Electronic and Optical Properties of Threading Dislocations in n-Type 4H-SiC Electronic and Optical Properties of Threading Dislocations in n-Type 4H-SiC AITranslate

Zhejiang University; Zhejiang University; Zhejiang Sci-Tech University; Zhejiang University; Zhengzhou University; Zhejiang University; Zhejiang University; Zhejiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the decades of development of the single-crystal growth and homoepitaxy of 4H silicon carbide (4H-SiC), high-density threading dislocations (TDs) still remain in 4H-SiC. In this work, we show that the diameters, depths, and inclination angles of molten-alkali etched pits can be employed to discriminate threading edge dislocations (TEDs), threading screw dislocations (TSDs), and threading mixed dislocations (TMDs) in 4H-SiC. The formation of etch pits of TEDs, TSDs, and TMDs during molten-alkali etching is found to be assisted by the dislocation line, dislocation step, and successively dislocation line and step, respectively. By inspecting the surface potentials of n-type 4H-SiC with Kelvin probe force microscopy (KPFM), we show that both TSDs and TEDs behave as donors in n-type 4H-SiC, which gives rise to charge depletion at TDs in n-type 4H-SiC. TDs are found to participate in the broad band D1 luminescence of 4H-SiC, as evidenced by the fact that the microphotoluminescence (micro-PL) intensities at the centers of TDs are stronger than those in dislocation-free regions of 4H-SiC. Understandings gained in this work may help the optimization of n-type 4H-SiC by manipulating the electronic and optical properties of TDs.

KeyWords AITranslate

4HSiC defects dislocations electronic properties optical properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01330

Chinese Library Classification Number:

Citation Information:

Despite the decades of development of the single-crystal growth and homoepitaxy of 4H silicon carbide (4H-SiC), high-density threading dislocations (TDs) still remain in 4H-SiC. In this work, we show that the diameters, depths, and inclination angles of molten-alkali etched pits can be employed to discriminate threading edge dislocations (TEDs), threading screw dislocations (TSDs), and threading mixed dislocations (TMDs) in 4H-SiC. The formation of etch pits of TEDs, TSDs, and TMDs during molten-alkali etching is found to be assisted by the dislocation line, dislocation step, and successively dislocation line and step, respectively. By inspecting the surface potentials of n-type 4H-SiC with Kelvin probe force microscopy (KPFM), we show that both TSDs and TEDs behave as donors in n-type 4H-SiC, which gives rise to charge depletion at TDs in n-type 4H-SiC. TDs are found to participate in the broad band D1 luminescence of 4H-SiC, as evidenced by the fact that the microphotoluminescence (micro-PL) intensities at the centers of TDs are stronger than those in dislocation-free regions of 4H-SiC. Understandings gained in this work may help the optimization of n-type 4H-SiC by manipulating the electronic and optical properties of TDs.

quote

GB/T 7714-2015 [1] Hao Luo, Jiajun Li, Guang Yang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01330.
MLA [1] Hao Luo, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01330.
APA [1] Hao Luo, Jiajun Li, Guang Yang, Ruzhong Zhu, Yiqiang Zhang, Rong Wang, Deren Yang, & Xiaodong Pi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01330
IEEE [1] Hao Luo, Jiajun Li, Guang Yang, Ruzhong Zhu, Yiqiang Zhang, Rong Wang, Deren Yang, and Xiaodong Pi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01330. keywords: {4HSiC defects dislocations electronic properties optical properties}