Large-Area Orientation-Controlled Growth of Hexagonal Boron Nitride on Liquid Copper Large-Area Orientation-Controlled Growth of Hexagonal Boron Nitride on Liquid Copper AITranslate
Abstract AITranslate
Two-dimensional semiconductors have great potential in applications of high-performance electrical and optoelectrical devices. Many efforts have been made to meet the challenge of reducing charge scattering between semiconducting and dielectric layers. Hexagonal boron nitride (h-BN) with a large band gap and a flat surface is thus an ideal dielectric layer for addressing this particular requirement. Therefore, preparing high-quality h-BN is an important topic in the electronic industry. In this work, two-opposite orientation growth modes of h-BN domains on liquid Cu are discovered. Comprehensive characterizations verify this anti-orientation feature of the as-grown domains and the grain boundary-free nature in the merged domains with the same orientation. The orientation-controlled h-BN domain growth is achieved by tuning the growth temperature and H2 and Ar flow rates, where the proportion of 0°-orientation domains is modulated in a wide range from ∼54.4 to 75%. Furthermore, based on the controllable growth of oriented h-BN, centimeter-sized h-BN films with high quality are produced.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01367
Chinese Library Classification Number:
Citation Information:
Two-dimensional semiconductors have great potential in applications of high-performance electrical and optoelectrical devices. Many efforts have been made to meet the challenge of reducing charge scattering between semiconducting and dielectric layers. Hexagonal boron nitride (h-BN) with a large band gap and a flat surface is thus an ideal dielectric layer for addressing this particular requirement. Therefore, preparing high-quality h-BN is an important topic in the electronic industry. In this work, two-opposite orientation growth modes of h-BN domains on liquid Cu are discovered. Comprehensive characterizations verify this anti-orientation feature of the as-grown domains and the grain boundary-free nature in the merged domains with the same orientation. The orientation-controlled h-BN domain growth is achieved by tuning the growth temperature and H2 and Ar flow rates, where the proportion of 0°-orientation domains is modulated in a wide range from ∼54.4 to 75%. Furthermore, based on the controllable growth of oriented h-BN, centimeter-sized h-BN films with high quality are produced.
quote
| GB/T 7714-2015 | [1] Xiahong Zhou, Xudong Xue, Le Cai, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01367. |
| MLA | [1] Xiahong Zhou, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01367. |
| APA | [1] Xiahong Zhou, Xudong Xue, Le Cai, Shan Liu, Mengya Liu, & Gui Yu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01367 |
| IEEE | [1] Xiahong Zhou, Xudong Xue, Le Cai, Shan Liu, Mengya Liu, and Gui Yu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01367. keywords: {chemical vapor deposition hexagonal boron nitride orientation control centimetersized film liquid substrate} |