Surfactant-Wrapped n-Type Organic Thermoelectric Carbon Nanotubes for Long-Term Air Stability and Power Characteristics Surfactant-Wrapped n-Type Organic Thermoelectric Carbon Nanotubes for Long-Term Air Stability and Power Characteristics AITranslate

Sanyo-Onoda City University; Sanyo-Onoda City University; Sanyo-Onoda City University; Soochow University; Sanyo-Onoda City University;Tokyo University of Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The low air stability and unfavorable power properties of n-type carbon nanotubes (CNTs) limit the development of flexible electronics and organic transistors. Hence, determining an optimal n-dopant remains crucial. We propose the high surface coverage of adsorbed surfactant layers on nanotubes to maintain a continuous carrier stability and preserve the organic thermoelectric properties of n-type materials. Aqueous solutions of gemini surfactants with a tail length of 8 or 12 C atoms (8-3-8 and 12-3-12) were used as dispersants for the nanotubes. The gemini surfactants facilitated the enhanced dispersion of nanotubes to a greater degree than single-chain surfactants, ultimately improving the thermoelectric performance of films. An in-plane dimensionless figure-of-merit value of 6.04 × 10–3 was recorded for the optimized 12-3-12/CNTs, which was comparable to that of oil-soluble dopants. In addition, the n-type thermoelectric characteristics had not been previously investigated beyond 100 d in conventional systems because of a significant drop in the power factor, which was caused by a decrease in the negative Seebeck coefficient. We therefore evaluated the air stabilities of CNTs fabricated using 8-3-8 and 12-3-12, observing that gemini surfactants extended the lifetimes and enhanced the thermoelectric performances of n-type carriers to a greater extent than single-chain surfactants. Approximately 83% of the initial power characteristics were retained for 12-3-12/CNTs after 120 d under air, which was attributed to the high surface area of the adsorbed gemini surfactant on the nanotubes. The low specific surface areas of the bare nanotubes reduced the oxygen-accessible area, suppressing hole doping caused by atmospheric oxygen and improving the stabilities and power characteristics of n-type CNTs. The future design of surfactants to control the form of cationic molecular adsorption is therefore essential to achieve sustained air stabilities and favorable output properties for n-type materials.

KeyWords AITranslate

air stability dispersion figureofmerit gemini surfactant ntype CNT power factor surfactant doping thermoelectric properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01256

Chinese Library Classification Number:

Citation Information:

The low air stability and unfavorable power properties of n-type carbon nanotubes (CNTs) limit the development of flexible electronics and organic transistors. Hence, determining an optimal n-dopant remains crucial. We propose the high surface coverage of adsorbed surfactant layers on nanotubes to maintain a continuous carrier stability and preserve the organic thermoelectric properties of n-type materials. Aqueous solutions of gemini surfactants with a tail length of 8 or 12 C atoms (8-3-8 and 12-3-12) were used as dispersants for the nanotubes. The gemini surfactants facilitated the enhanced dispersion of nanotubes to a greater degree than single-chain surfactants, ultimately improving the thermoelectric performance of films. An in-plane dimensionless figure-of-merit value of 6.04 × 10–3 was recorded for the optimized 12-3-12/CNTs, which was comparable to that of oil-soluble dopants. In addition, the n-type thermoelectric characteristics had not been previously investigated beyond 100 d in conventional systems because of a significant drop in the power factor, which was caused by a decrease in the negative Seebeck coefficient. We therefore evaluated the air stabilities of CNTs fabricated using 8-3-8 and 12-3-12, observing that gemini surfactants extended the lifetimes and enhanced the thermoelectric performances of n-type carriers to a greater extent than single-chain surfactants. Approximately 83% of the initial power characteristics were retained for 12-3-12/CNTs after 120 d under air, which was attributed to the high surface area of the adsorbed gemini surfactant on the nanotubes. The low specific surface areas of the bare nanotubes reduced the oxygen-accessible area, suppressing hole doping caused by atmospheric oxygen and improving the stabilities and power characteristics of n-type CNTs. The future design of surfactants to control the form of cationic molecular adsorption is therefore essential to achieve sustained air stabilities and favorable output properties for n-type materials.

quote

GB/T 7714-2015 [1] Shinichi Hata, Kanto Maeshiro, Misaki Shiraishi, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01256.
MLA [1] Shinichi Hata, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01256.
APA [1] Shinichi Hata, Kanto Maeshiro, Misaki Shiraishi, Yukou Du, Yukihide Shiraishi, & Naoki Toshima. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01256
IEEE [1] Shinichi Hata, Kanto Maeshiro, Misaki Shiraishi, Yukou Du, Yukihide Shiraishi, and Naoki Toshima, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01256. keywords: {air stability dispersion figureofmerit gemini surfactant ntype CNT power factor surfactant doping thermoelectric properties}