口锌离子存储[J].聊城大学学报:自然科学版,2023,36(1):85-92.

3黄纯琳,曾峻鹏,梁文钰.电厂SCR脱硝系统液氨改尿素性能分析[J].中国环保产业,2023(1):57-58.

4侯丽敏,许杰,付善聪,武文斐.Cu改性对稀土尾矿催化剂NH_(3)-SCR脱硝的影响[J].化工进展,2023,42(2):765-773.

5倪茂森,杨波,顾秋香,汪振辉,黄琼,陈敏东.具有球形催化界面的MnCeO_(x)/P84催化滤布的NOx脱除性能[J].环境工程,2022,40(12):157-164.

6张浩南,陈耿,朱颖颖.铁基氨气选择性催化还原(NH3-SCR)催化剂性能的研究进展[J].化学世界,2023,64(1):12-21.

7黄力,纵宇浩,李金珂,王虎,刘洋,高义博,韩沛.Cd对V-Mo/Ti脱硝催化剂性能的影响[J].锅炉技术,2023,54(1):15-20.

8刘康,魏博,王珊,王建江,陈丽娟.铥改性MnCeO_(x)/TiO_(2)催化剂在氨中低温还原NO_(x)的优越性能[J].有色金属:冶炼部分,2023(3):111-117.

9曲韦烨,马臻,唐幸福.双核催化位低温高效脱除氮氧化物[J].科学通报,2023,68(7):713-715.

10刘杨井浩,赵令葵,王雨轩,李俊杰,唐军,严家豪.Fe掺杂Mn-Ce多孔催化剂低温脱硝性能及甲苯的影响机制[J].环境科学学报,2023,43(3):405-415.

Basic Information:

DOI:

Chinese Library Classification Number:TD983[矿业工程—选矿]

Citation Information:

The catalyst of molybdenum oxide-loaded monazite was prepared by impregnation method,and tests for its characterization and NH3-SCR denitration performance were carried out.The results show that the NO conversion rate of the composite catalyst with Mo/Ce molar ratio of 0.3 reaches 75%at the denitration reaction temperature of 400℃.Monazite increases the specific surface area of the catalyst.The loaded metal oxides are uniformly dispersed on the monazite surface,resulting in the coexistence of Ce3+/Ce4+and Mo5+/Mo6+and promoting electron transfer to generate oxygen vacancy and unsaturated chemical bonds,which is in favor of the increase of the active site on the monazite surface.Compared with pure monazite,the redox property and the adsorption and activation capacity of NH3of the composite catalyst have been improved mainly in the high temperature range,with a relatively small improvement in the denitration efficiency in the low temperature section.

quote

GB/T 7714-2015 [1] WANG Ying, ZHAO Ran, ZHANG Kai, et al. Study on Preparation and NH3-SCR Denitration Performance of Molybdenum Oxide-Loaded Monazite Catalytic Materials[J]. Rare Metals and Cemented Carbides, 2023(1): 40-46.
MLA [1] WANG Ying, et al., "Study on Preparation and NH3-SCR Denitration Performance of Molybdenum Oxide-Loaded Monazite Catalytic Materials." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 40-46.
APA [1] WANG Ying, ZHAO Ran, ZHANG Kai, & WU Wen-fei. (2023). Study on Preparation and NH3-SCR Denitration Performance of Molybdenum Oxide-Loaded Monazite Catalytic Materials. Rare Metals and Cemented Carbides(1), 40-46.
IEEE [1] WANG Ying, ZHAO Ran, ZHANG Kai, and WU Wen-fei, "Study on Preparation and NH3-SCR Denitration Performance of Molybdenum Oxide-Loaded Monazite Catalytic Materials," Rare Metals and Cemented Carbides, no. 1, pp. 40-46, 2023. keywords: {composite catalyst;monazite;molybdenum oxide;denitration performance;Mo/Mocoexistence;Ce/Cecoexistence}