Determination of Calcium and Magnesium in Potassium Fluotantalate by ICP-AES AITranslate

Jiujiang Nonferrous Metal Smooth Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The content of Ca and Mg in potassium fluotantalate was determined by ICP-AES. After the conditions are determined of analytical spectral lines, detection limit, determination limit, bulk concentration and dissolving acidity,the Ca and Mg recovery of standard addition is 100.58%-102.5% ,and RSD value is 0.74%-10. 02% for the measured Ca and Mg content. The method is reliable, simple and fast to operate with high precision.

KeyWords AITranslate

ICP-AES potassium fluotantalate Ca and Mg content

1何蔓,胡斌,江祖成.用于研究ICP-MS中基体效应的逐级稀释法[J].高等学校化学学报,2004,25(12):2232-2237. 被引量:33

2Akbar Montaser,Golightly D W.电感耦等离子体在原子光谱分析法中的应用[M].北京:人民卫生出版社,1992.

3刘世毅,王静,宋金华,唐德胜.ICP-AES测定镝铁合金中的铁含量[J].稀有金属与硬质合金,2006,34(4):48-49. 被引量:4

4郑国经.ICP-AES分析技术的发展及其在冶金分析中的应用[J].冶金分析,2001,21(1):36-43. 被引量:102

1宋金华,戴和平,廖丹.电感耦合等离子质谱法测定钽粉中杂质[J].稀有金属与硬质合金,2012,40(2):68-71. 被引量:6

2张艳,周耀明,罗岳平,田耘,于磊,朱瑞瑞,林海兰.等离子发射光谱法快速测定自然水体中总硬度研究[J].环境科学与管理,2014,39(5):135-137. 被引量:1

3黄双,吴卓葵.电感耦合等离子体质谱法测定高纯氟钽酸钾中15种痕量杂质元素[J].硬质合金,2019,36(2):166-170. 被引量:1

1周耀明,张艳,罗岳平,田耘,胡华勇.ICP-AES法测定硝酸银中铋、铁、铜、铅含量研究[J].环境科学与管理,2014,39(12):142-144. 被引量:1

2马晓敏,王辉,李波,孙宝莲,梁清华,郑伟,王宽.直流电弧原子发射光谱法测定铌、钽中硅含量[J].理化检验:化学分册,2015,51(6):859-861. 被引量:2

3刘婷,白焕焕,雷小燕,罗策,李剑.电感耦合等离子体质谱法测定高纯五氧化二钽中20种痕量杂质元素[J].理化检验:化学分册,2017,53(4):451-455. 被引量:4

4刘洁,陈忠颖,刘巍,郭颖.电感耦合等离子体质谱法测定高纯铌中20种痕量杂质元素[J].理化检验:化学分册,2018,54(10):1158-1162. 被引量:4

5李甜,陈雄飞,桑永珠,孙海峰,刘英,童坚.电感耦合等离子体原子发射光谱法测定锂硼合金中5种杂质元素[J].化学试剂,2020,42(8):959-963. 被引量:2

6刘婷,罗策,李剑,李震乾,卢凡.电感耦合等离子体质谱法测定核级海绵锆及锆合金中16种痕量杂质元素[J].理化检验:化学分册,2022,58(9):1093-1098.

7黄双.电感耦合等离子体质谱法测定高纯五氧化二铌中25种痕量杂质元素[J].冶金分析,2019,39(3):13-20. 被引量:3

8黄双,吴卓葵.电感耦合等离子体质谱法测定高纯氟钽酸钾中15种痕量杂质元素[J].硬质合金,2019,36(2):166-170. 被引量:1

1宋允嘉.离子交换分离—DSPCF吸光光度法测定氟钽酸钾中痕量铌[J].有色金属分析通讯,1994(2):27-28.

2施平.发射光谱法分析氟钽酸钾中15个元素[J].广东有色金属学报,1994,4(2):148-152. 被引量:3

3张颖.电感耦合等离子体发射光谱法测定氟钽酸钾中十四种杂质元素[J].硬质合金,2002,19(2):107-111. 被引量:4

4伍尊中.氟钽酸钾中铬的测定[J].广东有色金属学报,2005,15(4):24-25.

5刘传雪,赖永玲.氟钽酸钾中碳存在形式的探讨[J].分析试验室,1994,13(2):23-24. 被引量:5

6华锋.氟钽酸钾中杂质的直接光谱测定[J].分析试验室,1990,9(1):67-67. 被引量:4

7吴辛友.阴离子交换分离-氯代磺酚C吸光光度法测定氟钽酸钾中痕量铌[J].理化检验:化学分册,1993,29(2):107-109.

8叶信火,王安邦.氟钽酸钾中氟的除去和微量碳的测定[J].分析试验室,1993,12(6):83-85. 被引量:4

9李小莉,梁岚.在用配位滴定法测钙镁含量过程中如何提高测量精度[J].天津建材,1999(3):14-15.

10王津,李沁,谢湘娜.ICP-AES法测定镁合金中的钐、镝、钬、钆、锑、铋、锡[J].材料研究与应用,2012,6(4):286-290. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:O657.31[理学—分析化学]

Citation Information:

The content of Ca and Mg in potassium fluotantalate was determined by ICP-AES. After the conditions are determined of analytical spectral lines, detection limit, determination limit, bulk concentration and dissolving acidity,the Ca and Mg recovery of standard addition is 100.58%-102.5% ,and RSD value is 0.74%-10. 02% for the measured Ca and Mg content. The method is reliable, simple and fast to operate with high precision.

quote

GB/T 7714-2015 [1] SONG Jin-hua. Determination of Calcium and Magnesium in Potassium Fluotantalate by ICP-AES[J]. Rare Metals and Cemented Carbides, 2012(1): 59-61.
MLA [1] SONG Jin-hua. "Determination of Calcium and Magnesium in Potassium Fluotantalate by ICP-AES." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 59-61.
APA [1] SONG Jin-hua. (2012). Determination of Calcium and Magnesium in Potassium Fluotantalate by ICP-AES. Rare Metals and Cemented Carbides(1), 59-61.
IEEE [1] SONG Jin-hua, "Determination of Calcium and Magnesium in Potassium Fluotantalate by ICP-AES," Rare Metals and Cemented Carbides, no. 1, pp. 59-61, 2012. keywords: {ICP-AES;potassium fluotantalate;Ca and Mg content}