Synthesis of Fe3O4/HAP/Ag Composite Nanomaterials and Their Photocatalytic Degradation of Ciprofloxacin AITranslate

School of Chemistry and Environmental Science,Shaanxi University of Technology;School of Chemistry and Environmental Science,Shaanxi University of Technology;School of Chemistry and Environmental Science,Shaanxi University of Technology;School of Chemistry and Environmental Science,Shaanxi University of Technology;School of Chemistry and Environmental Science,Shaanxi University of Technology;School of Chemistry and Environmental Science,Shaanxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As a widely used antibacterial drug,ciprofloxacin(CIP)residues have posed serious threats to ecosystems and human health.In order to solve this problem,magnetic hydroxyapatite/silver nanoparticle composite(Fe3O4/HAP/Ag)was synthesized via a blending method and employed as photocatalysts for CIP degradation,leveraging the photocatalytic properties of Ag.The phase and structure of the synthetic samples were characterized by X-ray diffraction(XRD)pattern,ultraviolet-visible(UV-Vis)absorption spectra and infrared(IR)spectra.The effects of CIP concentration,catalyst(Fe3O4/HAP/Ag)dosage and oxidant(peroxymonosulfate,PMS)amount on CIP degradation efficiency were investigated through degradation experiments.The results show that the optimized degradation conditions for 9 mL of ciprofloxacin solution are as follows:initial CIP concentration of 10 mg/L,Fe3O4/HAP/Ag dosage of 50 mg,and PMS amount of 5 mg.Under these conditions with 200 W light irradiation,the degradation rate of CIP reaches 70.36%within 60 min.The light irradiation can enhance the catalytic activity of the Fe3O4/HAP/Ag composite nanomaterials.This study establishes a novel approach for the efficient ciprofloxacin degradation.

KeyWords AITranslate

magnetic composite hydroxyapatite silver nanoparticle Fe3O4 ciprofloxacin(CIP) peroxymonosulfate(PMS) photocatalytic degradation
No data

Basic Information:

DOI:

Chinese Library Classification Number:TQ426.64[化学工程]

Citation Information:

As a widely used antibacterial drug,ciprofloxacin(CIP)residues have posed serious threats to ecosystems and human health.In order to solve this problem,magnetic hydroxyapatite/silver nanoparticle composite(Fe3O4/HAP/Ag)was synthesized via a blending method and employed as photocatalysts for CIP degradation,leveraging the photocatalytic properties of Ag.The phase and structure of the synthetic samples were characterized by X-ray diffraction(XRD)pattern,ultraviolet-visible(UV-Vis)absorption spectra and infrared(IR)spectra.The effects of CIP concentration,catalyst(Fe3O4/HAP/Ag)dosage and oxidant(peroxymonosulfate,PMS)amount on CIP degradation efficiency were investigated through degradation experiments.The results show that the optimized degradation conditions for 9 mL of ciprofloxacin solution are as follows:initial CIP concentration of 10 mg/L,Fe3O4/HAP/Ag dosage of 50 mg,and PMS amount of 5 mg.Under these conditions with 200 W light irradiation,the degradation rate of CIP reaches 70.36%within 60 min.The light irradiation can enhance the catalytic activity of the Fe3O4/HAP/Ag composite nanomaterials.This study establishes a novel approach for the efficient ciprofloxacin degradation.

quote

GB/T 7714-2015 [1] WANG Yu-lin, WU Rui, LI Hong-rui, et al. Synthesis of Fe3O4/HAP/Ag Composite Nanomaterials and Their Photocatalytic Degradation of Ciprofloxacin[J]. Rare Metals and Cemented Carbides, 2025(3): 119-126.
MLA [1] WANG Yu-lin, et al., "Synthesis of Fe3O4/HAP/Ag Composite Nanomaterials and Their Photocatalytic Degradation of Ciprofloxacin." Rare Metals and Cemented Carbides, no. 3, 2025, pp. 119-126.
APA [1] WANG Yu-lin, WU Rui, LI Hong-rui, LI Yi-huai, WANG Heng-bo, & ZHANG Qiang. (2025). Synthesis of Fe3O4/HAP/Ag Composite Nanomaterials and Their Photocatalytic Degradation of Ciprofloxacin. Rare Metals and Cemented Carbides(3), 119-126.
IEEE [1] WANG Yu-lin, WU Rui, LI Hong-rui, LI Yi-huai, WANG Heng-bo, and ZHANG Qiang, "Synthesis of Fe3O4/HAP/Ag Composite Nanomaterials and Their Photocatalytic Degradation of Ciprofloxacin," Rare Metals and Cemented Carbides, no. 3, pp. 119-126, 2025. keywords: {magnetic composite;hydroxyapatite;silver nanoparticle;FeO;ciprofloxacin(CIP);peroxymonosulfate(PMS);photocatalytic degradation}