Study of Effects of the Rare Earths on the Properties of WC-8Ni Cemented Carbide AITranslate

Department of Applied Physics, Sichuan Union University;Department of Applied Physics, Sichuan Union University;Department of Applied Physics, Sichuan Union University;Department of Applied Physics, Sichuan Union University;Department of Applied Physics, Sichuan Union University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Effects of the addition of the trace rare earth oxides on the physical and mechanical properties of WC-8Ni cemented carbide are studied.By X-ray diffraction, scanning electron microscopy(SEM) as well as transmission electron microscopy,the microstructure of the WC-8Ni alloy containing the rare earths were analysed and distri bution of the rare earths in the alloy,their effects on the texture and structure,and the strengthening mechanism of WC-8Ni alloy were investigated.It has pointel out that the physical and mechanical properties of WC-8Ni with rare earths can come near of up to that of YG8.

KeyWords AITranslate

rare-earth oxide cemented carbide Ni substituting Co pioperty effect.composition texture and structure

1李规华,严兰英,张鸿绪,梁洁,郝庆顺.稀土元素在硬质合金中的分布和存在形态[J].粉末冶金技术,1993,11(2):83-89. 被引量:12

1贾德林,巴爱叶,任云鹏.Ni在WC合成过程中加速效应机理的研究[J].超硬材料工程,2008,20(3):23-26.

2丁华东,马明亮,杨晓华,浩宏奇,金志浩.粉末冶金在探矿工程中的应用[J].探矿工程,1998(1):43-45. 被引量:2

3巴爱叶,孙丹.镍在WC合成中加速效应的机理[J].材料开发与应用,2009,24(5):40-43.

1丁华东,吕涛,傅苏黎,俞建荣,张莉.薄壁金刚石钻头热压弹性石墨模具设计[J].粉末冶金技术,2005,23(5):372-374.

2蔡家品.薄壁金刚石钻头的唇面设计[J].探矿工程,2000(2):46-48. 被引量:6

1孙宝琦,吴国龙,周建华.WC-Co硬质合金中的η相及其对合金性能的影响[J].硬质合金,1999,16(2):92-97. 被引量:8

2黄建忠,李晋尧,王建业.不同的复合粉末状态对W-Ni—Cu重合金显微组织和物理机械性能的影响[J].稀有金属与硬质合金,1989(2):67-7. 被引量:3

3雍志华,汪仕元,程娟,冯钰鑫,张伟,朱俊峰.WC-8(Fe/Ni/Co)R硬质合金的研究[J].稀有金属材料与工程,2000,29(4):273-275. 被引量:1

4韩淑霞.稀土在烧结过程中的行为研究[J].稀土,2011,32(1):54-58. 被引量:4

5谢明,陈力,陈江,宁德魁,曾容川,霍光,符世继.机械合金化CuRECr合金的显微组织结构及性能分析[J].云南冶金,2003,32(3):36-40. 被引量:5

6熊继,羊建高.新型YWR_2稀土硬质合金的使用性能与显微结构[J].稀有金属与硬质合金,1993,21(S1):372-376. 被引量:1

7樊毅,刘先交.MoS_2在铁基摩擦材料中的应用研究[J].湖南冶金,1994,22(1):14-16. 被引量:6

8蔡颖,李松波,李国祥.钢中微量稀土的测定[J].包头钢铁学院学报,2003,22(1):54-58. 被引量:3

9王久彬,袁福延,李超.微量稀土扁钢锭模使用过程中组织性能的变化[J].钢铁研究,1991(2):20-24. 被引量:1

10盛达.喷吹稀土工艺在高炉铁水钢锭模生产中的应用研究通过鉴定[J].稀土信息,1993(2):6-6.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

Effects of the addition of the trace rare earth oxides on the physical and mechanical properties of WC-8Ni cemented carbide are studied.By X-ray diffraction, scanning electron microscopy(SEM) as well as transmission electron microscopy,the microstructure of the WC-8Ni alloy containing the rare earths were analysed and distri bution of the rare earths in the alloy,their effects on the texture and structure,and the strengthening mechanism of WC-8Ni alloy were investigated.It has pointel out that the physical and mechanical properties of WC-8Ni with rare earths can come near of up to that of YG8.

quote

GB/T 7714-2015 [1] YONG Zhi-hua, PAN Qi-fang, WANG Shi-yuan, et al. Study of Effects of the Rare Earths on the Properties of WC-8Ni Cemented Carbide[J]. Rare Metals and Cemented Carbides, 1996(2): 19-26.
MLA [1] YONG Zhi-hua, et al., "Study of Effects of the Rare Earths on the Properties of WC-8Ni Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 1996, pp. 19-26.
APA [1] YONG Zhi-hua, PAN Qi-fang, WANG Shi-yuan, ZHANG Hai-fan, & LI De-you. (1996). Study of Effects of the Rare Earths on the Properties of WC-8Ni Cemented Carbide. Rare Metals and Cemented Carbides(2), 19-26.
IEEE [1] YONG Zhi-hua, PAN Qi-fang, WANG Shi-yuan, ZHANG Hai-fan, and LI De-you, "Study of Effects of the Rare Earths on the Properties of WC-8Ni Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 19-26, 1996. keywords: {rare-earth oxide,cemented carbide, Ni substituting Co,pioperty effect.composition texture and structure}