Fabrication Approaches of Soft Electronics Fabrication Approaches of Soft Electronics AITranslate

Nanyang Technological University; The Hebrew University of Jerusalem; The Hebrew University of Jerusalem; The Hebrew University of Jerusalem
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The use of conductive materials to be printed/embedded onto/within a polymeric matrix has gained increasing attention in the fabrication of next-generation soft electronics. In this review, we provide a comprehensive overview of the materials and approaches for the fabrication of 2D and 3D conductive structures while focusing on the importance of the compatibility between the particles’ shape, the polymeric matrix type, and the deposition method, along with the target application. The review presents a summary of the main conductive materials and the type of polymeric materials which were utilized for fabricating soft electronic devices that are bendable/twistable and stretchable. It is divided into two sections: Introduction section, which presents briefly conductive materials, polymeric matrix, and fabrication methods, and Fabrication section, presenting the main 6 approaches of fabrication. Each of the fabrication subsections presents the main recent reports in a detailed table. The review is concluded with an Outlook section, describing the current challenges in this field. Despite the progress in the fabrication of 2D bendable/twistable electronic devices toward industrial integration, there is still a need for tailoring and improving the durability and robustness of 3D stretchable electronic devices.

KeyWords AITranslate

printed electronics soft electronics soft sensors 2D printed sensors 3D printed sensors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01728

Chinese Library Classification Number:

Citation Information:

The use of conductive materials to be printed/embedded onto/within a polymeric matrix has gained increasing attention in the fabrication of next-generation soft electronics. In this review, we provide a comprehensive overview of the materials and approaches for the fabrication of 2D and 3D conductive structures while focusing on the importance of the compatibility between the particles’ shape, the polymeric matrix type, and the deposition method, along with the target application. The review presents a summary of the main conductive materials and the type of polymeric materials which were utilized for fabricating soft electronic devices that are bendable/twistable and stretchable. It is divided into two sections: Introduction section, which presents briefly conductive materials, polymeric matrix, and fabrication methods, and Fabrication section, presenting the main 6 approaches of fabrication. Each of the fabrication subsections presents the main recent reports in a detailed table. The review is concluded with an Outlook section, describing the current challenges in this field. Despite the progress in the fabrication of 2D bendable/twistable electronic devices toward industrial integration, there is still a need for tailoring and improving the durability and robustness of 3D stretchable electronic devices.

quote

GB/T 7714-2015 [1] Joel Ming Rui Tan, Yousef Farraj, Alexander Kamyshny, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01728.
MLA [1] Joel Ming Rui Tan, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01728.
APA [1] Joel Ming Rui Tan, Yousef Farraj, Alexander Kamyshny, & Shlomo Magdassi. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01728
IEEE [1] Joel Ming Rui Tan, Yousef Farraj, Alexander Kamyshny, and Shlomo Magdassi, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01728. keywords: {printed electronics soft electronics soft sensors 2D printed sensors 3D printed sensors}