Solvent-Free Synthesis of a Superamphiphobic Surface by Green Chemistry AITranslate

Gebze Technical University; Canakkale Onsekiz Mart University; Gebze Technical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A superamphiphobic surface having both water and oil repellence was prepared by applying a solvent-free surface coating method using liquid-CO2 in the scope of “green chemistry”. Poly(perfluoroalkyl ethyl acrylate) homopolymer was synthesized by a free radical polymerization in supercritical CO2 medium. This polymer was dissolved in liquid-CO2 containing hydrophilic nanosilica particles in a stirred stainless steel reactor at room temperature under a low CO2 pressure. The polymer/nanosilica dispersion was used to coat glass slides located horizontally in a stainless steel tube by using the “free meniscus coating” method. A series of superamphiphobic coatings were formed under different coating conditions with the variation of polymer/nanosilica concentrations, the types of nanosilica powders, system pressures, and degassing flow rates. The highest apparent water contact angle was 173° and the hexadecane contact angle was 169° on these superamphiphobic hybrid coatings with roll-off angles that were <7°. Such superamphiphobic surfaces have a large potential in biomedical applications for the preservation of small amounts of bioliquids during analysis. In a parallel study, a superhydrophobic surface without containing any nanosilica powder was also obtained by applying the “rapid expansion supercritical solution” method. Polyperfluoroacrylate polymer was dissolved in supercritical CO2 and was sprayed onto glass slides that were previously coated with a polyacrylate adhesive layer. The water contact angles were larger than 170° on this superhydrophobic coating. To optimize the coating conditions, the cloud point pressures of polyperfluoroacrylate polymer in sc-CO2 were determined at various polymer concentrations and temperatures for this purpose.

KeyWords AITranslate

superamphiphobic superhydrophobic free meniscus coating liquidCO2 RESS cloud point
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00322

Chinese Library Classification Number:

Citation Information:

A superamphiphobic surface having both water and oil repellence was prepared by applying a solvent-free surface coating method using liquid-CO2 in the scope of “green chemistry”. Poly(perfluoroalkyl ethyl acrylate) homopolymer was synthesized by a free radical polymerization in supercritical CO2 medium. This polymer was dissolved in liquid-CO2 containing hydrophilic nanosilica particles in a stirred stainless steel reactor at room temperature under a low CO2 pressure. The polymer/nanosilica dispersion was used to coat glass slides located horizontally in a stainless steel tube by using the “free meniscus coating” method. A series of superamphiphobic coatings were formed under different coating conditions with the variation of polymer/nanosilica concentrations, the types of nanosilica powders, system pressures, and degassing flow rates. The highest apparent water contact angle was 173° and the hexadecane contact angle was 169° on these superamphiphobic hybrid coatings with roll-off angles that were <7°. Such superamphiphobic surfaces have a large potential in biomedical applications for the preservation of small amounts of bioliquids during analysis. In a parallel study, a superhydrophobic surface without containing any nanosilica powder was also obtained by applying the “rapid expansion supercritical solution” method. Polyperfluoroacrylate polymer was dissolved in supercritical CO2 and was sprayed onto glass slides that were previously coated with a polyacrylate adhesive layer. The water contact angles were larger than 170° on this superhydrophobic coating. To optimize the coating conditions, the cloud point pressures of polyperfluoroacrylate polymer in sc-CO2 were determined at various polymer concentrations and temperatures for this purpose.

quote

GB/T 7714-2015 [1] Salih Ozbay, Ugur Cengiz, H. Yildirim Erbil. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00322.
MLA [1] Salih Ozbay, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00322.
APA [1] Salih Ozbay, Ugur Cengiz, & H. Yildirim Erbil. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00322
IEEE [1] Salih Ozbay, Ugur Cengiz, and H. Yildirim Erbil, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00322. keywords: {superamphiphobic;superhydrophobic;free meniscus coating;liquidCO2;RESS;cloud point}