daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Performance Conductive Polymer Composites by Incorporation of Polyaniline-Wrapped Halloysite Nanotubes and Silver Microflakes AITranslate

Southern University of Science and Technology; Southern University of Science and Technology; Harbin Institute of Technology; Southern University of Science and Technology; Southern University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conductive polymer composites (CPCs) with high conductivity and flexibility play a crucial role in emerging flexible electronics. However, the facile fabrication of high-performance flexible conductors is still challenging due to cumbersome manufacturing steps and the need for expensive metal nanomaterials as conductive fillers. Herein, we presented a facile and cost-effective method to prepare CPCs with an ultralow resistivity of 2.4 × 10–5 Ω·cm at 60% silver micronflakes. The elastic CPCs are simply composed of conductive cofillers of commercial silver micronflakes and polyaniline/halloysite nanotubes (PANI/HNTs) and water-based polyurethane (WPU) resin as the matrix. With a delicate design, the PANI/HNTs could locate adjacent silver micronflakes in the WPU resin and form conducting paths to improve the electrically conductive performance of the composites significantly. Thus, the CPCs serve as flexible conductors showing high conductivity and excellent stability during numerous cyclic mechanical deformations, such as bending, stretching, twisting, and folding. These advantages make the valuable materials candidates for the next generation of flexible conductors.

KeyWords AITranslate

conductive polymer composites polyaniline halloysite nanotubes silver microflakes flexible conductors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01929

Chinese Library Classification Number:

Citation Information:

Conductive polymer composites (CPCs) with high conductivity and flexibility play a crucial role in emerging flexible electronics. However, the facile fabrication of high-performance flexible conductors is still challenging due to cumbersome manufacturing steps and the need for expensive metal nanomaterials as conductive fillers. Herein, we presented a facile and cost-effective method to prepare CPCs with an ultralow resistivity of 2.4 × 10–5 Ω·cm at 60% silver micronflakes. The elastic CPCs are simply composed of conductive cofillers of commercial silver micronflakes and polyaniline/halloysite nanotubes (PANI/HNTs) and water-based polyurethane (WPU) resin as the matrix. With a delicate design, the PANI/HNTs could locate adjacent silver micronflakes in the WPU resin and form conducting paths to improve the electrically conductive performance of the composites significantly. Thus, the CPCs serve as flexible conductors showing high conductivity and excellent stability during numerous cyclic mechanical deformations, such as bending, stretching, twisting, and folding. These advantages make the valuable materials candidates for the next generation of flexible conductors.

quote

GB/T 7714-2015 [1] Ge Cao, Shaoyong Cai, He Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01929.
MLA [1] Ge Cao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01929.
APA [1] Ge Cao, Shaoyong Cai, He Zhang, Yonghao Chen, & Yanqing Tian. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01929
IEEE [1] Ge Cao, Shaoyong Cai, He Zhang, Yonghao Chen, and Yanqing Tian, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01929. keywords: {conductive polymer composites;polyaniline;halloysite nanotubes;silver microflakes;flexible conductors}