Technological Study and Characterization of ZrO_2-doped Tungsten Alloy Powders with Hydrothermal Method AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

ZrO2-doped tungsten alloy powders were prepared with step hydrothermal method combined with calcination and two-stage hydrogen reduction process using APT and zirconium nitrate as raw materials.Phase composition,morphology and phase transformation were analyzed of the products from different preparation process by XRD,EDS,SEM and TEM.The results show that a tungstenic acid of 1.5WO3·2H2O is generated in the hydrothermal reaction of APT and nitric acid,and monoclinic ZrO2 is generated in the hydrothermal reaction of zirconium nitrate and ammonia.The above products were uniformly mixed by liquid-liquid doping and dried to obtain the precursor powders.After calcination of the precursor powders at500-550 ℃,cubic 1.5WO3·2H2O transforms into monoclinic WO3.After 800 ℃×2h+900 ℃×2hhydrogen reduction,ZrO2-doped tungsten alloy powders were obtained with average particle size of 10-20nm.Based on the results of contrast experiments,it is concluded that doping ZrO2 can play a role in refinement of tungsten grains.

KeyWords AITranslate

tungsten alloy powder ZrO2 doping hydrothermal reaction grain refinement APT

1卢平,沈春英,丘泰.掺杂稀土CeO_2亚微米钨粉的制备[J].粉末冶金工业,2008,18(2):6-8. 被引量:4

2陈一胜,朱志云,陈辉煌.稀土元素对掺杂钨粉还原过程及性能的影响[J].中国钨业,2006,21(6):39-41. 被引量:6

3梁健,黄惠忠,谢有畅.共沉淀法制备ZrO_2-Al_2O_3纳米复合氧化物的物相表征[J].物理化学学报,2003,19(1):30-34. 被引量:27

4张存信,秦丽柏,米文宇,白志国.我国穿甲弹用钨合金研究的最新进展与展望[J].粉末冶金材料科学与工程,2006,11(3):127-132. 被引量:45

5祝宝军,陶颖,邱玉婷,谢旻.水热法合成的纳米氧化锆结构[J].粉末冶金材料科学与工程,2008,13(2):111-114. 被引量:11

6范景莲,汪登龙,刘涛.细晶钨合金制备工艺的研究[J].兵器材料科学与工程,2006,29(2):1-5. 被引量:18

7孙秀娟,杨娟,刘芹芹,程晓农.水热法制备负热膨胀性ZrW_2O_8粉体(英文)[J].硅酸盐学报,2008,36(1):35-39. 被引量:8

1王军.高性能钨合金制备技术研究现状[J].有色金属材料与工程,2019,40(4):53-60. 被引量:5

2宋万里,徐流杰,尚清毅,黄志民.不同氧化物掺杂钼合金粉末的形貌变化[J].稀有金属与硬质合金,2021,49(1):40-47. 被引量:2

3焦照临,徐流杰,徐照宁,周玉成,杨璐.Al_(2)O_(3)掺杂钼合金的显微组织及电化学腐蚀行为研究[J].稀有金属与硬质合金,2022,50(5):59-65.

4叶家豪,赵云超,李洲,朱晨辉,徐流杰.水热法制备ZrO_(2)掺杂钨粉体过程中的粉体形貌与相转变[J].稀有金属,2023,47(6):825-833.

1李锋,钱康乐,傅珠荣,葛鑫,薛建平.辊模拉拔软钎料金属的变形特征及其改进设计[J].有色金属加工,2020,49(6):49-53. 被引量:4

2黄安平,郑海强,翁羽.高性能钨合金制备技术研究现状[J].中国金属通报,2020(18):84-85.

3杨文涛,薛冰,代永富,蒲传金,肖定军.球磨时间对钨粉粒度分布及形貌影响[J].粉末冶金技术,2021,39(5):423-428. 被引量:1

4王俊杰,杨建,成小乐,丁露露.摩擦系数及模角对钨合金静液挤压过程的影响研究[J].重型机械,2021(6):56-62. 被引量:2

5常富强,牛南南,梁献振.洛钼选厂二段球磨机钢球配比优化研究[J].现代矿业,2022,38(3):125-128. 被引量:2

6蒋丽娟,曹亮,高海亮,刘燕,刘晓辉,张智伟.2021年钼业年评[J].中国钼业,2022,46(2):1-7.

7王玲,秦颖楠,单东栋,熊宁.93WNiCu合金的高温性能及断裂机理研究[J].中国钨业,2022,37(1):55-59.

1郭松亮,张国赏,魏世忠,徐流杰,崔超鹏.ZrO_2掺杂Mo基合金的制备及强化机理分析[J].稀有金属与硬质合金,2014,42(5):48-50. 被引量:1

2彭卫珍.蓝钨物理性能对钨粉和碳化钨粉性能的影响[J].硬质合金,2004,21(3):142-148. 被引量:7

3肖方闹,徐流杰,周玉成,潘昆明,魏世忠.ZrO_2增强钨基复合材料制备工艺与性能[J].材料热处理学报,2016,37(2):12-19.

4刘光跃.仲钨酸铵的热分解过程[J].钨钼材料,1994(1):10-13.

5合金钢中合金元素的存在形式[J].金属热处理,2012,37(3):61-61. 被引量:1

6史翙青,贾志新,滕向阳.三乙醇胺对电火花线切割加工的影响[J].机械制造与自动化,2007,36(1):49-50. 被引量:2

7范景莲,黄伯云,曲选辉,张传福.纳米晶钨合金粉末常压烧结的致密化和晶粒长大[J].粉末冶金材料科学与工程,2001,6(2):83-88. 被引量:3

8张.刀具制造商开展硬质合金废料回收活动[J].工具展望,2006(4):24-24.

9张.APT——硬质合金刀具涨价之源[J].工具展望,2006(2):21-21.

10APT——硬质合金刀具涨价之源[J].工具技术,2006,40(7):59-59.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

ZrO2-doped tungsten alloy powders were prepared with step hydrothermal method combined with calcination and two-stage hydrogen reduction process using APT and zirconium nitrate as raw materials.Phase composition,morphology and phase transformation were analyzed of the products from different preparation process by XRD,EDS,SEM and TEM.The results show that a tungstenic acid of 1.5WO3·2H2O is generated in the hydrothermal reaction of APT and nitric acid,and monoclinic ZrO2 is generated in the hydrothermal reaction of zirconium nitrate and ammonia.The above products were uniformly mixed by liquid-liquid doping and dried to obtain the precursor powders.After calcination of the precursor powders at500-550 ℃,cubic 1.5WO3·2H2O transforms into monoclinic WO3.After 800 ℃×2h+900 ℃×2hhydrogen reduction,ZrO2-doped tungsten alloy powders were obtained with average particle size of 10-20nm.Based on the results of contrast experiments,it is concluded that doping ZrO2 can play a role in refinement of tungsten grains.

quote

GB/T 7714-2015 [1] LI Zhou, XU Liu-jie, WEI Shi-zhong, et al. Technological Study and Characterization of ZrO_2-doped Tungsten Alloy Powders with Hydrothermal Method[J]. Rare Metals and Cemented Carbides, 2017(1): 31-35.
MLA [1] LI Zhou, et al., "Technological Study and Characterization of ZrO_2-doped Tungsten Alloy Powders with Hydrothermal Method." Rare Metals and Cemented Carbides, no. 1, 2017, pp. 31-35.
APA [1] LI Zhou, XU Liu-jie, WEI Shi-zhong, PAN Kun-ming, & XIAO Fang-nao. (2017). Technological Study and Characterization of ZrO_2-doped Tungsten Alloy Powders with Hydrothermal Method. Rare Metals and Cemented Carbides(1), 31-35.
IEEE [1] LI Zhou, XU Liu-jie, WEI Shi-zhong, PAN Kun-ming, and XIAO Fang-nao, "Technological Study and Characterization of ZrO_2-doped Tungsten Alloy Powders with Hydrothermal Method," Rare Metals and Cemented Carbides, no. 1, pp. 31-35, 2017. keywords: {tungsten alloy powder;ZrO2 doping;hydrothermal reaction;grain refinement;APT}