daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of Ultra-fine CeO_2 Precursor for Optical Glass Polishing Material AITranslate

School of Chemistry and Materials Science, Nanchang University;School of Chemistry and Materials Science, Nanchang University;School of Chemistry and Materials Science, Nanchang University;School of Chemistry and Materials Science, Nanchang University;School of Chemistry and Materials Science, Nanchang University;School of Chemistry and Materials Science, Nanchang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ultra-fine CeO2 precursor for optical glass polishing material was prepared by selective oxidation and precipitation, washing, drying and calcination from low-cerium complex rare earth chlorides solution with NH3.H2O as precipitator, air and H2O2 as oxidative agent.The effect of reaction conditions and feeding mode on the content of CeO2 in precursor,and the correlativity between calcination temperature and particle size,specific surface area and mineralogical composition of precursor powder were investigated.The results show that by forward dripping, pH value controlled within 4.5 and 5.5,Ce3+ can be oxidized into Ce4+ to form hydroxide precipitant,followed by separation with other RE ions the ultra-fine polishing powder and precipitation before calcinations at 600~700 ℃ to obtain ultra-fine CeO2 precursor with CeO2 content over 80%,median particle size D50 less than 1.5 μm.

KeyWords AITranslate

ultrafine CeO2 precursor polishing material

1李永绣.稀土产品的物性控制与稀土产业的发展[J].稀土,1999,20(4):73-77. 被引量:20

2江祖成 蔡汝秀 等.稀土元素分析化学[M].北京:科学出版社,2001.29.

3李永绣 等.稀土灯用荧光粉生产中的前驱体制备技术[A].中国稀土学会.中国稀土科技进展[C].北京:冶金工业出版社,2000.473.

4徐光宪.稀士[M].北京:冶金工业出版社,1995..

5李永绣,周新木,辜子英,彭德院,胡平贵,周雪珍,焦晓燕,何小彬,魏坤,刘桂华.稀土抛光材料的生产、应用及其新进展[J].稀土,2002,23(5):71-74. 被引量:28

6郑武成.稀土抛光粉的物化性能与抛光能力问的关系[J].稀土,1981,(1):46-46.

1周雪珍,程昌明,胡建东,辜子英,胡平贵,李永绣.以碳酸铈为前驱体制备超细氧化铈及其抛光性能[J].稀土,2006,27(1):1-3. 被引量:16

2柴明霞,李永绣,胡建东,周雪珍.复合稀土氧化物的制备技术[J].广东化工,2007,34(2):5-7.

3宋晓岚,李宇焜,江楠,屈一新,邱冠周.化学机械抛光技术研究进展[J].化工进展,2008(1):26-31. 被引量:43

4李颖毅,陈伟凡.影响抛光粉抛蚀率的因素[J].有色金属:冶炼部分,2011(9):44-46. 被引量:2

5张迎春.由“计划进度分析”引发对生产均衡性问题的思考[J].上海统计,2002(6):42-43.

6昝苗苗,何志宏,曾昕鸣,陈金发,肖燕飞.机械球磨法在稀土材料制备领域的研究进展[J].有色金属科学与工程,2023,14(4):580-586.

1储向峰,汤丽娟,董永平,乔红斌,朱小华.锇在醋酸体系抛光液中化学机械抛光研究[J].金刚石与磨料磨具工程,2012,32(4):31-36.

2智红梅,蒋清民,陈金身,董德胜,郭钰龙.氧化铝-氧化铈核/壳复合磨料的性能测定[J].金刚石与磨料磨具工程,2013,33(2):72-75. 被引量:1

3杜晓冉,智红梅,陈金身,董德胜,王梅英.氧化铝-氧化铈核/壳复合磨粒的研究[J].金刚石与磨料磨具工程,2013,33(3):75-78. 被引量:2

4王波.A New Method for the Ultra-smooth Machining of the Silicon Based Materials[J].武汉理工大学学报:材料科学英文版,2009,0(S1):244-246.

5张逸飞.化学机械磨削技术发展历程及现状[J].航空精密制造技术,2013,49(3):26-28. 被引量:1

6李学舜,谢兵,杨国胜,吴文远,涂赣峰.稀土抛光粉颜色的测定及影响因素[J].稀土,2007,28(1):34-37. 被引量:1

7谢兵,任慧平,李学舜.稀土抛光粉颜色的表征及影响因素研究[J].包钢科技,2007,33(3):14-16. 被引量:2

8修树东,倪忠进,陈茂军.化学机械抛光的研究进展[J].机械研究与应用,2008,21(6):10-13. 被引量:4

9吴文远,李学舜,陈杰,杨国胜,涂赣峰.Effect of Roasting Conditions of Rich Cerium Rare Earth Carbonate on Crystallite Morphology and Polishing Ability of Ceria-Based Rare Earth Oxide[J].稀土学报:英文版,2007,0(S1):125-128. 被引量:2

10肖强,李言,李淑娟.SiC单晶片加工技术的发展[J].新技术新工艺,2009(6):91-94.

1李春鸿.从稀土残渣中回收重稀土[J].稀土信息,1997,3(Z1):22-22.

2ZhangWen-sheng.用SO2/O2从钴和镍溶液中氧化沉淀锰[J].铀矿冶,2002,21(4):219-219.

3任峰.近期国内稀土产品市场参考价[J].稀土信息,1993(9):14-14.

4周新木,阮桑桑,王爱勤,李永绣.钽铌沉淀母液制备含氟稀土产品的研究[J].稀有金属,2016,40(12):1276-1281.

5郝仕油.超细CeO2的微波辅助加热合成及其抛光性能[J].无机化学学报,2008,24(6):1012-1016. 被引量:5

6王金超,陈厚生.多聚钒酸铵沉淀条件的研究[J].钢铁钒钛,1993,14(2):28-32. 被引量:17

7顾楠.稀土关税取消之后[J].中国有色金属,2015,0(18):42-43. 被引量:1

8殷国平,苏英豪,邱鹏逵.光学玻璃用钼棒电极的研制[J].上海钢研,1993(3):13-17.

9李永绣,程昌明,陈伟凡,胡建东,周雪珍,胡平贵,辜子英,周新木.水合醋酸铈直接热分解制备超细氧化铈及其抛光性能[J].无机化学学报,2006,22(4):733-737. 被引量:7

10兰可.包钢稀土:行业领军 受益整合并购[J].中国金属通报,2008,0(19):19-21.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.25[冶金工程—粉末冶金]

Citation Information:

The ultra-fine CeO2 precursor for optical glass polishing material was prepared by selective oxidation and precipitation, washing, drying and calcination from low-cerium complex rare earth chlorides solution with NH3.H2O as precipitator, air and H2O2 as oxidative agent.The effect of reaction conditions and feeding mode on the content of CeO2 in precursor,and the correlativity between calcination temperature and particle size,specific surface area and mineralogical composition of precursor powder were investigated.The results show that by forward dripping, pH value controlled within 4.5 and 5.5,Ce3+ can be oxidized into Ce4+ to form hydroxide precipitant,followed by separation with other RE ions the ultra-fine polishing powder and precipitation before calcinations at 600~700 ℃ to obtain ultra-fine CeO2 precursor with CeO2 content over 80%,median particle size D50 less than 1.5 μm.

quote

GB/T 7714-2015 [1] LI Jin, HE Xiao-bin, GU Zi-ying, et al. Preparation of Ultra-fine CeO_2 Precursor for Optical Glass Polishing Material[J]. Rare Metals and Cemented Carbides, 2003(3): 1-4.
MLA [1] LI Jin, et al., "Preparation of Ultra-fine CeO_2 Precursor for Optical Glass Polishing Material." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 1-4.
APA [1] LI Jin, HE Xiao-bin, GU Zi-ying, HU Ping-gui, PENG De-yuan, & LI Yong-xiu. (2003). Preparation of Ultra-fine CeO_2 Precursor for Optical Glass Polishing Material. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] LI Jin, HE Xiao-bin, GU Zi-ying, HU Ping-gui, PENG De-yuan, and LI Yong-xiu, "Preparation of Ultra-fine CeO_2 Precursor for Optical Glass Polishing Material," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2003. keywords: {ultrafine CeO2;precursor;polishing material}