Brief Introduction to Wet Milling-spray Drying Granulation Process for the Cemented Carbide Mixture AITranslate

Changsha Nonferrous Metallurgical Design Research Institute;Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Brief introduction is made to the wet milling-spray drying granulation technology and equipment with analysis made of the main factors affecting the mixture quality in the blending,wet milling,spray drying granulation operations.The main techno-economic indices are evaluated.

KeyWords AITranslate

cemented carbide mixture wet milling-spray drying granulation process influence factor techno-economic index

1张立,陈述,刘刚,杨贵彬,黄泽兰,黄伯云,张传福.高性能超细、纳米硬质合金及其制备过程中的关键技术问题[J].材料导报,2005,19(11):4-7. 被引量:21

2卓海宇,卓萍.硬质合金混合料制备过程中的质量控制[J].湖南理工学院学报:自然科学版,2004,17(4):68-70. 被引量:5

3徐涛,李学芳.湿磨—喷雾干燥工艺混合料生产中的质量控制及其特点[J].硬质合金,2000,17(4):221-224. 被引量:4

4梁志刚,任小洪.PWG-300型喷雾干燥设备的研制[J].硬质合金,2005,22(4):221-225. 被引量:3

5陈楚轩.硬质合金质量控制原理[Z].自贡:中国钨业协会硬质合金分会(自贡硬质合金有限责任公司),2008.3-26.

1彭文,邓涛.硬质合金先进技术在大规格顶锤制造中的应用[J].超硬材料工程,2013,25(1):25-29. 被引量:5

2赵丽丽,张严,许鹏飞,吕豫湘,冯文.硬质合金混合料粒度分布对成型尺寸精度的影响[J].硬质合金,2018,35(5):344-350. 被引量:3

3袁康,张洪刚.混合料大小批研磨效率差异的影响因素研究[J].稀有金属与硬质合金,2018,46(3):75-79. 被引量:1

4王慧群,彭晖,石丽秋.研磨体形状对亚细晶硬质合金混合料研磨效率及合金性能的影响[J].四川冶金,2019,41(3):37-41.

5朱二涛,张久兴,杨新宇,羊建高,潘亚飞.金相分析在YG类硬质合金中的应用[J].中国钨业,2019,34(2):50-66. 被引量:1

1彭文,舒军.硬质合金Ф160mm以上超大顶锤的现状与发展[J].超硬材料工程,2014,26(2):11-17. 被引量:3

2张忠健,赵声志,彭文,张倩霞,陈鼎.硬质合金疲劳裂纹的萌生与扩展行为[J].中国有色金属学报,2014,24(12):3031-3041. 被引量:19

3彭文,彭伟,孔德方.国产无压机分球式超高压装置用硬质合金顶锤的研究[J].金刚石与磨料磨具工程,2016,36(1):50-56. 被引量:2

4冯文,袁彩云,赵丽丽,宁华林,何莹.一种双面负角铣削刀片模具补偿设计方法的研究[J].硬质合金,2019,36(3):221-227. 被引量:1

5唐炜,肖颖奕,杨树忠,张帆,文小强,许洋.超细晶硬质合金混合料的球磨混料机制[J].中国钨业,2019,34(4):47-54.

6刘文彬,陈飞雄,裴新军,熊宁,王铁军.大尺寸亚微米硬质合金顶锤的热等静压研制[J].稀有金属与硬质合金,2020,48(2):82-89. 被引量:1

7周永川,吴献军,谢州.FeSiCr磁粉心造粒粒径分布对其性能的影响[J].粉末冶金工业,2021,31(5):61-65.

8郭宏海.硬质合金棒料上的两条裂纹有何影响——仿真分析告诉你[J].金属世界,2023(2):1-6.

9冯克明,王庆伟,杜晓旭,贾伟民,夏学锋.四柱压机的精密压制技术[J].金刚石与磨料磨具工程,2023,43(3):298-304.

10廖英杰,刘岩岩,熊德树,张柯.石墨烯对气压烧结WC-Co硬质合金性能的影响[J].有色金属材料与工程,2023,44(4):42-51.

1徐涛,李学芳.湿磨—喷雾干燥工艺混合料生产中的质量控制及其特点[J].硬质合金,2000,17(4):221-224. 被引量:4

2石怀涛.铟精炼工艺的改进[J].南方金属,2008(4):50-53.

3李长岫.用火焰原子吸收光谱法研究球磨过程中带入杂质Fe、Co、Ni的含量变化[J].粉末冶金技术,1993,11(4):295-297.

4梁志刚,任小洪.PWG-300型喷雾干燥设备的研制[J].硬质合金,2005,22(4):221-225. 被引量:3

5潘俊新,邓凯,陈列湘.硬质合金混合料脏化分析[J].硬质合金,1997,14(2):82-86. 被引量:8

6吴向忠.硬质合金混合料制备系统工艺及设备的改进[J].稀有金属与硬质合金,2001,29(1):57-60. 被引量:2

7高培明,尹涛,薛卫.硬质合金类烟机配件的性能改善[J].中国材料科技与设备,2009,6(2):75-77. 被引量:3

8林河成.中国稀土永磁材料的高速发展及前景[J].四川有色金属,2007(3):14-21. 被引量:7

9粟一峰,伏坤,李行,孙五四,周建华.纯水作湿磨介质对WC-Co硬质合金性能的影响[J].稀有金属与硬质合金,2015,43(6):65-68. 被引量:2

10吴德强,黄波,沈继刚.一套典型的宽厚板轧机生产工艺及设备[J].钢铁技术,2008(1):19-23.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.11[冶金工程—粉末冶金]

Citation Information:

Brief introduction is made to the wet milling-spray drying granulation technology and equipment with analysis made of the main factors affecting the mixture quality in the blending,wet milling,spray drying granulation operations.The main techno-economic indices are evaluated.

quote

GB/T 7714-2015 [1] CUI Jia-na, CHEN Qi-ming. Brief Introduction to Wet Milling-spray Drying Granulation Process for the Cemented Carbide Mixture[J]. Rare Metals and Cemented Carbides, 2010(2): 57-61.
MLA [1] CUI Jia-na, and CHEN Qi-ming. "Brief Introduction to Wet Milling-spray Drying Granulation Process for the Cemented Carbide Mixture." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 57-61.
APA [1] CUI Jia-na, & CHEN Qi-ming. (2010). Brief Introduction to Wet Milling-spray Drying Granulation Process for the Cemented Carbide Mixture. Rare Metals and Cemented Carbides(2), 57-61.
IEEE [1] CUI Jia-na and CHEN Qi-ming, "Brief Introduction to Wet Milling-spray Drying Granulation Process for the Cemented Carbide Mixture," Rare Metals and Cemented Carbides, no. 2, pp. 57-61, 2010. keywords: {cemented carbide mixture;wet milling-spray drying;granulation;process;influence factor;techno-economic index}