daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Synthesis and Electrochemical Properties of Rare Earth Ce-doped LiFePO_4 Cathode Material AITranslate

School of Mechanical and Electrical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China Shaanxi Key Laboratory of Nano Materials and Technology;School of Mechanical and Electrical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China Shaanxi Key Laboratory of Nano Materials and Technology;School of Mechanical and Electrical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China Shaanxi Key Laboratory of Nano Materials and Technology;School of Mechanical and Electrical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China Shaanxi Key Laboratory of Nano Materials and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

. LiFe1-xCex PO4/C (x= 0,0. 01,0. 03,0. 05) cathode material doped with rare earth Ce was syn- thesized with hydrothermal method. The electrochemical properties of the prepared material were studied by a series of systematic tests. XRD results show that the olivine crystal structure of LiFePO4 stays the same after doping 1 %- 5 % Ce, but cell volume is extended, which is favorable for the Li+ extraction-inser- tion. The SEM images further demonstrate that doping rare earth Ce can refine the grain size,and then ef- fectively reduce Li+ diffusion and migration pathway. In the potential range of 2. 044.0 V,the initial dis- charge specific capacity of LiFe1-xCexPO4/C at the discharge rate of 0.1C firstly increases and then decrea- ses with Ce dosage increasing,and it reaches the maximum value of 144.1 mA /g at x= 0. 03 , increased by 17.4% compared with the undoped LiFePO4/C. And its capacity retention ratio is 95.0% after 50 cy- cles. CV and EIS measurements show that LiFe1-xCexPO4/C (x=0.03) has the lowest charge transfer re- sistance,and the redox peak of the sample remains visible after 50 cycles at the charge and discharge rate of 0.1C,demonstrating that the sample has stable structure and good reversible reaction performance.

KeyWords AITranslate

lithium-ion battery cathode material LiFePO4 Ce rare earth doping electrochemical property

1陈晗,向楷雄,龚文强,刘建华.稀土金属离子掺杂对LiFePO_4结构和性能的影响[J].稀有金属材料与工程,2011,40(11):1936-1940. 被引量:4

2张秋明,乔玉卿,赵敏寿,王立民.稀土Sm掺杂LiFePO4/C正极材料的结构和电化学性能[J].无机化学学报,2012,28(1):67-73. 被引量:8

3白咏梅,陈晗,邱鹏,文中流,韩绍昌.Er^(3+)掺杂LiFePO_4正极材料的制备与性能[J].湖南大学学报:自然科学版,2010,37(6):57-60. 被引量:2

4张丽,赵敏寿,王丹丹,沙鸥,邓瑞平,孟健.Nd^(3+)掺杂对LiFePO_4结构及电化学性能的改善[J].无机化学学报,2009,25(10):1724-1728. 被引量:3

5田彦文,康晓雪,刘丽英,徐茶青,曲涛.Research on cathode material of Li-ion battery by yttrium doping[J].稀土学报:英文版,2008,26(2):279-283. 被引量:14

6习小明,王双才,湛中魁,胡常波.Li^+、La^(3+)掺杂对尖晶石LiMn_2O_4的电化学性能影响[J].矿冶工程,2009,29(6):85-88. 被引量:4

7邓斌,阎杰,张朝帅.LiCoO_2掺杂稀土元素研究[J].电池,2003,33(2):74-76. 被引量:19

8魏进平,曹晓燕,潘桂玲,叶茂,阎杰.Rare Earth Elements-Doped LiCoO_2 Cathode Material for Lithium-Ion Batteries[J].稀土学报:英文版,2003,21(4):466-468. 被引量:6

9武聪,罗绍华,田勇,唐子龙,张中太.稀土铈掺杂LiFePO_4正极材料的电化学性能研究[J].硅酸盐通报,2009,28(B08):153-156. 被引量:15

10侯娟,殷保祥,刘国明,张清龙,王帆.Ce^(4+)掺杂对LiFePO_4/C正极材料微观结构和性能的影响[J].电子元件与材料,2011,30(7):32-34. 被引量:6

1陈瑞强.稀土掺杂锂离子电池正极材料的研究进展[J].世界有色金属,2021(8):107-109.

2宋欣美,邱杰.金属铂-稀土合金电催化剂的制备研究[J].中国石油和化工标准与质量,2018,38(7):81-82.

1王国诚.吉林橄榄石简介[J].珠宝,1992(1):48-48. 被引量:1

2Mey.,HOA,王五一.金刚石中的包裹体[J].国外矿床地质,1991(4):72-98. 被引量:1

3杨富绪,刘树忠.中国橄榄石[J].中国宝石,1993(4):12-13.

4王力臻,江庆,高可政,方华.超高压处理前驱体对LiFePO_4/C性能的影响[J].电池,2017,47(4):193-195.

5董振信.山东金伯利岩中榄橄石的研究[J].岩石矿物学杂志,1991,10(4):354-362. 被引量:5

6卢吉明,周盈科,田小慧.多孔LiFePO_4正极材料的研究进展[J].稀有金属材料与工程,2017,46(8):2327-2344. 被引量:2

7郝丽敏.锂离子电池正极材料LiFePO4研究现状及其改性方法[J].重庆航天职业技术学院学报,2017,0(3):49-56.

8李涛,刘毅.稀土Ce对7A04铝合金组织和力学性能的影响[J].铸造技术,2017,38(9):2080-2083. 被引量:4

9张文龙,白清,吴宏钧,陈丽.Co_3O_4/C混合包覆对LiMnPO_4正极材料电化学性能的影响[J].电源技术,2017,41(9):1255-1257. 被引量:1

10张冬,李亭亭,邱海龙,魏英进,王春忠,陈岗,岳惠娟.氮掺杂硅酸亚铁锂正极材料的制备及电化学性能[J].高等学校化学学报,2017,38(9):1633-1638. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]

Citation Information:

. LiFe1-xCex PO4/C (x= 0,0. 01,0. 03,0. 05) cathode material doped with rare earth Ce was syn- thesized with hydrothermal method. The electrochemical properties of the prepared material were studied by a series of systematic tests. XRD results show that the olivine crystal structure of LiFePO4 stays the same after doping 1 %- 5 % Ce, but cell volume is extended, which is favorable for the Li+ extraction-inser- tion. The SEM images further demonstrate that doping rare earth Ce can refine the grain size,and then ef- fectively reduce Li+ diffusion and migration pathway. In the potential range of 2. 044.0 V,the initial dis- charge specific capacity of LiFe1-xCexPO4/C at the discharge rate of 0.1C firstly increases and then decrea- ses with Ce dosage increasing,and it reaches the maximum value of 144.1 mA /g at x= 0. 03 , increased by 17.4% compared with the undoped LiFePO4/C. And its capacity retention ratio is 95.0% after 50 cy- cles. CV and EIS measurements show that LiFe1-xCexPO4/C (x=0.03) has the lowest charge transfer re- sistance,and the redox peak of the sample remains visible after 50 cycles at the charge and discharge rate of 0.1C,demonstrating that the sample has stable structure and good reversible reaction performance.

quote

GB/T 7714-2015 [1] ZHANG Yang, WANG Juan, WANG Liang-liang, et al. Study on Synthesis and Electrochemical Properties of Rare Earth Ce-doped LiFePO_4 Cathode Material[J]. Rare Metals and Cemented Carbides, 2017(4): 42-46.
MLA [1] ZHANG Yang, et al., "Study on Synthesis and Electrochemical Properties of Rare Earth Ce-doped LiFePO_4 Cathode Material." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 42-46.
APA [1] ZHANG Yang, WANG Juan, WANG Liang-liang, & XU Yun-hua. (2017). Study on Synthesis and Electrochemical Properties of Rare Earth Ce-doped LiFePO_4 Cathode Material. Rare Metals and Cemented Carbides(4), 42-46.
IEEE [1] ZHANG Yang, WANG Juan, WANG Liang-liang, and XU Yun-hua, "Study on Synthesis and Electrochemical Properties of Rare Earth Ce-doped LiFePO_4 Cathode Material," Rare Metals and Cemented Carbides, no. 4, pp. 42-46, 2017. keywords: {lithium-ion battery;cathode material;LiFePO4;Ce;rare earth doping;electrochemical property}