Piezoresistive and Electrical Properties of a Catecholic Amino Acid–Polyacrylamide Single-Walled Carbon Nanotube Hydrogel Hybrid Network AITranslate
Abstract AITranslate
We have developed a functional hydrogel combining the advantages of single-walled carbon nanotube (SWCNT) hydrogels and 3,4-dihydroxy-l-phenylalanine (l-DOPA) that would be expected to lead to a material with elevated piezoresistive ability. SWCNT hydrogel precursors were thus embedded into the catecholic amino acid 3,4-dihydroxy-l-phenylalanine–polyacrylamide (l-DOPA-PAM) hydrogel to form a l-DOPA-PAM-SWCNT hydrogel hybrid network. This hybrid network as formed was soft but became a hard gel at room temperature. An advantage of this material design is the prevention of overoxidation of l-DOPA to maintain enough free catechol groups to endow the desired properties. Several characterization techniques, including optical microscopy, field-emission scanning electron microscopy, Raman spectroscopy, and dynamic mechanical analysis, were utilized to characterize the l-DOPA-PAM-SWCNT hydrogel hybrid network. The negative piezoresistive effect and electrical properties of the l-DOPA-PAM hydrogel and the l-DOPA-PAM-SWCNT hydrogel hybrid network were measured under different pressures and at different times after the application of pressure started, demonstrating the potential for pressure-sensing applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c00983
Chinese Library Classification Number:
Citation Information:
We have developed a functional hydrogel combining the advantages of single-walled carbon nanotube (SWCNT) hydrogels and 3,4-dihydroxy-l-phenylalanine (l-DOPA) that would be expected to lead to a material with elevated piezoresistive ability. SWCNT hydrogel precursors were thus embedded into the catecholic amino acid 3,4-dihydroxy-l-phenylalanine–polyacrylamide (l-DOPA-PAM) hydrogel to form a l-DOPA-PAM-SWCNT hydrogel hybrid network. This hybrid network as formed was soft but became a hard gel at room temperature. An advantage of this material design is the prevention of overoxidation of l-DOPA to maintain enough free catechol groups to endow the desired properties. Several characterization techniques, including optical microscopy, field-emission scanning electron microscopy, Raman spectroscopy, and dynamic mechanical analysis, were utilized to characterize the l-DOPA-PAM-SWCNT hydrogel hybrid network. The negative piezoresistive effect and electrical properties of the l-DOPA-PAM hydrogel and the l-DOPA-PAM-SWCNT hydrogel hybrid network were measured under different pressures and at different times after the application of pressure started, demonstrating the potential for pressure-sensing applications.
quote
| GB/T 7714-2015 | [1] Hao Zhang, Qiao Yan, Joseph Horvat, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c00983. |
| MLA | [1] Hao Zhang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c00983. |
| APA | [1] Hao Zhang, Qiao Yan, Joseph Horvat, & Roger A. Lewis. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c00983 |
| IEEE | [1] Hao Zhang, Qiao Yan, Joseph Horvat, and Roger A. Lewis, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c00983. keywords: {polyacrylamide;singlewalled carbon nanotube hydrogel;negative piezoresistive effect;electric transport;quantum tunneling;creep;Show More} |