daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fluorinated Poly(ionic liquid) Copolymers as Transparent, Strong, and Versatile Adhesive Materials AITranslate

P. R. China|University of Science and Technology of China; The Chinese University of Hong Kong; The Chinese University of Hong Kong; P. R. China|University of Science and Technology of China; P. R. China|University of Science and Technology of China; The Chinese University of Hong Kong; The Chinese University of Hong Kong; The Chinese University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Poly(ionic liquid)s (PILs), combining the advantages of both polymers and ionic liquids, have attracted significant attention from the academia and industry. This study has developed a fluorinated PIL copolymer-based adhesive with versatile adhesion ability and high transparency. The adhesive was prepared by in situ UV-curing a precursor solution composed of commercially available monomers, that is, 2,2,3,4,4,4-hexafluorobutyl methacrylate and 1-vinyl-3-butylimidazolium bis(trifluoromethylsulfonyl)imide. The prepared adhesive showed a superior adhesion strength of 6.61 MPa toward glass substrates. Furthermore, minimal addition of a plasticizer in the bulk adhesive could significantly enhance the adhesion performance on fluorinated polymer substrates while maintaining the polar surface bonding strength and high transparency. The resulting PIL-based adhesive showed a strong adhesion on various adherends, such as glass, steel, ceramics, and low surface energy polymers. This work provides a methodology for using PILs as adhesives and is believed to have good potential for commercialization.

KeyWords AITranslate

adhesive fluorinated monomer ion−dipole interaction low surface energy poly(ionic liquid)s toughness
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01785

Chinese Library Classification Number:

Citation Information:

Poly(ionic liquid)s (PILs), combining the advantages of both polymers and ionic liquids, have attracted significant attention from the academia and industry. This study has developed a fluorinated PIL copolymer-based adhesive with versatile adhesion ability and high transparency. The adhesive was prepared by in situ UV-curing a precursor solution composed of commercially available monomers, that is, 2,2,3,4,4,4-hexafluorobutyl methacrylate and 1-vinyl-3-butylimidazolium bis(trifluoromethylsulfonyl)imide. The prepared adhesive showed a superior adhesion strength of 6.61 MPa toward glass substrates. Furthermore, minimal addition of a plasticizer in the bulk adhesive could significantly enhance the adhesion performance on fluorinated polymer substrates while maintaining the polar surface bonding strength and high transparency. The resulting PIL-based adhesive showed a strong adhesion on various adherends, such as glass, steel, ceramics, and low surface energy polymers. This work provides a methodology for using PILs as adhesives and is believed to have good potential for commercialization.

quote

GB/T 7714-2015 [1] Shuaishuai Huang, Yichen Wan, Yuxuan Sun, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01785.
MLA [1] Shuaishuai Huang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01785.
APA [1] Shuaishuai Huang, Yichen Wan, Yuxuan Sun, Kaka Zhang, Xiaoqing Ming, He Zhu, Qi Zhang, & Shiping Zhu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01785
IEEE [1] Shuaishuai Huang, Yichen Wan, Yuxuan Sun, Kaka Zhang, Xiaoqing Ming, He Zhu, Qi Zhang, and Shiping Zhu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01785. keywords: {adhesive;fluorinated monomer;ion−dipole interaction;low surface energy;poly(ionic liquid)s;toughness}