Lutetium-Doped ZnO to Improve Photovoltaic Performance: A First-Principles Study Lutetium-Doped ZnO to Improve Photovoltaic Performance: A First-Principles Study AITranslate

Jiangsu University; Texas A&M University; Jiangsu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We investigated the effect of different impurity concentrations of lutetium (Lu)-doped ZnO on its optoelectronic properties utilizing the first principles based on density functional theory. The findings show that 1.85 at.% Lu-ZnO has the smallest lattice distortion and the impurity formation energy is less than zero, with the likelihood of chemical preparation. Analysis of electrical properties revealed that the conductivity of Lu-doped ZnO decreases with increasing impurity concentration and all show n-type semiconductors. Moreover, the spectral data suggested that the transmittivity increases with increasing doping concentration, and optical properties were extremely sensitive to the impurity concentration in the visible region. The current findings will greatly broaden the application of ZnO in photovoltaic devices.

KeyWords AITranslate

photoelectric properties first principles DFT simulation transmittivity conductivity Ludoped ZnO
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01365

Chinese Library Classification Number:

Citation Information:

We investigated the effect of different impurity concentrations of lutetium (Lu)-doped ZnO on its optoelectronic properties utilizing the first principles based on density functional theory. The findings show that 1.85 at.% Lu-ZnO has the smallest lattice distortion and the impurity formation energy is less than zero, with the likelihood of chemical preparation. Analysis of electrical properties revealed that the conductivity of Lu-doped ZnO decreases with increasing impurity concentration and all show n-type semiconductors. Moreover, the spectral data suggested that the transmittivity increases with increasing doping concentration, and optical properties were extremely sensitive to the impurity concentration in the visible region. The current findings will greatly broaden the application of ZnO in photovoltaic devices.

quote

GB/T 7714-2015 [1] Lin Li, Haiying Yang, Ping Yang. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01365.
MLA [1] Lin Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01365.
APA [1] Lin Li, Haiying Yang, & Ping Yang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01365
IEEE [1] Lin Li, Haiying Yang, and Ping Yang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01365. keywords: {photoelectric properties first principles DFT simulation transmittivity conductivity Ludoped ZnO}