Discussion on the Recovery of Rare Metals from Ta/Nb Hydrometallurgy AITranslate

Zhuzhou Hard Alloy Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Analysis and discussion is made with respect to the recovery of rare metals from several types of Ta/Nb raw materials, highly containing rare metals. It is concluded that the recovery of the rare metals during Ta/Nb production offers good economic and social benefits.

KeyWords AITranslate

Ta/Nb production raw material rare metal recovery economic benefit

1陈既明,张耀华.从钽铌萃余液中萃取回收钨的试验研究[J].矿冶工程,1994,14(2):45-48. 被引量:1

1韩建设,赵明智,王才明,张劲,周勇.钽铌湿法冶炼的“三废”综合治理工艺探讨[J].稀有金属与硬质合金,2006,34(4):40-44. 被引量:12

2黄膑.钽铌矿冶炼中的放射性污染及活度计算方法[J].能源研究与管理,2020(3):91-95. 被引量:4

1韩建设,刘建华,叶祥,凌诚.南方稀土水冶含氨废水综合回收工艺探讨[J].稀土,2008,29(6):69-75. 被引量:27

2韩建设,李丰,吴鹰.钽铌湿法冶炼工序成本及其核算管理探讨[J].稀有金属与硬质合金,2010,38(4):46-51.

3杨清宇,王琳丽,蔡锡元,韩建设.南方稀土湿法冶炼废水综合回收与治理研究(下)[J].有色冶金节能,2012,27(2):6-10. 被引量:4

4黄江波,徐文炘.钽铌钨锡多金属矿冶炼项目污染防治措施探讨[J].广州化工,2013,41(3):109-111. 被引量:1

5杨继红.钽铌冶炼生产中余热资源回收和利用工艺研究[J].稀有金属与硬质合金,2013,41(4):58-61.

6陈涛,李宁,晏波,肖贤明.稀土湿法冶炼废水污染治理技术与对策[J].化工进展,2014,33(5):1306-1311. 被引量:19

7董春明,张志和,刘峙嵘.共伴生放射性废渣合理化处置探讨[J].铀矿冶,2017,36(1):46-50. 被引量:7

8姜智超,邓景衡,张浩.钽铌冶炼铁泥制备聚硅酸硫酸铁絮凝剂及其应用[J].环境化学,2017,36(1):159-166. 被引量:5

9赵培培,陶莉,刘晨明,林晓.钽铌冶炼“三废”治理技术研究现状[J].有色金属:冶炼部分,2020,0(5):93-99. 被引量:5

10黄膑.钽铌矿冶炼中的放射性污染及活度计算方法[J].能源研究与管理,2020(3):91-95. 被引量:4

1罗会秋.从钽铌冶炼废水中回收钛的工艺研究[J].稀有金属与硬质合金,1997,25(4):19-22. 被引量:2

2张耀华,陈既明.不同浓度的仲辛醇对钽铌的萃取与反萃取性能的影响[J].稀有金属与硬质合金,1996,24(2):6-9. 被引量:3

3马伟,钟祥,贺泽全.包头铌精矿内配碳球团还原行为研究[J].矿冶工程,1996,16(2):51-54. 被引量:4

4张俊卿,冯德荣.N_(235)萃取铌的研究[J].包头钢铁学院学报,1999,18(2):156-158. 被引量:1

5王昆山.钽铌企业中的放射性水平及对人体的影响[J].工业安全与防尘,1998,24(7):25-28. 被引量:3

6马伟,钟祥,贺泽全,杨应亮.铌精矿内配炭球团预还原技术条件的研究[J].稀有金属与硬质合金,1995,23(4):12-17. 被引量:1

7杨继红.钽铌冶炼生产中余热资源回收和利用工艺研究[J].稀有金属与硬质合金,2013,41(4):58-61.

8陈宏,韩其勇,胡志高,吴雪平,朱腾.酸洗铌精矿富铌除磷的研究[J].稀有金属,1995,19(2):86-88.

9李建强.火焰原子吸收法测定铌精矿及炉渣中氧化钙[J].北京科技大学学报,1997,19(2):218-222. 被引量:1

10熊一凡,戴和平.钽铌湿法冶炼配水洗涤监控系统设计[J].江西科学,2013,31(5):679-681.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

Analysis and discussion is made with respect to the recovery of rare metals from several types of Ta/Nb raw materials, highly containing rare metals. It is concluded that the recovery of the rare metals during Ta/Nb production offers good economic and social benefits.

quote

GB/T 7714-2015 [1] CHEN Ji-ming. Discussion on the Recovery of Rare Metals from Ta/Nb Hydrometallurgy[J]. Rare Metals and Cemented Carbides, 1997(4): 56-58.
MLA [1] CHEN Ji-ming. "Discussion on the Recovery of Rare Metals from Ta/Nb Hydrometallurgy." Rare Metals and Cemented Carbides, no. 4, 1997, pp. 56-58.
APA [1] CHEN Ji-ming. (1997). Discussion on the Recovery of Rare Metals from Ta/Nb Hydrometallurgy. Rare Metals and Cemented Carbides(4), 56-58.
IEEE [1] CHEN Ji-ming, "Discussion on the Recovery of Rare Metals from Ta/Nb Hydrometallurgy," Rare Metals and Cemented Carbides, no. 4, pp. 56-58, 1997. keywords: {Ta/Nb production raw material, rare metal recovery,economic benefit}