Present Development of Titanium Industry and its Outlook AITranslate

Beijing Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Distribution of mineral resources of Ti in the world and its physical and chemical properties are briefly introduced in the paper. The Present status of Ti applications in the fields of aeronautics and aerospace .military affairs .petrol-chemical industry, marine, automobile. metallurgy, medicine.agriculture and animal husbandry and others are reviewed in details. And the supply and demand of Ti in the world from 1996 to 2005 are predicted.

KeyWords AITranslate

Titanium industry Application present development outlook prediction

1杨晶晶,缪强,梁文萍,李龙,任蓓蕾,朱丹阳.Ti_2AlNb基O相合金双辉等离子渗碳层摩擦磨损性能[J].金属热处理,2013,38(6):110-113. 被引量:6

2张文朴.含钛催化剂研究新进展[J].稀有金属与硬质合金,2001,29(4):39-41.

1任蓓蕾,梁文萍,缪强,潘晓扬,刘文.Ti_2AlNb合金表面等离子渗铝层的摩擦性能[J].金属热处理,2015,40(11):56-60. 被引量:2

2潘晓扬,梁文萍,缪强,任蓓蕾,刘文.不同温度下TC21钛合金等离子表面渗Cr层的摩擦磨损性能[J].南京航空航天大学学报,2016,48(1):35-41. 被引量:3

3吴凯,姚为,张铁军,韩维群,王胜龙,王志敏.焊接工艺对Ti2AlNb合金焊接接头组织和性能的影响[J].金属热处理,2018,43(1):72-77. 被引量:3

4张方.Ti2AlNb基合金高温防护涂层的研究现状[J].材料保护,2019,52(11):124-131.

5林宏春,马丹丹,于盛旺,马永,周兵,高洁,黑鸿君,薛彦鹏.高黏附性超疏水表面的制备及耐腐蚀性[J].金属热处理,2022,47(2):193-199.

6朱旭,陈建文,蒋亦舟,刘克,罗子相,高毅强,向臻东.20Cr2Ni4A钢和17Cr2Ni2MoVNb钢渗碳层的组织与性能[J].金属热处理,2022,47(5):166-171.

1常工.工程领域的最大挑战之六:把超导材料推向市场[J].新产品世界,1993(4):21-23.

2全旭.以推进品牌建设为契机 提升材料院质量管理水平[J].航空标准化与质量,2007(3):55-56.

3王惠良.科技成果的转化与营销策略:北京航空材料研究所"三防"产品经营[J].航空军转民技术与产品,1996(11):7-9.

4卢怀谦,李玉海.美国、日本将“超导”列为21世纪支柱产业[J].中国软科学,1997(5):123-125.

5刘世友.日本超导材料的生产与开发[J].有色金属技术经济研究,1994(11):25-28.

6李伟.市场经济与质量管理[J].航空科学技术,1999(3):9-11.

7秦喜杰.北京超导材料产业化发展战略研究[J].科技进步与对策,2003,20(6):53-54.

8吴晓梅,林平忠.如何进行附件包修小时修理费率的测算[J].民航管理,2003(3):51-52.

9袁文明.航空材料标准化工作取得显著进展[J].航空标准化与质量,2009(3):3-3.

10朱剑英.世界航空发展趋势及其关键技术[J].航空知识,1996,0(7):8-11.

Basic Information:

DOI:

Chinese Library Classification Number:F407.4[经济管理—产业经济]

Citation Information:

Distribution of mineral resources of Ti in the world and its physical and chemical properties are briefly introduced in the paper. The Present status of Ti applications in the fields of aeronautics and aerospace .military affairs .petrol-chemical industry, marine, automobile. metallurgy, medicine.agriculture and animal husbandry and others are reviewed in details. And the supply and demand of Ti in the world from 1996 to 2005 are predicted.

quote

GB/T 7714-2015 [1] LIU Shi-you. Present Development of Titanium Industry and its Outlook[J]. Rare Metals and Cemented Carbides, 1997(4): 58-63.
MLA [1] LIU Shi-you. "Present Development of Titanium Industry and its Outlook." Rare Metals and Cemented Carbides, no. 4, 1997, pp. 58-63.
APA [1] LIU Shi-you. (1997). Present Development of Titanium Industry and its Outlook. Rare Metals and Cemented Carbides(4), 58-63.
IEEE [1] LIU Shi-you, "Present Development of Titanium Industry and its Outlook," Rare Metals and Cemented Carbides, no. 4, pp. 58-63, 1997. keywords: {Titanium industry, Application, present development,outlook, prediction}