Abstract AITranslate
This article summarizes the general structural features and important properties of quasicrystals, a relatively new class of materials belonging to solid-state substances. Quasicrystals, which have a long-range quasiperiodic order but no three-dimensional translational periodicity, are structurally different from both conventional crystals and glassy solids. Although applications are still highly limited, quasicrystals are attracting significant attention as a structual constituent of mixed-phase materials exhibiting high strength together with certain ductility and can be applied as structural materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1146/annurev.matsci.38.060407.130318
Chinese Library Classification Number:
Citation Information:
This article summarizes the general structural features and important properties of quasicrystals, a relatively new class of materials belonging to solid-state substances. Quasicrystals, which have a long-range quasiperiodic order but no three-dimensional translational periodicity, are structurally different from both conventional crystals and glassy solids. Although applications are still highly limited, quasicrystals are attracting significant attention as a structual constituent of mixed-phase materials exhibiting high strength together with certain ductility and can be applied as structural materials.
quote
| GB/T 7714-2015 | [1] D.V. LouzguineLuzgin, A. Inoue. Annual Review of Materials Research, 2008(38). DOI:10.1146/annurev.matsci.38.060407.130318. |
| MLA | [1] D.V. LouzguineLuzgin, and A. Inoue. Annual Review of Materials Research, no. 38, 2008, https://doi.org/10.1146/annurev.matsci.38.060407.130318. |
| APA | [1] D.V. LouzguineLuzgin, & A. Inoue. (2008). Annual Review of Materials Research(38). https://doi.org/10.1146/annurev.matsci.38.060407.130318 |
| IEEE | [1] D.V. LouzguineLuzgin and A. Inoue, Annual Review of Materials Research, no. 38, 2008, doi: 10.1146/annurev.matsci.38.060407.130318. keywords: {icosahedral phase;structure;high strength} |