Photocurrent Polarity Switching and Enhanced Photoresponse in Silver Nanoparticles Decorated a-GaN-Based Photodetector Photocurrent Polarity Switching and Enhanced Photoresponse in Silver Nanoparticles Decorated a-GaN-Based Photodetector AITranslate
Abstract AITranslate
The photodetection properties of a-GaN nanorods-based photodetector and the effect of decorating silver nanoparticles are reported. For the pristine a-GaN detector, a surprising phenomenon of negative photoconductivity is observed, explained on the basis of defect states present in GaN nanorods. After the introduction of nanoparticles, the device exhibits reversal in the photocurrent polarity. The photoresponsivity reverses its sign from −0.12 A/W (bare a-GaN) to +6.75 A/W, with the introduction of nanoparticles (wavelength: 355 nm, 4.9 V bias). This current reversal and enhanced performance have been rationalized by considering passivation of surface defect states, resulting into significantly reduced dark current in the hybrid detector.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01549
Chinese Library Classification Number:
Citation Information:
The photodetection properties of a-GaN nanorods-based photodetector and the effect of decorating silver nanoparticles are reported. For the pristine a-GaN detector, a surprising phenomenon of negative photoconductivity is observed, explained on the basis of defect states present in GaN nanorods. After the introduction of nanoparticles, the device exhibits reversal in the photocurrent polarity. The photoresponsivity reverses its sign from −0.12 A/W (bare a-GaN) to +6.75 A/W, with the introduction of nanoparticles (wavelength: 355 nm, 4.9 V bias). This current reversal and enhanced performance have been rationalized by considering passivation of surface defect states, resulting into significantly reduced dark current in the hybrid detector.
quote
| GB/T 7714-2015 | [1] Deependra Kumar Singh, Pukhraj Prajapat, Jyoti Saroha, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01549. |
| MLA | [1] Deependra Kumar Singh, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01549. |
| APA | [1] Deependra Kumar Singh, Pukhraj Prajapat, Jyoti Saroha, Rohit Kumar Pant, Shailesh Narain Sharma, Karuna Kar Nanda, Saluru Baba Krupanidhi, & Govind Gupta. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01549 |
| IEEE | [1] Deependra Kumar Singh, Pukhraj Prajapat, Jyoti Saroha, Rohit Kumar Pant, Shailesh Narain Sharma, Karuna Kar Nanda, Saluru Baba Krupanidhi, and Govind Gupta, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01549. keywords: {aGaN nanorods Ag nanoparticles photodetection polarity switching defect passivation} |