Abstract AITranslate

Visible light-regulated organocatalytic polymerization has attracted considerable attention in recent years due to its mild, metal-free reaction conditions and the capability of mediating polymerization with spatial and temporal controls. Here, we report the successful identification of hydroxybenzophenones (BPOHs) as an effective class of photoacid catalysts for the ring-opening polymerization of lactones, which could afford biodegradable polyester products with predictable molecular mass and low dispersity under the irradiation of visible light.

KeyWords AITranslate

visible light organocatalysis ringopening polymerization polyesters hydroxybenzophenones
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01931

Chinese Library Classification Number:

Citation Information:

Visible light-regulated organocatalytic polymerization has attracted considerable attention in recent years due to its mild, metal-free reaction conditions and the capability of mediating polymerization with spatial and temporal controls. Here, we report the successful identification of hydroxybenzophenones (BPOHs) as an effective class of photoacid catalysts for the ring-opening polymerization of lactones, which could afford biodegradable polyester products with predictable molecular mass and low dispersity under the irradiation of visible light.

quote

GB/T 7714-2015 [1] Siping Hu, Jianxu Chen, Xun Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01931.
MLA [1] Siping Hu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01931.
APA [1] Siping Hu, Jianxu Chen, Xun Zhang, Yuying Zhang, & Saihu Liao. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01931
IEEE [1] Siping Hu, Jianxu Chen, Xun Zhang, Yuying Zhang, and Saihu Liao, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01931. keywords: {visible light;organocatalysis;ringopening polymerization;polyesters;hydroxybenzophenones}