The evaporation behavior of metal cerium was analyzed and proper evaporation temperature was determined. And then design of the electromagnetic induction evaporation device and research of evapora- tion technology were carried out. Evaporation rate of metal cerium was measured, vapor density distribu- tion was analyzed with film thickness method, and vapor density was measured with weighing method. The results show that evaporation rate of metal cerium at 2 000 ℃ is about 99-135 g/h,and the measured val- ue is slightly lower than the theoretical value. The density distribution of cerium vapor approximately fol- lows the relationship of high order power of cosine function,and atomic vapor density magnitude is about 1011 atom/cm3. The application of electromagnetic induction heating evaporation for cerium film deposition is feasible.
KeyWords AITranslate
1戴春爱,刘博,颜鲁婷,刘莲云.铈作为环境材料的研究及应用[J].稀有金属材料与工程,2009,38(A01):357-360. 被引量:4
2孙小庆,魏峰,杨志民,陈秋云,陈军.高真空脉冲激光沉积CeO_2(111)/Si(111)薄膜的结构与形貌研究[J].稀有金属,2013,37(3):389-395. 被引量:8
3刘日新,戴永年,李本文,吴铧.纯金属真空蒸馏研究(Ⅰ):数学模型[J].真空科学与技术,1996,16(2):134-139. 被引量:3
4范凤英,高鹏,江涛.激光吸收光谱法实时监测原子蒸气密度[J].原子能科学技术,2012,46(6):726-729. 被引量:2
1吕绪明,马贤,何荧,罗立平,张晓卫.真空蒸发镀膜法制备金属铈薄膜的表征[J].稀有金属与硬质合金,2019,47(4):39-43. 被引量:2
2王淑婷,幸福堂,韩军,梅丹.常压条件下锌挥发特性及预测模型研究[J].工业安全与环保,2020,46(6):56-60.
1张秀艳,常诚,包香春,张慧珍,于亚辉.硅藻土负载TODGA分离-电感耦合等离子体质谱法测定氧化铈中氧化钆、氧化铽[J].理化检验:化学分册,2021,57(7):642-647.
2张健,牛夏斌,孟辉波,齐振华,李建浩.探究氧气流量对新型高阻隔薄膜材料的制备及性能的影响[J].真空科学与技术学报,2021,41(7):694-698. 被引量:1
1周华生.余弦函数一个性质的引伸与推广[J].湖南数学通讯,1998(4):16-18.
2刘端森,李超,杨存典.关于余弦函数的一组恒等式[J].商洛师范专科学校学报,2001,15(2):17-19. 被引量:3
3王宝存.自然数高次幂的求和公式的一种推导[J].安徽教育学院学报,2001,19(6):9-9.
4陈晓萌.相似于对角矩阵的方阵高次幂的求法[J].昌潍师专学报,1999,18(2):75-77. 被引量:1
5应制夷.三角学的公理化(英文)[J].数学研究与评论:英文版,1993,13(2):245-247.
6程金凤.公允价值在新会计准则中的应用研究[J].产业与科技论坛,2017,16(17):96-98. 被引量:1
7王法永.油罐烃蒸气回收工艺在南堡油田人工岛上的应用[J].工程建设与设计,2017(18):128-129.
8孙昱辰,秦柳.基于电磁感应加热技术的家用采暖器[J].上海电气技术,2017,10(3):33-36. 被引量:3
9樊海峰.浅析作业成本法在证券公司全成本核算中的应用[J].财会学习,2017,0(17):94-95.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
The evaporation behavior of metal cerium was analyzed and proper evaporation temperature was determined. And then design of the electromagnetic induction evaporation device and research of evapora- tion technology were carried out. Evaporation rate of metal cerium was measured, vapor density distribu- tion was analyzed with film thickness method, and vapor density was measured with weighing method. The results show that evaporation rate of metal cerium at 2 000 ℃ is about 99-135 g/h,and the measured val- ue is slightly lower than the theoretical value. The density distribution of cerium vapor approximately fol- lows the relationship of high order power of cosine function,and atomic vapor density magnitude is about 1011 atom/cm3. The application of electromagnetic induction heating evaporation for cerium film deposition is feasible.
quote
| GB/T 7714-2015 | [1] LUO Li-ping, ZHANG He. Metal Cerium Evaporation by Electromagnetic Induction Heating and Vapor Density Measurement[J]. Rare Metals and Cemented Carbides, 2017(4): 37-41. |
| MLA | [1] LUO Li-ping, and ZHANG He. "Metal Cerium Evaporation by Electromagnetic Induction Heating and Vapor Density Measurement." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 37-41. |
| APA | [1] LUO Li-ping, & ZHANG He. (2017). Metal Cerium Evaporation by Electromagnetic Induction Heating and Vapor Density Measurement. Rare Metals and Cemented Carbides(4), 37-41. |
| IEEE | [1] LUO Li-ping and ZHANG He, "Metal Cerium Evaporation by Electromagnetic Induction Heating and Vapor Density Measurement," Rare Metals and Cemented Carbides, no. 4, pp. 37-41, 2017. keywords: {metal cerium film;electromagnetic induction heating;evaporation;vapor density;vapor density distribution} |