Determination of Oxygen in Doped Tungsten Powder by Pulse Heating Coulomb Testing AITranslate
Abstract AITranslate
Study is made on the condition and analysis method for oxygen determination from doped tungsten powder by pulse heating coulomb testing.The results indicated that the analytical heating temperature of doped tungsten powder controlled by heating current can be identical with that of the tungsten powder.Normally,the heating current is 750~800 A,analysis carrier gas flowrate is 150 mL/min.The flux should be wrapped by Ni-foil.The relative standard deviation is 2%.The method is applicable for production analysis.
KeyWords AITranslate
1张文朴.几种含钨精细化学品与无机非金属材料[J].中国钨业,1995,0(3):7-11. 被引量:3
2罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14
3庞广兴.储存时间对碳化钨粉的影响[J].稀有金属与硬质合金,1990(3):6-11. 被引量:1
4裘立奋,王水法.硬质材料和难熔金属气体分析进展[J].硬质合金,1999,16(2):109-113. 被引量:7
1朱跃进.金属中气体分析现状与未来[J].冶金分析,2014,34(3):19-23. 被引量:12
2郭飞飞,张文,费婷,侯红霞,李宏伟.脉冲熔融-惰气保护红外法测定铁硅合金中的氧含量[J].广州化工,2016,44(22):104-106. 被引量:3
3刘攀,杜丽丽,唐伟,李治亚.无机固态材料中气体元素分析的现状与进展[J].理化检验:化学分册,2015,51(1):131-136. 被引量:9
1朱跃进,徐磊,吴杰,郭瑞鹏,代春丽,杨锐.钛基合金中氩的分析探讨及应用[J].冶金分析,2015,35(3):13-18. 被引量:2
2刘攀,聂富强.手动加样-惰气熔融-热导法测定氮化铬铁含氮量[J].化学工程师,2015,29(6):36-38. 被引量:1
3徐敏秀,何莉,姚凤花,袁凯笛,杨君,蒋威.高频燃烧红外吸收法测定硅粉中总碳[J].冶金分析,2015,35(9):25-31. 被引量:1
4刘攀,聂富强,董俊轩.Top-down技术评估钢中氧的测量不确定度[J].福建分析测试,2015,24(6):38-44. 被引量:7
5刘文玖.钢铁材料中氧氮氢的测定分析[J].世界有色金属,2015,40(12):53-54. 被引量:2
6钟华.钢中氧氮氢同时测定方法中氢空白值的控制[J].冶金分析,2016,36(5):12-15. 被引量:3
7王晓旋,卜兆杰,黄健强,李文新.惰气熔融-红外热导法测定12Cr_2Mo_1R焊缝金属中氧氮氢[J].冶金分析,2017,37(7):63-67. 被引量:6
8蒋亚芳.ONH836分析仪同时测定钽制品中氧、氮、氢含量研究[J].硬质合金,2017,34(6):429-435. 被引量:6
9孙海峰,周海收,陈彩霞.惰性气体熔融-热导法测定硅材料中的氧[J].化学分析计量,2018,27(5):48-50. 被引量:1
10谢君,朱瑛才,仉凤江,张琳,朱跃进.坩埚对高温合金中氧氮及氢分析结果的影响[J].冶金分析,2018,38(10):7-15. 被引量:9
1刘莹晶.火焰原子吸收光谱法测定镉锭中的铁[J].湖南有色金属,2009,25(3):63-65. 被引量:1
2师世龙.XRF法测定锌合金中的铝[J].光谱实验室,2006,23(1):96-98. 被引量:3
3胡少成,葛程,马红权,王超刚,胡学强,马飞超,王蓬.脉冲加热-红外吸收热导法同时测定钢铁材料中氧和氢[J].冶金分析,2014,34(4):37-41. 被引量:10
4张明明,田晓露,关永毅.气相色谱法快速测定间甲酚含量[J].燃料与化工,2011,42(6):50-51. 被引量:8
5钟华.脉冲加热-红外吸收光谱法测定钒铝合金中氢[J].中国无机分析化学,2013,3(2):56-59. 被引量:11
6徐本平,李晖.钒氮合金中的高含量氮的测定[J].冶金分析,2004(z1):358-360. 被引量:2
7陈文宾,许兴友,马卫兴,李艳辉.在CTMAB存在下用2-羟基-5磺酸基苯基重氮氨基偶氮苯光度法测定铟[J].理化检验:化学分册,2007,43(5):367-368. 被引量:4
8沈英姬.脉冲加热惰性气体熔融红外吸收-热导法测定镍基高温合金中痕量氧、氮[J].山东化工,2015,44(12):64-66. 被引量:4
9张瑞霖,郭燕青,梁敏鉴.脉冲加热熔融热导法测定钛铁合金中氮含量[J].冶金分析,2010,31(8):25-29. 被引量:3
10李青,雷清如,朱育胜,陈精强,范广智,徐本平.脉冲加热气相色谱法测定高钛型炉渣中的氮[J].分析试验室,1989,8(6):26-27. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:O657.12[理学—分析化学]
Citation Information:
Study is made on the condition and analysis method for oxygen determination from doped tungsten powder by pulse heating coulomb testing.The results indicated that the analytical heating temperature of doped tungsten powder controlled by heating current can be identical with that of the tungsten powder.Normally,the heating current is 750~800 A,analysis carrier gas flowrate is 150 mL/min.The flux should be wrapped by Ni-foil.The relative standard deviation is 2%.The method is applicable for production analysis.
quote
| GB/T 7714-2015 | [1] HE Ying. Determination of Oxygen in Doped Tungsten Powder by Pulse Heating Coulomb Testing[J]. Rare Metals and Cemented Carbides, 2010(2): 62-63. |
| MLA | [1] HE Ying. "Determination of Oxygen in Doped Tungsten Powder by Pulse Heating Coulomb Testing." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 62-63. |
| APA | [1] HE Ying. (2010). Determination of Oxygen in Doped Tungsten Powder by Pulse Heating Coulomb Testing. Rare Metals and Cemented Carbides(2), 62-63. |
| IEEE | [1] HE Ying, "Determination of Oxygen in Doped Tungsten Powder by Pulse Heating Coulomb Testing," Rare Metals and Cemented Carbides, no. 2, pp. 62-63, 2010. keywords: {doped tungsten powder;oxygen content;pulse-heating;coulomb-oxygen testing} |