A Supramolecular Platform for the Introduction of Fc-Fusion Bioactive Proteins on Biomaterial Surfaces AITranslate

Eindhoven University of Technology; Eindhoven University of Technology; Eindhoven University of Technology; University of Turku and Åbo Akademi University; Eindhoven University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bioorthogonal chemistry is an excellent method for functionalization of biomaterials with bioactive molecules, as it allows for decoupling of material processing and bioactivation. Here, we report on a modular system created by means of tetrazine/trans-cyclooctene (Tz/TCO) click chemistry undergoing an inverse electron demand Diels–Alder cycloaddition. A reactive supramolecular surface based on ureido-pyrimidinones (UPy) is generated via a UPy-Tz additive, in order to introduce a versatile TCO-protein G conjugate for immobilization of Fc-fusion proteins. As a model bioactive protein, we introduced Fc-Jagged1, a Notch ligand, to induce Notch signaling activity on the material. Interestingly, HEK293 FLN1 cells expressing the Notch1 receptor were repelled by films modified with TCO-protein G but adhered and spread on functionalized electrospun meshes. This indicates that the material processing method influences the biocompatibility of the postmodification. Notch signaling activity was upregulated 5.6-fold with respect to inactive controls on electrospun materials modified with TCO-protein G/Fc-Jagged1. Furthermore, downstream effects of Notch signaling were detected on the gene level in vascular smooth muscle cells expressing the Notch3 receptor. Taken together, our results demonstrate the successful use of a modular supramolecular system for the postprocessing modification of solid materials with functional proteins.

KeyWords AITranslate

supramolecular biomaterial protein G Jagged1 clickchemistry supramolecular additive
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00334

Chinese Library Classification Number:

Citation Information:

Bioorthogonal chemistry is an excellent method for functionalization of biomaterials with bioactive molecules, as it allows for decoupling of material processing and bioactivation. Here, we report on a modular system created by means of tetrazine/trans-cyclooctene (Tz/TCO) click chemistry undergoing an inverse electron demand Diels–Alder cycloaddition. A reactive supramolecular surface based on ureido-pyrimidinones (UPy) is generated via a UPy-Tz additive, in order to introduce a versatile TCO-protein G conjugate for immobilization of Fc-fusion proteins. As a model bioactive protein, we introduced Fc-Jagged1, a Notch ligand, to induce Notch signaling activity on the material. Interestingly, HEK293 FLN1 cells expressing the Notch1 receptor were repelled by films modified with TCO-protein G but adhered and spread on functionalized electrospun meshes. This indicates that the material processing method influences the biocompatibility of the postmodification. Notch signaling activity was upregulated 5.6-fold with respect to inactive controls on electrospun materials modified with TCO-protein G/Fc-Jagged1. Furthermore, downstream effects of Notch signaling were detected on the gene level in vascular smooth muscle cells expressing the Notch3 receptor. Taken together, our results demonstrate the successful use of a modular supramolecular system for the postprocessing modification of solid materials with functional proteins.

quote

GB/T 7714-2015 [1] Matilde Putti, Simone M. J. de Jong, Oscar M. J. A. Stassen, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00334.
MLA [1] Matilde Putti, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00334.
APA [1] Matilde Putti, Simone M. J. de Jong, Oscar M. J. A. Stassen, Cecilia M. Sahlgren, & Patricia Y. W. Dankers. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00334
IEEE [1] Matilde Putti, Simone M. J. de Jong, Oscar M. J. A. Stassen, Cecilia M. Sahlgren, and Patricia Y. W. Dankers, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00334. keywords: {supramolecular biomaterial;protein G;Jagged1;clickchemistry;supramolecular additive}