Electroluminescent Aggregation-Induced Emission-Active Discotic Liquid Crystals Based on Alkoxy Cyanostilbene-Functionalized Benzenetricarboxamide with Ambipolar Charge Transport AITranslate

Indian Institute of Science Education and Research (IISER) Mohali; Indian Institute of Science Education and Research (IISER) Mohali; Indian Institute of Science Education and Research (IISER) Mohali; National Tsing Hua University; Indian Institute of Science Education and Research (IISER) Mohali; Patna University; National Tsing Hua University; Shiv Nadar University; Indian Institute of Science Education and Research (IISER) Mohali
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

There is significant demand for molecular functional materials with tailored light-emissive and charge transport properties for their utilization in organic optoelectronic devices. Motivated by such promising properties, we present the synthetic design and emissive and semiconducting properties of aggregation-induced emission (AIE)-active columnar discotic liquid crystals based on cyanostilbene-modified benzenetricarboxamide derivatives (1a, 1b, and 1c). Enantiotropic mesomorphic behavior over a wide temperature range, including room temperature, with columnar hexagonal self-assembly was observed for all of the compounds. The space-charge limited current (SCLC) technique revealed the ambipolar charge transport for reported materials with balanced electron and hole transport of the order of 10–3 cm2/(V s). On the other hand, all of the compounds 1a–c were tested as emitter materials in solution-processed organic light-emitting devices at different concentrations with several hosts, viz., poly(vinylcarbazole) (PVK), 1,3-bis(N-carbazolyl)benzene (mCP), bis[3,5-di(9H-carbazol-9-yl)phenyl]diphenylsilane (SimCP2), and (carbazolyl)-1,10-biphenyl (CBP). The maximum luminance of 1255 cd/m2 corresponding to sky-blue emission was observed for compound 1a at 3.0 wt % with the CBP host.

KeyWords AITranslate

discotic liquid crystals ambipolar charge transport OLEDs columnar hexagonal organic semiconductors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01251

Chinese Library Classification Number:

Citation Information:

There is significant demand for molecular functional materials with tailored light-emissive and charge transport properties for their utilization in organic optoelectronic devices. Motivated by such promising properties, we present the synthetic design and emissive and semiconducting properties of aggregation-induced emission (AIE)-active columnar discotic liquid crystals based on cyanostilbene-modified benzenetricarboxamide derivatives (1a, 1b, and 1c). Enantiotropic mesomorphic behavior over a wide temperature range, including room temperature, with columnar hexagonal self-assembly was observed for all of the compounds. The space-charge limited current (SCLC) technique revealed the ambipolar charge transport for reported materials with balanced electron and hole transport of the order of 10–3 cm2/(V s). On the other hand, all of the compounds 1a–c were tested as emitter materials in solution-processed organic light-emitting devices at different concentrations with several hosts, viz., poly(vinylcarbazole) (PVK), 1,3-bis(N-carbazolyl)benzene (mCP), bis[3,5-di(9H-carbazol-9-yl)phenyl]diphenylsilane (SimCP2), and (carbazolyl)-1,10-biphenyl (CBP). The maximum luminance of 1255 cd/m2 corresponding to sky-blue emission was observed for compound 1a at 3.0 wt % with the CBP host.

quote

GB/T 7714-2015 [1] Indu Bala, Harpreet Kaur, Madhusudan Maity, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01251.
MLA [1] Indu Bala, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01251.
APA [1] Indu Bala, Harpreet Kaur, Madhusudan Maity, Rohit Ashok Kumar Yadav, Joydip De, Santosh Prasad Gupta, JwoHuei Jou, Upendra Kumar Pandey, & Santanu Kumar Pal. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01251
IEEE [1] Indu Bala, Harpreet Kaur, Madhusudan Maity, Rohit Ashok Kumar Yadav, Joydip De, Santosh Prasad Gupta, JwoHuei Jou, Upendra Kumar Pandey, and Santanu Kumar Pal, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01251. keywords: {discotic liquid crystals ambipolar charge transport OLEDs columnar hexagonal organic semiconductors}