daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Accelaration Effect of Mechanical Activation on Chemical Reaction in the Light of Fractal Geometry AITranslate

Department of Metallurgical, Central South China University of Technology;Department of Metallurgical, Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In consideration of the fact that mechanical activation affects the surface fractal property of solid, the leaching kinetic equation was rededuced in the light of fractal geometry. This equation shows clearly the increase of surface fractal demention will accelarate the leaching. This effect was distinguished from that of the increase of k value due to mechanical activation and decrease of γ0 due to milling.

KeyWords AITranslate

fractal leaching kinetic mechanical activation

1刘静欣,郭学益,刘旸.废弃电路板多金属粉末碱性熔炼产物分形浸出动力学[J].中国有色金属学报,2015,25(2):545-552. 被引量:10

2王少芬,方正,陈阳国.机械活化在方铅矿发电浸出过程中的应用[J].湿法冶金,2003,22(2):93-96. 被引量:7

1王少芬,方正,王云燕.氯离子对硫化矿发电浸出过程影响的机理研究[J].中国稀土学报,2004(z1):248-250.

2黎铉海,刘伟涛,潘柳萍,粟海锋,黄祖强,潘蓉.机械活化强化从锑渣氧粉中回收铟锑的工艺研究[J].金属矿山,2004(z1):489-492. 被引量:1

3王少芬,方正.硫化矿发电浸出过程的催化和强化研究[J].长沙理工大学学报:自然科学版,2004,1(3):87-91.

4王少芬,方正,王云燕.碳糊电极在硫化矿发电浸出过程中的应用研究[J].电化学,2005,11(1):77-82. 被引量:5

5王少芬,方正,王云燕.超声波在硫化矿发电浸出过程中的应用[J].应用声学,2005,24(4):255-258. 被引量:1

6王少芬,方正.Mechanism of influence of ferric ion on electrogenerative leaching of sulfide minerals with FeCl_3[J].中国有色金属学会会刊:英文版,2006,16(2):473-476. 被引量:2

7王少芬,方正.硫化矿阳极氧化的交流阻抗[J].中南大学学报:自然科学版,2006,37(2):274-279. 被引量:4

8薛真,薛彦辉,王力.拜耳法赤泥中铝铁的盐酸浸出过程研究[J].矿产综合利用,2018(6):139-143. 被引量:8

9胡宇杰,唐朝波,陈永明,唐谟堂,杨声海,杨建广,何静.铅锌混合硫化精矿的低温熔盐还原固硫熔炼[J].中国有色金属学报,2015,25(12):3488-3496. 被引量:10

10谢炜,唐镇宇,符寒光,邹诚茜,匡加才,邓应军.硼在碱解反应过程中的动力学研究[J].材料导报,2016,30(12):158-162.

1陈勤.工程设计问题求解的2+3模型及其分形性质[J].大连理工大学学报,1992,32(1):40-46. 被引量:2

2刘彦霞,鲁玉祥,张亚萍,缪伟民,任云鹏.铝在机械合金化合成TiC过程中的加速效应研究[J].稀有金属,2006,30(z2):9-11.

3李运佩,王兴庆,戴瑞光,林峰.微纳米氧化铁粉低温还原动力学及机理的研究[J].上海金属,2008,30(5):44-47. 被引量:1

4万林生,邓佐国,徐廷华.钠化合物洗提钨及混合洗提中共存反离子的加速效应[J].离子交换与吸附,1996,12(3):259-263.

5何绍刚.喷煤对钒钛磁铁矿高炉冶炼的有利影响[J].四川冶金,2002,24(2):17-19. 被引量:1

6刘小兵.RE对Fe-Mn热锻钢微观组织结构的影响[J].长沙水电师院自然科学学报,1994,9(1):38-43. 被引量:1

7蔡伟琦,应正卫.分形的生成算法在产品造型设计中的研究与应用[J].美术大观,2009(12):216-217.

8李铭.ISO/TS 12033:2001 电子成像——文件图像压缩方法选择导则(下)[J].数字与缩微影像,2005(2):38-39.

9李小兵,刘莹.随机结构粗糙表面的湿润性研究[J].材料导报,2013,27(6):154-156.

10曹汉强,朱光喜,朱耀庭.基于超复数系的分形准全息图象生成[J].中国图象图形学报:A辑,1998,3(8):637-640.

Basic Information:

DOI:

Chinese Library Classification Number:TF121[冶金工程—粉末冶金];TB44[一般工业技术]

Citation Information:

In consideration of the fact that mechanical activation affects the surface fractal property of solid, the leaching kinetic equation was rededuced in the light of fractal geometry. This equation shows clearly the increase of surface fractal demention will accelarate the leaching. This effect was distinguished from that of the increase of k value due to mechanical activation and decrease of γ0 due to milling.

quote

GB/T 7714-2015 [1] ZHAO Zhong-wei, YANG Jia-hong. Accelaration Effect of Mechanical Activation on Chemical Reaction in the Light of Fractal Geometry[J]. Rare Metals and Cemented Carbides, 1998(1): 1-4.
MLA [1] ZHAO Zhong-wei, and YANG Jia-hong. "Accelaration Effect of Mechanical Activation on Chemical Reaction in the Light of Fractal Geometry." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 1-4.
APA [1] ZHAO Zhong-wei, & YANG Jia-hong. (1998). Accelaration Effect of Mechanical Activation on Chemical Reaction in the Light of Fractal Geometry. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] ZHAO Zhong-wei and YANG Jia-hong, "Accelaration Effect of Mechanical Activation on Chemical Reaction in the Light of Fractal Geometry," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 1998. keywords: {fractal;leaching;kinetic mechanical activation}