A Conductive Hydrophobic Polyaniline Sandwiched Polyvinylidene Fluoride Membrane for Early Detection of Surfactant-Induced Wetting in Membrane Distillation Using Impedance AITranslate

City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; Technological and Higher Education Institute of Hong Kong (THEi); City University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wetting of hydrophobic membranes is considered to be one of the major limitations that must be overcome to further the development of membrane distillation technology. Low surface tension liquids can induce wetting, which can significantly affect permeate conductivity after the complete wetting of the membrane pores. In this study, a thin conductive hydrophobic polyaniline (PANI) layer was sandwiched between two nonconductive polyvinylidene fluoride (PVDF) layers by the phase inversion method. The surface of this PANI-PVDF membrane was then electrosprayed with polytetrafluoroethylene to impart superhydrophobicity (water contact angle, ∼160°). Finally, the wetting of membranes was monitored and detected during direct contact membrane distillation of a low surface tension saline feed containing sodium dodecyl sulfate by electrochemical impedance spectroscopy. Compared with measuring conductivity of the permeate side, we found that measuring the cross-membrane impedance at a constant frequency (100 kHz) demonstrated more precise detection and a superior ability in distinguishing different stages of wetting and their intrusion. Further, our experiments demonstrated the possible strategies to elude membrane wetting by flushing distilled water periodically.

KeyWords AITranslate

electrochemical impedance spectroscopy (EIS) electrospray hydrophobic polyaniline (PANI) membrane distillation Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c00991

Chinese Library Classification Number:

Citation Information:

Wetting of hydrophobic membranes is considered to be one of the major limitations that must be overcome to further the development of membrane distillation technology. Low surface tension liquids can induce wetting, which can significantly affect permeate conductivity after the complete wetting of the membrane pores. In this study, a thin conductive hydrophobic polyaniline (PANI) layer was sandwiched between two nonconductive polyvinylidene fluoride (PVDF) layers by the phase inversion method. The surface of this PANI-PVDF membrane was then electrosprayed with polytetrafluoroethylene to impart superhydrophobicity (water contact angle, ∼160°). Finally, the wetting of membranes was monitored and detected during direct contact membrane distillation of a low surface tension saline feed containing sodium dodecyl sulfate by electrochemical impedance spectroscopy. Compared with measuring conductivity of the permeate side, we found that measuring the cross-membrane impedance at a constant frequency (100 kHz) demonstrated more precise detection and a superior ability in distinguishing different stages of wetting and their intrusion. Further, our experiments demonstrated the possible strategies to elude membrane wetting by flushing distilled water periodically.

quote

GB/T 7714-2015 [1] Bhaskar Jyoti Deka, Jiaxin Guo, Pak Wai Wong, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c00991.
MLA [1] Bhaskar Jyoti Deka, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c00991.
APA [1] Bhaskar Jyoti Deka, Jiaxin Guo, Pak Wai Wong, Noman Khalid Khanzada, Jehad A. Kharraz, ChiWing Tsang, & Alicia Kyoungjin An. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c00991
IEEE [1] Bhaskar Jyoti Deka, Jiaxin Guo, Pak Wai Wong, Noman Khalid Khanzada, Jehad A. Kharraz, ChiWing Tsang, and Alicia Kyoungjin An, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c00991. keywords: {electrochemical impedance spectroscopy (EIS);electrospray;hydrophobic polyaniline (PANI);membrane distillation;Show More}