Abstract AITranslate
The crystal chemistry of complex perovskite dielectric oxides is reviewed, with an emphasis on structures derived from ordering of the cations on the octahedral B-sites. New classes of perovskites, designed to exhibit 1:2 or 1:3 B-site order for application as low-dielectric-loss microwave ceramics, are identified, and their synthesis, structure, and properties are described. Through the use of B-site chemistries based on Li, Nb, Ta, Ti, and W, members of four new families with 1:2 order, A(βI 1/3βII 2/3)O3, and three new families with 1:3 order, A(βI 1/4βII 3/4)O3, were successfully prepared. The formation and stability of the new and previously prepared ordered perovskites are rationalized through the use of familiar crystal chemical tools such as cation size and charge difference, bond valence, tolerance factor, and new concepts related to the local charge imbalance on the A- and B-sublattices. These tools can be successfully applied to develop stability field maps for each structure and to predict other new ordered systems.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1146/annurev.matsci.37.052506.084356
Chinese Library Classification Number:
Citation Information:
The crystal chemistry of complex perovskite dielectric oxides is reviewed, with an emphasis on structures derived from ordering of the cations on the octahedral B-sites. New classes of perovskites, designed to exhibit 1:2 or 1:3 B-site order for application as low-dielectric-loss microwave ceramics, are identified, and their synthesis, structure, and properties are described. Through the use of B-site chemistries based on Li, Nb, Ta, Ti, and W, members of four new families with 1:2 order, A(βI 1/3βII 2/3)O3, and three new families with 1:3 order, A(βI 1/4βII 3/4)O3, were successfully prepared. The formation and stability of the new and previously prepared ordered perovskites are rationalized through the use of familiar crystal chemical tools such as cation size and charge difference, bond valence, tolerance factor, and new concepts related to the local charge imbalance on the A- and B-sublattices. These tools can be successfully applied to develop stability field maps for each structure and to predict other new ordered systems.
quote
| GB/T 7714-2015 | [1] P.K. Davies, H. Wu, A.Y. Borisevich, et al. Annual Review of Materials Research, 2008(38). DOI:10.1146/annurev.matsci.37.052506.084356. |
| MLA | [1] P.K. Davies, et al., Annual Review of Materials Research, no. 38, 2008, https://doi.org/10.1146/annurev.matsci.37.052506.084356. |
| APA | [1] P.K. Davies, H. Wu, A.Y. Borisevich, I.E. Molodetsky, & L. Farber. (2008). Annual Review of Materials Research(38). https://doi.org/10.1146/annurev.matsci.37.052506.084356 |
| IEEE | [1] P.K. Davies, H. Wu, A.Y. Borisevich, I.E. Molodetsky, and L. Farber, Annual Review of Materials Research, no. 38, 2008, doi: 10.1146/annurev.matsci.37.052506.084356. keywords: {cation ordering;microwave ceramics;niobates;tantalates;titanates} |