daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Atomistic simulations of morphology and spreading behavior of cluster beam deposition AITranslate

National Kaohsiung University of Applied Sciences; National Kaohsiung University of Applied Sciences; National Kaohsiung University of Applied Sciences; National Yunlin University of Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cluster sizes of Co10 (10 atoms of 1 cluster), Co20, and Co30 and Co atoms are deposited to compare the average kinetic energy and surface roughness on a Cu(0 0 1) substrate using molecular dynamics (MD). The incident atoms do not penetrate into the surface of the substrate for an incident energy of 1 eV and a deposition rate of 30 atoms/ps. However, Co30 of the incident atoms penetrate into the surface of the substrate for an incident energy of 1 eV per atom and a deposition rate of 1 cluster/ps. Therefore, the intermixing and the sputtering is embedded in the surface layers of the substrate in the cluster beam deposition process due to high energy and mobility. The surface becomes smoother with increasing deposition rate and/or substrate temperature. For atomic-level stress, a transition from compressive to tensile stress occurs. The average stresses are −0.38 and −0.19 GPa when incident Co10 and Co30 are absorbed, respectively. Therefore, the atoms with tensile stress at the surface layers, and the atoms with compressive stress are mainly distributed at the bottom layers.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.06.035

Chinese Library Classification Number:

Citation Information:

Cluster sizes of Co10 (10 atoms of 1 cluster), Co20, and Co30 and Co atoms are deposited to compare the average kinetic energy and surface roughness on a Cu(0 0 1) substrate using molecular dynamics (MD). The incident atoms do not penetrate into the surface of the substrate for an incident energy of 1 eV and a deposition rate of 30 atoms/ps. However, Co30 of the incident atoms penetrate into the surface of the substrate for an incident energy of 1 eV per atom and a deposition rate of 1 cluster/ps. Therefore, the intermixing and the sputtering is embedded in the surface layers of the substrate in the cluster beam deposition process due to high energy and mobility. The surface becomes smoother with increasing deposition rate and/or substrate temperature. For atomic-level stress, a transition from compressive to tensile stress occurs. The average stresses are −0.38 and −0.19 GPa when incident Co10 and Co30 are absorbed, respectively. Therefore, the atoms with tensile stress at the surface layers, and the atoms with compressive stress are mainly distributed at the bottom layers.

quote

GB/T 7714-2015 [1] ZhengHan Hong, TeHua Fang, ShiangJiun Lin, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.06.035.
MLA [1] ZhengHan Hong, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.06.035.
APA [1] ZhengHan Hong, TeHua Fang, ShiangJiun Lin, & ShunFa Hwang. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.06.035
IEEE [1] ZhengHan Hong, TeHua Fang, ShiangJiun Lin, and ShunFa Hwang, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.06.035.