Abstract AITranslate
Flexible piezoresistive sensors have been widely used in the fields of wearable electronic devices, electronic skin, intelligent human–computer interaction, health monitoring, life medicine research, intelligent robot, and so on. However, how to find a balance between stability, sensitivity, and sensing range, especially under the low-pressure range, is still an immediate challenge waiting to be solved. Herein, a highly flexible and compressible aerogel with a smooth layer structure was successfully fabricated by combining Ag nanowires into poly(3,4-ethylenedioxythiophene):polystyrene sulfonate and polyimide composites by casting and thermal annealing. As a result, the elastic aerogel with large reversible compressibility exhibited a good compression sensitivity of 0.31 kPa–1 in the pressure range of 0–1.25 kPa, high linearity of compression strain and resistance change rate, great fatigue resistance (height retention of 98–99% at 1000% strain/min), and large reversible compressibility (height retention of 90% after 200 compression cycles). The excellent performance of conductive aerogels shows their promising potential in the field of piezoelectric sensing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01765
Chinese Library Classification Number:
Citation Information:
Flexible piezoresistive sensors have been widely used in the fields of wearable electronic devices, electronic skin, intelligent human–computer interaction, health monitoring, life medicine research, intelligent robot, and so on. However, how to find a balance between stability, sensitivity, and sensing range, especially under the low-pressure range, is still an immediate challenge waiting to be solved. Herein, a highly flexible and compressible aerogel with a smooth layer structure was successfully fabricated by combining Ag nanowires into poly(3,4-ethylenedioxythiophene):polystyrene sulfonate and polyimide composites by casting and thermal annealing. As a result, the elastic aerogel with large reversible compressibility exhibited a good compression sensitivity of 0.31 kPa–1 in the pressure range of 0–1.25 kPa, high linearity of compression strain and resistance change rate, great fatigue resistance (height retention of 98–99% at 1000% strain/min), and large reversible compressibility (height retention of 90% after 200 compression cycles). The excellent performance of conductive aerogels shows their promising potential in the field of piezoelectric sensing.
quote
| GB/T 7714-2015 | [1] Jiangnan Wang, Xueying Yue, Xiuting Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01765. |
| MLA | [1] Jiangnan Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01765. |
| APA | [1] Jiangnan Wang, Xueying Yue, Xiuting Li, Jie Dong, Qinghua Zhang, & Xin Zhao. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01765 |
| IEEE | [1] Jiangnan Wang, Xueying Yue, Xiuting Li, Jie Dong, Qinghua Zhang, and Xin Zhao, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01765. keywords: {polyimide;PEDOT/PSS;silver nanowire;aerogel;piezoresistive;sensors} |