daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Production of High-purity Dy Metal by Magnesium Reduction AITranslate

Hunan Rare Earth Metal Materials Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of production of high purity Dy metals by magnesium reduction.The results showed that high purity (up to 99.99%)Dy can be obtained by the following process:preparation of unhydrous DyCl 3 by chloridization of high purity(4N)Dy 2O 3 with high purity chloridizing agent;then magnesium reduction of unhydrous DyCl 3 to obtain Mg Dy alloy followed by distillation to obtain Dy metal.

KeyWords AITranslate

high purity Dy unhydrous Dy 2O 3 magnesium reduction

1杨遇春.稀土漫谈[M].北京:化学工业出版社,1995.

2VERHOEVEN J D,et al.The Effet of Composition and Ma gnetic Heat Treatment on the Magnetostriction of TbxDy1-xFey Twinned Single Crystals[J].J Appl Phys,1989,66(2):15.

1李国云,李国栋,刘永林.熔盐萃取法制备低氧、低氟金属镝的机制研究[J].中国稀土学报,2002,20(z2):263-265. 被引量:1

1刘文生,云月厚,李国栋.干法氟化制备高纯金属镝的工艺研究[J].稀有金属,2003,27(1):154-156. 被引量:7

1徐静,张炜,肖锋,赵斌,杨广禄,张耀,李宗安.中间合金-真空蒸馏法制备高纯金属镝工艺研究[J].稀土,2003,24(4):36-38. 被引量:4

2苏明忠,宋丕莹,邹天楚,路连清,刘素兰,杜森林.熔盐电解制备Al—Dy合金[J].稀土,1995,16(5):61-63. 被引量:3

3雷伯朝,刘斌.高纯金属镝的制备工艺研究与工业实践[J].稀有金属与硬质合金,2001,29(4):18-20. 被引量:4

4刘文生,云月厚,李国栋.干法氟化制备高纯金属镝的工艺研究[J].稀有金属,2003,27(1):154-156. 被引量:7

5陈国华,王小青,刘玉宝,赵二雄,于兵,李坤.熔盐电解法制备镨钕镝合金的研究[J].稀土,2015,36(1):80-84. 被引量:14

6梁勇,吕江涛,林如丹,刘玉城,廖春发.Dy_2O_3(Dy)-HCl-CaF_2-H_2O体系热力学研究[J].湿法冶金,2016,35(6):469-472. 被引量:2

7林河成.我国金属镝材料的生产及应用[J].稀有金属快报,2001,20(5):5-7.

8简启发,邱小英.废旧钕铁硼提取氧化钕和氯化镝工艺及生产实践[J].江西有色金属,2001,15(3):26-29. 被引量:4

9张红英.采用氯化镝溶液生产氟化镝的工艺研究[J].江西有色金属,1998,12(4):29-31. 被引量:3

102009年12月30日稀土价格[J].四川稀土,2009(4):32-32.

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

Study is made of production of high purity Dy metals by magnesium reduction.The results showed that high purity (up to 99.99%)Dy can be obtained by the following process:preparation of unhydrous DyCl 3 by chloridization of high purity(4N)Dy 2O 3 with high purity chloridizing agent;then magnesium reduction of unhydrous DyCl 3 to obtain Mg Dy alloy followed by distillation to obtain Dy metal.

quote

GB/T 7714-2015 [1] YU Qiang-guo. Production of High-purity Dy Metal by Magnesium Reduction[J]. Rare Metals and Cemented Carbides, 2001(2): 11-14.
MLA [1] YU Qiang-guo. "Production of High-purity Dy Metal by Magnesium Reduction." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 11-14.
APA [1] YU Qiang-guo. (2001). Production of High-purity Dy Metal by Magnesium Reduction. Rare Metals and Cemented Carbides(2), 11-14.
IEEE [1] YU Qiang-guo, "Production of High-purity Dy Metal by Magnesium Reduction," Rare Metals and Cemented Carbides, no. 2, pp. 11-14, 2001. keywords: {high purity Dy;unhydrous Dy 2O 3;magnesium reduction}