Influence of Pure Water as Wet Milling Media on Performance of WC-Co Cemented Carbide AITranslate
Abstract AITranslate
WC-Co cemented carbide blend was prepared by addition of antioxidant,pH regulator and defoamer with pure water as the wet milling media to replace conventional reagents,i.e.ethanol,petrol,acetone,hexane and heptane.The properties of prepared WC-Co cemented carbide sample are the same with that of the sample prepared with conventional reagents.Meanwhile,this process has the advantages of high security,low cost and environmental friendliness.
KeyWords AITranslate
1吴达华.??消泡剂和消泡机理(J)油田化学. 1992(01)
2孔祥林,赵以恒.新型除氧剂除氧性能比较[J].吉林电力技术,1998,11(5):17-20. 被引量:3
3景宗梁,吴树新.正辛醇改善浆料涂挂性的试验研究[J].铸造技术,2005,26(2):127-128. 被引量:2
4赵丽梅,王秉臣,何少文.吗啉的生产应用及市场分析[J].化工中间体,2005,1(10):11-14. 被引量:10
5王芸,吴飞,曹治平.消泡剂的研究现状与展望[J].化学工程师,2008,22(9):26-28. 被引量:35
6戴煜.一种以水为介质生产硬质合金或钨钼混合料的新方法[J].稀有金属与硬质合金,2010,38(2):10-10. 被引量:2
1王慧群,彭晖,石丽秋.研磨体形状对亚细晶硬质合金混合料研磨效率及合金性能的影响[J].四川冶金,2019,41(3):37-41.
2吴高潮.研磨体形状对湿磨WC粉末粒度、微观形貌及氧含量的影响[J].硬质合金,2021,38(5):344-350.
1张立,Schubert W.D.,黄伯云.超细硬质合金混合料的制备与制粒技术[J].硬质合金,2003,20(3):129-132. 被引量:12
2张立,陈述,SCHUBERT WD,黄伯云,吴恩熙.纯氧气氛下硬质合金及其原料的热稳定性[J].中南大学学报:自然科学版,2004,35(6):931-934. 被引量:3
3李长岫.用火焰原子吸收光谱法研究球磨过程中带入杂质Fe、Co、Ni的含量变化[J].粉末冶金技术,1993,11(4):295-297.
4张立,陈述,张传福,黄伯云.硬质合金混合料制备新工艺特征分析[J].中国有色金属学报,2005,15(2):236-240. 被引量:9
5潘俊新,邓凯,陈列湘.硬质合金混合料脏化分析[J].硬质合金,1997,14(2):82-86. 被引量:8
6冯建忠,蔡湄夏.太钢4号高炉铁水炉前预脱硅工艺优化[J].炼铁,2004,23(B07):84-86. 被引量:3
7徐伟平,杨会宾.拜耳法种分槽内泡沫对分解率影响的研究[J].铝镁通讯,2007(4):1-2. 被引量:1
8崔佳娜,谌启明.硬质合金混合料的湿磨-喷雾干燥生产工艺及设备[J].稀有金属与硬质合金,2010,38(2):57-61. 被引量:5
9吴向忠.硬质合金混合料制备系统工艺及设备的改进[J].稀有金属与硬质合金,2001,29(1):57-60. 被引量:2
10高培明,尹涛,薛卫.硬质合金类烟机配件的性能改善[J].中国材料科技与设备,2009,6(2):75-77. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金];TF124[冶金工程—粉末冶金]
Citation Information:
WC-Co cemented carbide blend was prepared by addition of antioxidant,pH regulator and defoamer with pure water as the wet milling media to replace conventional reagents,i.e.ethanol,petrol,acetone,hexane and heptane.The properties of prepared WC-Co cemented carbide sample are the same with that of the sample prepared with conventional reagents.Meanwhile,this process has the advantages of high security,low cost and environmental friendliness.
quote
| GB/T 7714-2015 | [1] SU Yi-feng, FU Kun, LI Xing, et al. Influence of Pure Water as Wet Milling Media on Performance of WC-Co Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2015(6): 65-68. |
| MLA | [1] SU Yi-feng, et al., "Influence of Pure Water as Wet Milling Media on Performance of WC-Co Cemented Carbide." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 65-68. |
| APA | [1] SU Yi-feng, FU Kun, LI Xing, SUN Wu-si, & ZHOU Jian-hua. (2015). Influence of Pure Water as Wet Milling Media on Performance of WC-Co Cemented Carbide. Rare Metals and Cemented Carbides(6), 65-68. |
| IEEE | [1] SU Yi-feng, FU Kun, LI Xing, SUN Wu-si, and ZHOU Jian-hua, "Influence of Pure Water as Wet Milling Media on Performance of WC-Co Cemented Carbide," Rare Metals and Cemented Carbides, no. 6, pp. 65-68, 2015. keywords: {WC-Co cemented carbide blend;wet milling media;pure water} |