Fluorin Determination in High Purity Niobium or Tantalum Oxides by Spectrophotometry AITranslate
Abstract AITranslate
The high purity niobium or tantalum oxides were firstlymelted with NaOH and leached with hot water,and then analyzed to determine their fluorin content by spectrophotometry with xylenol orange as the chromogenic reagent. The results show that the abovemethod is accurate and reliablewith high precisionand stability,and therefore can satisfy the analysis requirementfor the low content fluorin in the products of high purity niobium or tantalum oxides.
KeyWords AITranslate
1武骏钦.离子选择电极法测定氧化铌中氟[J].分析试验室,1990,9(3):70-71. 被引量:2
2萧满田.镀铬溶液中氟硅酸的快速光度测定(锆-二甲酚橙-氟硅酸退色光度法).电镀与环保,1985,(6):41-43.
1秦宗会,谢兵,刘艳.氟含量测定方法综述[J].中国西部科技,2010,9(21):1-2. 被引量:17
2郝一莼,孙小单,徐桐,席淑华.氟离子检测分析方法研究进展[J].中国地方病防治,2010,25(6):412-415. 被引量:15
3张颖.高纯钨、钼、钽、铌工业分析进展[J].湖南有色金属,2012,28(6):71-76. 被引量:9
4陈益山,刘善江.土壤中氟离子检测方法的研究进展[J].安徽农业科学,2013,41(25):10288-10289. 被引量:2
5赵振.ICP-AES测定铌、钽矿前处理影响因素优化[J].企业技术开发,2014,33(6):56-57. 被引量:1
6盖依冰,叶飞,叶晓英.ICP-AES法测定金属铌中Cu元素的方法研究[J].失效分析与预防,2014,9(4):228-231. 被引量:1
7刘洁,陈忠颖,刘巍,郭颖.电感耦合等离子体质谱法测定高纯铌中20种痕量杂质元素[J].理化检验:化学分册,2018,54(10):1158-1162. 被引量:4
8赖心,谢辉,张婷,杨勇,陈颖欣,张翠云.离子选择电极法测定镨钕合金中的氟含量[J].材料研究与应用,2019,13(3):242-246.
9侯倩倩,董雅卓,林帅,宋磊,许峰,张文申,冀克俭.高温燃烧吸收-离子色谱法测定氟醚橡胶中氟溴[J].中国测试,2020,46(9):53-58. 被引量:6
10施艳艳,田强坤,李超,杨琳娟,胡存申.离子选择电极法测定铜及铜合金中氟含量[J].云南冶金,2022,51(1):120-125.
1李增强.煤中氟的离子选择性电极法测定方法研究[J].科技风,2013(17):140-140. 被引量:4
2马恒.离子选择电极法测定岩石矿物中氟含量的方法讨论[J].新疆有色金属,2013,36(A02):103-104.
3屈桃李,左晓宇,王联芝.恩施市居民饮用水中F^-含量的测定[J].湖北民族学院学报:自然科学版,2013,31(4):426-427. 被引量:1
4曾青云,张勇,帅庚未.微波及超声波在钨冶金中的研究进展[J].有色金属科学与工程,2014,5(2):15-19. 被引量:2
5李汉超.ICP–AES法测定金属钼中微量Fe,Ni[J].化学分析计量,2014,23(4):73-75. 被引量:3
6喻艳华,付成.用基于苯并噻二唑衍生物的比率荧光化学传感器检测氟离子[J].化学研究,2014,25(5):482-487. 被引量:2
7屈桃李,李卫华,王联芝.水中F^-的检测与去除研究进展[J].湖北民族学院学报:自然科学版,2014,32(2):173-178. 被引量:4
8宋崇富,王中跃,田志美,李若,蒋雪月,张坤,盛良全.含氟牙膏中的氟含量测定方法准确度探究[J].安徽农业科学,2015,43(1):214-216. 被引量:5
9王楠,郭霞.X射线荧光光谱法熔融制样测定矿物中的铌钽[J].科学技术与工程,2015,35(11):140-142.
10孙烨,杨柳桦,单燕莉.离子色谱法测定不粘锅聚四氟乙烯涂层中溶出的氟[J].中国卫生检验杂志,2015,25(8):1140-1142. 被引量:2
1黄双.ICP—AES法测定高纯氧化铌中钨和钽[J].有色金属分析通讯,2000(2):20-21. 被引量:1
2张颖.阳离子交换ICP-OES测定高纯氧化铌中十三种杂质元素[J].硬质合金,2006,23(3):147-149. 被引量:4
3任凤莲,张颖.ICP-AES测定高纯氧化钽中13种杂质元素[J].光谱实验室,2003,20(1):74-76. 被引量:5
4郭鹏.电感耦合等离子体质谱法测定高纯氧化钽中28种痕量杂质元素[J].分析试验室,2008,27(3):106-109. 被引量:15
5张颖.电感耦合等离子体原子发射光谱法测定高纯氧化铌中13种杂质元素[J].理化检验:化学分册,2008,44(11):1097-1098. 被引量:9
6张颖.氢化发生ICP-OES测定高纯氧化铌中铋、硒、碲量[J].硬质合金,2007,24(4):240-242. 被引量:6
7巩卫东,宋顺茂,宁水平,齐国亮.国家标准钼精矿中钼的测定方法探讨[J].光谱实验室,2008,25(5):861-864. 被引量:2
8郭振华.电感耦合等离子体发射光谱法测定磷矿石中常量元素硅磷硫钙镁铝铁钛锰[J].岩矿测试,2012,31(3):446-449. 被引量:21
9张宁.电感耦合等离子体原子发射光谱法测定铜精矿和铅精矿中二氧化硅[J].冶金分析,2011,31(5):60-62. 被引量:11
10张晓丹.导数光谱法测定食品中的山梨酸[J].中外企业家,2015(12X).
Basic Information:
DOI:
Chinese Library Classification Number:O657.3[理学—分析化学]
Citation Information:
The high purity niobium or tantalum oxides were firstlymelted with NaOH and leached with hot water,and then analyzed to determine their fluorin content by spectrophotometry with xylenol orange as the chromogenic reagent. The results show that the abovemethod is accurate and reliablewith high precisionand stability,and therefore can satisfy the analysis requirementfor the low content fluorin in the products of high purity niobium or tantalum oxides.
quote
| GB/T 7714-2015 | [1] MA Yu-li. Fluorin Determination in High Purity Niobium or Tantalum Oxides by Spectrophotometry[J]. Rare Metals and Cemented Carbides, 2009(3): 36-38. |
| MLA | [1] MA Yu-li. "Fluorin Determination in High Purity Niobium or Tantalum Oxides by Spectrophotometry." Rare Metals and Cemented Carbides, no. 3, 2009, pp. 36-38. |
| APA | [1] MA Yu-li. (2009). Fluorin Determination in High Purity Niobium or Tantalum Oxides by Spectrophotometry. Rare Metals and Cemented Carbides(3), 36-38. |
| IEEE | [1] MA Yu-li, "Fluorin Determination in High Purity Niobium or Tantalum Oxides by Spectrophotometry," Rare Metals and Cemented Carbides, no. 3, pp. 36-38, 2009. keywords: {high purity niobium oxide;high purity tantalum oxide;fluorin;zirconium;xylenol orange} |