Study on Oxidation Leaching of Vanadium from Stone Coal with Sodium Persulfate and its Kinetics AITranslate
Abstract AITranslate
In order to explore the mechanism of oxidation leaching of stone coal,the vanadium was leached directly from stone coal vanadium ore by sulfuric acid solution at atmospheric pressure.By adding sodium persulfate in the process of acid leaching,the effects of various conditions on vanadium leaching rate were investigated.The results show that V leaching rate reached 88.9% under the experimental conditions of sodium persulfate 2% ,sulfuric acid 35 %,solid-liquid ratio 1:1,leaching temperature 95℃ and leaching time 11 h.Fitting the V leaching rate-time curves at different reaction temperatures shows that the oxidation leaching process conforms to the shrinking core model and the leaching process is controlled by the chemical reaction on the particle surface.According to Arrhenius equation,the apparent activation energy of the reaction was approximately calculated to be 66.08 kJ ·mol^-1 by using curve fitting method.
KeyWords AITranslate
1杨大锦,廖元双,刘瑜.石煤钒矿提钒新工艺研究[J].云南冶金,2014,43(1):41-44. 被引量:7
2梁泰然,谭立新.复合型助浸剂对钒浸出率的影响[J].材料研究与应用,2016,10(4):255-257. 被引量:5
3华骏,颜文斌,高峰,易静,刘倩倩.湘西石煤湿法提钒中复合添加剂的研究[J].矿冶工程,2016,36(1):72-75. 被引量:6
4陈放,张一敏,黄晶,刘涛,薛楠楠.二氧化锰对石煤提钒直接酸浸的影响[J].化工进展,2017,36(3):1126-1133. 被引量:12
5李莹,颜文斌,华骏,方玉,刘阳文.软锰矿氧化石煤钒矿的湿法浸出研究[J].应用化工,2013,42(7):1170-1173. 被引量:9
6陈明辉,胡详昭,孙际茂,徐军伟,鲍振襄,包觉敏.湖南省寒武系黑色岩系页岩型钒矿概论[J].地质找矿论丛,2012,27(4):410-420. 被引量:18
7陈庆根.石煤钒矿提钒工艺技术的研究进展[J].矿产综合利用,2009(2):30-34. 被引量:35
8李浩然,冯雅丽,罗小兵,王宏杰,杜竹玮.湿法浸出粘土矿中钒的动力学[J].中南大学学报:自然科学版,2008,39(6):1181-1184. 被引量:21
9周宇照,冯雅丽,李浩然,蔡震雷,李辉,程玉龙.石煤与软锰矿焙烧样耦合提取钒锰的动力学[J].中国锰业,2014,32(1):20-25. 被引量:6
10张国范,闫继武,刘琨,龙思思.石煤脱硅渣中钒的浸出动力学[J].有色金属:冶炼部分,2012(6):1-3. 被引量:11
1高峰,华骏,颜文斌,蔡俊,石美莲.石煤清洁焙烧提钒工艺[J].有色金属工程,2020,10(5):44-48. 被引量:7
2华骏,蔡俊,颜文斌,高峰,李丽洁,邹姣.+4价石煤钒矿的制备及其直接浸出动力学[J].化学工程,2020,48(7):68-72. 被引量:2
3李丽洁,石美莲,华骏,颜文斌,高峰,黄超.二氧化锰氧化浸出石煤钒矿动力学研究[J].稀有金属与硬质合金,2020,48(6):24-29. 被引量:2
4孙思涵,潘福生,谢勇冰,曹宏斌,张懿.化学氧化强化湿法冶金清洁生产:进展与展望[J].过程工程学报,2022,22(2):145-161. 被引量:7
5蔡俊,高峰,颜文斌,华骏.浓硫酸熟化浸出提取湘西石煤中的钒[J].稀有金属与硬质合金,2023,51(4):24-27.
1高文选,白书明.湿法冶金工艺赤铁矿法除铁技术原理研究[J].建筑工程与管理,2021,3(3):32-34.
2高崇,王为振,常耀超,黄海辉,李拓夫.HDS渣综合回收利用钒钼的研究[J].有色金属:冶炼部分,2021(7):92-97. 被引量:2
3洪颖,郭双华,李雨,田佳蓉.提钒技术研究进展[J].广州化工,2021,49(17):23-25. 被引量:1
4胡洋,何东升,张琦,张可成,朱志伟.电场强化石煤浸出提钒试验研究[J].金属矿山,2021(9):102-106.
5樊青林.页岩钒选冶工艺技术研究进展[J].中国钼业,2021,45(5):36-40. 被引量:1
6周思雨,兰帅,赖发英,刘凡,秦张杰.钒(V^(3+))与水钠锰矿共沉淀的相互作用及对Pb^(2+)和Zn^(2+)的去除研究[J].江西农业大学学报,2021,43(6):1423-1431.
7曹欢,吴天骄,程倩,宁新霞,赵笑益.硅质钒矿硫酸熟化常温水浸提钒[J].有色金属:冶炼部分,2022(1):67-72.
8赵明辉,成宝海.石煤钒矿浸出过程研究与动力学分析[J].湖南有色金属,2022,38(2):35-37.
9亢选雄,叶国华,朱思琴,梁雪崟.从含钒页岩中提取五氧化二钒的研究进展[J].钢铁钒钛,2022,43(2):25-34. 被引量:4
10张琳,韩晓,李华昌.碱熔-电感耦合等离子体原子发射光谱(ICP-AES)法测定废弃加氢脱硫(HDS)催化剂中的钒[J].中国无机分析化学,2022,12(4):131-135.
1左恒,汪虎.石煤钒矿选矿过程中萃余水回用试验研究[J].中国资源综合利用,2019,37(2):36-39. 被引量:1
2潘荣迪,李建坤,黄崇洋,易轲,张继国.改性单宁的制备及吸附动力学[J].广东化工,2019,46(1):10-11.
3侯安鑫,王增长.德国正式告别石煤开采[J].生态经济,2019,35(3):1-4.
4赵昌明,宁哲,张崇民,蔡永红,王一雍,邵品,李继东.含钛钢渣在熔融NaOH体系中焙烧过程及其反应机理[J].中南大学学报:自然科学版,2018,49(12):2908-2914. 被引量:2
5葛敏.湖北某炭硅质钒矿提钒工艺研究[J].河北地质,2018,0(4):32-37.
6张庆,郝庆兰,赵若竹,豆宝娟,王宇豪,康润宁,宾峰.Cu-Ce-Zr基催化剂上CO自持燃烧及动力学实验研究[J].化学工程,2018,46(11):40-45.
7杨前浩,袁媛,李红艳,章晋武,李广炎,邓泽元.Arrhenius模型模拟蜂蜜黏度-温度-含水量变化规律[J].南昌大学学报:理科版,2018,42(4):364-368. 被引量:2
8董祥宇.硫酸提浓技术在化工生产过程中的应用[J].科技风,2019(8):152-152.
9刘庆,杨军耀,王亚琴,任柳妹.氟在库水与库底沉积物之间的作用过程及机理[J].水电能源科学,2019,37(1):57-60. 被引量:2
10刘会武,黄永,贾秀敏,马嘉,刘忠臣,师留印,杨剑飞,向秋林.氧压酸浸法从铌钛铀矿中选择性提取铀[J].有色金属:冶炼部分,2019(1):48-52.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
In order to explore the mechanism of oxidation leaching of stone coal,the vanadium was leached directly from stone coal vanadium ore by sulfuric acid solution at atmospheric pressure.By adding sodium persulfate in the process of acid leaching,the effects of various conditions on vanadium leaching rate were investigated.The results show that V leaching rate reached 88.9% under the experimental conditions of sodium persulfate 2% ,sulfuric acid 35 %,solid-liquid ratio 1:1,leaching temperature 95℃ and leaching time 11 h.Fitting the V leaching rate-time curves at different reaction temperatures shows that the oxidation leaching process conforms to the shrinking core model and the leaching process is controlled by the chemical reaction on the particle surface.According to Arrhenius equation,the apparent activation energy of the reaction was approximately calculated to be 66.08 kJ ·mol^-1 by using curve fitting method.
quote
| GB/T 7714-2015 | [1] HUA Jun, YAN Wen-bin, GAO Feng, et al. Study on Oxidation Leaching of Vanadium from Stone Coal with Sodium Persulfate and its Kinetics[J]. Rare Metals and Cemented Carbides, 2019(1): 1-5. |
| MLA | [1] HUA Jun, et al., "Study on Oxidation Leaching of Vanadium from Stone Coal with Sodium Persulfate and its Kinetics." Rare Metals and Cemented Carbides, no. 1, 2019, pp. 1-5. |
| APA | [1] HUA Jun, YAN Wen-bin, GAO Feng, & CAI Jun. (2019). Study on Oxidation Leaching of Vanadium from Stone Coal with Sodium Persulfate and its Kinetics. Rare Metals and Cemented Carbides(1), 1-5. |
| IEEE | [1] HUA Jun, YAN Wen-bin, GAO Feng, and CAI Jun, "Study on Oxidation Leaching of Vanadium from Stone Coal with Sodium Persulfate and its Kinetics," Rare Metals and Cemented Carbides, no. 1, pp. 1-5, 2019. keywords: {stone coal;vanadium;sodium persulfate;oxidation leaching;kinetics} |