Properties of AlCrN Coatings on Cemented Carbide Prepared by Arc Ion Plating Assisted by Gas Ion Source AITranslate
Abstract AITranslate
AlCrN coatings were deposited on cemented carbide by gas ion source-assisted arc ion plating and conventional arc ion plating,respectively.The microstructure,composition,hardness,bonding strength and wear resistance of AlCrN coatings prepared by these two methods were compared and analyzed.The results show that the surface of AlCrN coatings prepared by the two methods is smooth,and the bonding strength of all the coatings is above 100 N.The thickness of AlCrN coatings prepared by conventional arc ion plating is relatively thin,the proportion of metal atoms is small,the surface roughness is low,the friction coefficient is small,and the hardness and wear resistance are also low.Since the gas ion source-assisted deposition can improve the ionization rate of metal atoms,the growth rate of AlCrN coatings prepared by gas ion source-assisted arc ion plating is faster,and the hardness and wear resistance are improved.
KeyWords AITranslate
1居志兰,花国然,张华.硬质合金刀具材料的研究进展[J].稀有金属与硬质合金,2011,39(2):50-53. 被引量:10
2储开宇.我国硬质合金产业的发展现状与展望[J].稀有金属与硬质合金,2011,39(1):52-56. 被引量:23
3张文毓.硬质合金涂层刀具研究进展[J].稀有金属与硬质合金,2008,36(1):59-63. 被引量:41
4陈颢,羊建高,王宝健,刘海浪.硬质合金刀具涂层技术现状及展望[J].硬质合金,2009,26(1):54-58. 被引量:30
5范迪,雷浩,宫骏,孙超.正交电磁场离子源及其在PVD法制备硬质涂层中的应用[J].真空,2014,51(4):48-52. 被引量:3
6吴健,胡社军,曾鹏,谢光荣,周泽.低能氮离子束辅助真空电弧沉积Zr-Cu-N薄膜的研究[J].材料导报,2006,20(11):141-143. 被引量:1
7吴健,胡社军,曾鹏,李宇恒,谢光荣.离子束辅助真空电弧沉积Zr—Ni—N薄膜的研究[J].工具技术,2006,40(12):15-17. 被引量:1
8秦聪祥,曾鹏,胡社军,汝强.离子束辅助沉积对TiAlSiN薄膜性能的影响[J].钛工业进展,2006,23(2):25-28. 被引量:6
9吕树国,李玉海,张罡,姚俊,毕鉴智,金光.电弧离子镀制备TiAlN膜工艺研究[J].沈阳理工大学学报,2006,25(1):78-82. 被引量:9
1吴振宇,郑光明,盖少磊,李方梁,杨先海,程祥.微喷砂前处理对AlCrN涂层刀具表面完整性的影响[J].制造技术与机床,2022(1):103-106.
2张家敏,蔡飞,王文健,张世宏.不同后处理对AlCrN涂层结构和性能的影响[J].中国表面工程,2021,34(3):168-177. 被引量:1
3房磊琦,张家敏,蔡飞,李明喜,吴丽君,郑军,汤昌仁,朱瑞源.不同基体前处理对AlCrN涂层结构和性能的影响[J].表面技术,2022,51(2):66-76.
4张士勇,刘艳梅,张雅倩,郭桦帅,王铁钢.AlCrSiN/AlCrN/AlCrON/AlCrN多层复合涂层的研究[J].装备环境工程,2022,19(2):106-114. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG711[金属学及工艺—刀具与模具]
Citation Information:
AlCrN coatings were deposited on cemented carbide by gas ion source-assisted arc ion plating and conventional arc ion plating,respectively.The microstructure,composition,hardness,bonding strength and wear resistance of AlCrN coatings prepared by these two methods were compared and analyzed.The results show that the surface of AlCrN coatings prepared by the two methods is smooth,and the bonding strength of all the coatings is above 100 N.The thickness of AlCrN coatings prepared by conventional arc ion plating is relatively thin,the proportion of metal atoms is small,the surface roughness is low,the friction coefficient is small,and the hardness and wear resistance are also low.Since the gas ion source-assisted deposition can improve the ionization rate of metal atoms,the growth rate of AlCrN coatings prepared by gas ion source-assisted arc ion plating is faster,and the hardness and wear resistance are improved.
quote
| GB/T 7714-2015 | [1] RAN Long-jiao, ZHENG Si-ting, FAN Hong-yuan, et al. Properties of AlCrN Coatings on Cemented Carbide Prepared by Arc Ion Plating Assisted by Gas Ion Source[J]. Rare Metals and Cemented Carbides, 2021(6): 94-98. |
| MLA | [1] RAN Long-jiao, et al., "Properties of AlCrN Coatings on Cemented Carbide Prepared by Arc Ion Plating Assisted by Gas Ion Source." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 94-98. |
| APA | [1] RAN Long-jiao, ZHENG Si-ting, FAN Hong-yuan, XIAN Guang, XIONG Ji, GUO Zhi-xing, ZHAO Hai-bo, & JING Zheng-biao. (2021). Properties of AlCrN Coatings on Cemented Carbide Prepared by Arc Ion Plating Assisted by Gas Ion Source. Rare Metals and Cemented Carbides(6), 94-98. |
| IEEE | [1] RAN Long-jiao, ZHENG Si-ting, FAN Hong-yuan, XIAN Guang, XIONG Ji, GUO Zhi-xing, ZHAO Hai-bo, and JING Zheng-biao, "Properties of AlCrN Coatings on Cemented Carbide Prepared by Arc Ion Plating Assisted by Gas Ion Source," Rare Metals and Cemented Carbides, no. 6, pp. 94-98, 2021. keywords: {gas ion source;assisted deposition;arc ion plating;AlCrN coating;cemented carbide} |