Development of Thin-wall Diamond Bit AITranslate
Abstract AITranslate
A new type of thin-wall diamond core drill bit is developed through the analysis of drilling feature on the R.C and granite structures.In comparison with the existing manual drilling and electro-hammer drilling, this new bit can easily cut all the building materials such as reinforced concrete and granite,etc with accurate drilling dimension and good surface finish.There will be no damage to the wall,no dust or noise during drilling. The machine can be miniaturized because it needs less drilling power and pressure.
KeyWords AITranslate
1丁华东,冯庆芬,金志浩.薄壁金刚石钻头感应加热机理探讨[J].探矿工程,1995(5):34-35. 被引量:4
2丁华东,冯庆芬,金志浩.降低金刚石钻头烧结温度的方法[J].探矿工程,1995(3):38-39. 被引量:6
3丁华东,林炳.添加铜,镍对W—Ag材料烧结过程和性能的影响[J].湖南冶金,1989(2):14-17. 被引量:2
1丁华东,陈岳军,赵海燕,杨晓华.两种钻孔工具适用范围的比较[J].安装,1997(2):19-19.
2王佳亮,姜荣超.铁路混凝土轨枕硫磺锚固螺栓拔出用金刚石取芯钻头[J].超硬材料工程,2009,21(3):1-4. 被引量:1
1黄杰.轨枕螺栓快速更换成套装置的研制[J].电子世界,2018,0(11):11-13.
1董家辅.制作薄壁金刚石钻头的几个关键问题[J].超硬材料与工程,2000(1):17-18.
2徐新成.冲击电锤离合件温挤压成形[J].热加工工艺,1997,26(2):55-56.
3宋辉.用加工中心加工电锤减速箱和中间盖[J].电动工具,1994(2):12-14.
4王生福,李焰.热压烧结对金刚石性能影响的测试[J].超硬材料与工程,1998(1):12-14.
5孙堃,柯兵,孙立飞,韩晓春,王克勤.精密激光打孔方法模糊优化组合[J].应用激光,1993,13(1):5-7.
6赵红亮,张川,翁康荣,徐忠鑫,金陈跃.RE对电锤用AM60B镁合金曲轴箱件组织和性能的影响[J].郑州大学学报:工学版,2013,34(1):58-61. 被引量:1
7朱丹,潘东杰,沈永华,夏小江.五方向分型自动射芯机的研发[J].铸造,2012,61(12):1422-1424. 被引量:1
8丁华东,金志浩,冯庆芬,张吟秋,张砚祥.添加P降低胎体材料的烧结温度[J].中国有色金属学报,1995,5(3):119-122. 被引量:2
9李焰,王生福.薄壁金刚石钻头在建筑工程中的应用[J].建筑机械化,1999,20(5):47-49.
10张水忠,赵中华.冲钻套筒冷挤压工艺[J].锻压机械,2002,37(2):16-18. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG713.1[金属学及工艺—刀具与模具]
Citation Information:
A new type of thin-wall diamond core drill bit is developed through the analysis of drilling feature on the R.C and granite structures.In comparison with the existing manual drilling and electro-hammer drilling, this new bit can easily cut all the building materials such as reinforced concrete and granite,etc with accurate drilling dimension and good surface finish.There will be no damage to the wall,no dust or noise during drilling. The machine can be miniaturized because it needs less drilling power and pressure.
quote
| GB/T 7714-2015 | [1] DING Hua-dong, HAO Hong-qi, JIN Zhi-hao, et al. Development of Thin-wall Diamond Bit[J]. Rare Metals and Cemented Carbides, 1996(2): 26-29. |
| MLA | [1] DING Hua-dong, et al., "Development of Thin-wall Diamond Bit." Rare Metals and Cemented Carbides, no. 2, 1996, pp. 26-29. |
| APA | [1] DING Hua-dong, HAO Hong-qi, JIN Zhi-hao, & GUO Ping. (1996). Development of Thin-wall Diamond Bit. Rare Metals and Cemented Carbides(2), 26-29. |
| IEEE | [1] DING Hua-dong, HAO Hong-qi, JIN Zhi-hao, and GUO Ping, "Development of Thin-wall Diamond Bit," Rare Metals and Cemented Carbides, no. 2, pp. 26-29, 1996. keywords: {thin-wall diamond bit,core drilling,development,hot pressing} |