Unexpected Direct Synthesis of Tunable Redox-Active Benzil-Linked Polymers via the Benzoin Reaction AITranslate
Abstract AITranslate
Strategies for the sustainable synthesis of redox-active organic polymers could lead to next-generation organic electrode materials for electrochemical energy storage, electrocatalysis, and electro-swing chemical separations. Among redox-active moieties, benzils or aromatic 1,2-diones are particularly attractive due to their high theoretical gravimetric capacities and fast charge/discharge rates. Herein, we demonstrate that the cyanide-catalyzed polymerization of simple dialdehyde monomers unexpectedly leads to insoluble redox-active benzil-linked polymers instead of the expected benzoin polymers, as supported by solid-state nuclear magnetic resonance spectroscopy and electrochemical characterization. Mechanistic studies suggest that cyanide-mediated benzoin oxidation occurs by hydride transfer to the solvent and that the insolubility of the benzil-linked polymers protects them from subsequent cyanolysis. The thiophene-based polymer poly(BTDA) is an intriguing organic electrode material that demonstrates two reversible one-electron reductions with monovalent cations such as Li+ and Na+ but one two-electron reduction with divalent Mg2+. As such, the tandem benzoin-oxidation polymerization reported herein represents a sustainable method for the synthesis of highly tunable and redox-active organic materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c02047
Chinese Library Classification Number:
Citation Information:
Strategies for the sustainable synthesis of redox-active organic polymers could lead to next-generation organic electrode materials for electrochemical energy storage, electrocatalysis, and electro-swing chemical separations. Among redox-active moieties, benzils or aromatic 1,2-diones are particularly attractive due to their high theoretical gravimetric capacities and fast charge/discharge rates. Herein, we demonstrate that the cyanide-catalyzed polymerization of simple dialdehyde monomers unexpectedly leads to insoluble redox-active benzil-linked polymers instead of the expected benzoin polymers, as supported by solid-state nuclear magnetic resonance spectroscopy and electrochemical characterization. Mechanistic studies suggest that cyanide-mediated benzoin oxidation occurs by hydride transfer to the solvent and that the insolubility of the benzil-linked polymers protects them from subsequent cyanolysis. The thiophene-based polymer poly(BTDA) is an intriguing organic electrode material that demonstrates two reversible one-electron reductions with monovalent cations such as Li+ and Na+ but one two-electron reduction with divalent Mg2+. As such, the tandem benzoin-oxidation polymerization reported herein represents a sustainable method for the synthesis of highly tunable and redox-active organic materials.
quote
| GB/T 7714-2015 | [1] Christina Cong, Jaehwan Kim, Cara N. Gannett, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02047. |
| MLA | [1] Christina Cong, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02047. |
| APA | [1] Christina Cong, Jaehwan Kim, Cara N. Gannett, Héctor D. Abruña, & Phillip J. Milner. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02047 |
| IEEE | [1] Christina Cong, Jaehwan Kim, Cara N. Gannett, Héctor D. Abruña, and Phillip J. Milner, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02047. keywords: {organic polymers;benzoin reaction;lithiumion batteries (LIBs);redoxactive organic materials;electrocatalysis} |