Laser Hardening Surface Treatment Technology and its Present Application AITranslate

Department of Transport and Municipal Engineering, Sichuan Vocational and Technical College;Department of Material Engineering, Sichuan Vocational and Technical College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the characteristics of laser hardening technology, including the processes of laser phase transformation hardening, laser melting hardening and laser impact hardening. And the present application of laser hardening technology is reviewed.

KeyWords AITranslate

laser hardening surface treatment technical characteristic present application

1Tang Yaxin, Zhang Yongkang, Zhang Hong, et al. Laser shock induced stress wave in metal and its prospects of applications[J]. Chinese JournaI of Lasers, 1998, B7 (3) : 269-275.

2应小东,李午申,冯灵芝.激光表面改性技术及国内外发展现状[J].焊接,2003(1):5-8. 被引量:64

3Tang Y X, Zhang Y K, Yu C C. Effect of laser shock processing on the fatigue resistangce of an aluminum alloy[J]. Journal of Engineering Materials and Technology, 2000,122 (1) : 104-107.

4关振中.激光加工工艺手册[M].北京:中国计量出版社,2002.

5Sagaro R,Ceballos J S, Masearell J, et al. Tribological behaviour of line hardening of steel U13A with Nd: YAG laser[J]. Rev Metal Madrid, 1999,35(3) : 166-172.

6Zhang Y K,Zhang X R,Wang X D,et al. Elastic properities modification in aluminum alloy induced by lasershock processing[J]. Material Science and Engineering, 2001, A297(1-2) : 138-143.

7任旭东,张永康,周建忠,冯爱新,鲁金忠.激光冲击处理对Ti6A14V力学性能的影响[J].功能材料,2006,37(11):1781-1783. 被引量:6

8王贵,王建国,周新初,麻永林.轧辊钢激光熔凝处理组织及性能研究[J].金属热处理,2001,26(3):35-37. 被引量:16

9Pantsar H,Kujanphh V. Diode laser beam absorption in laser transformation hardening of low alloy steel[J]. Journel of Laser Applications, 2004,16(3) : 147-152.

10Ouyang Jiahu, Li Xiadong, Pei Yutao. Structure and properties of laser quenched 4Cr13 steel [J]. Chinese Journal of Lasers, 1993, B2(5) : 475-480.

1刘慧林,雷玉霞,贺家健,李晗,林高用.激光熔凝表面强化技术及其数值模拟研究进展[J].兵器材料科学与工程,2013,36(4):86-91. 被引量:1

2王宏立,张伟,申玉军,田永财.激光淬火65Mn钢表面摩擦磨损性能研究[J].应用激光,2015,35(6):652-656. 被引量:10

3符轲,张修庆,续晓霄,吴建峰,李翔,徐金富.45钢激光淬火工艺优化及性能[J].金属热处理,2017,42(1):154-158. 被引量:20

4刘政,沈俊波,张伟,周刘勇,赵海生.45钢激光束扫描数值模拟与组织性能[J].材料热处理学报,2017,38(3):193-202. 被引量:7

5覃敏.激光表面处理技术在重工业领域的研究和应用进展[J].装备制造技术,2017(12):51-53. 被引量:4

6汪少婷,彭文屹,张林伟,陆磊,陆德平,邓晓华.45钢的脉冲爆炸-等离子体表面改性[J].中国表面工程,2018,31(4):88-95. 被引量:4

7张伟,刘政,周刘勇,赵海生.基于正交试验设计的45钢激光表面强化工艺优化[J].润滑与密封,2019,44(2):81-86. 被引量:3

8李昌,于志斌,赵金月,李云飞,韩兴.碟片激光器激光淬火过程数值模拟与试验研究[J].表面技术,2019,48(6):203-211. 被引量:4

9彭文屹,朱峰,汪少婷,张林伟,陆磊,陆德平,邓晓华.T10钢的脉冲爆炸-等离子体表面改性[J].材料保护,2020,53(1):49-54. 被引量:1

10李昌,张大成,陈正威,于志斌,韩兴.激光淬火技术优势及研究现状[J].辽宁科技大学学报,2020,43(2):97-103. 被引量:1

1王梁,胡勇,宋诗英,赖三聘,姚建华.稳态磁场辅助对激光熔凝层表面波纹的抑制作用研究[J].中国激光,2015,42(11):69-77. 被引量:15

2王晓莉,王旭明,牛翰卿,温宝峰,王旭.农机深松铲材料的研究现状及进展[J].农机使用与维修,2017(2):1-5. 被引量:1

3刘富,相珺,张越,马胜男,赵志伟.多道网格扫描激光相变硬化的性能研究[J].热加工工艺,2017,46(22):139-142.

4高慧,吕奎龙.31CrMoV6表面激光淬火工艺及性能研究[J].煤矿机械,2017,38(11):84-87.

5马斌斌,胡立威,刘学,李晋锋,张佳佳,乐国敏,李秀燕.激光功率对Fe-Si-B激光熔覆涂层微观组织与性能的影响[J].材料热处理学报,2018,39(7):113-118. 被引量:6

6陈小明,王海金,周夏凉,赵坚,伏利,刘伟.激光表面改性技术及其研究进展[J].材料导报,2018,32(A01):341-344. 被引量:25

7李赫亮,冯立丽,付文达,刘敬福.功率对激光热处理ZA35合金组织和性能的影响[J].金属热处理,2018,43(7):95-99. 被引量:1

8汪少婷,彭文屹,张林伟,陆磊,陆德平,邓晓华.45钢的脉冲爆炸-等离子体表面改性[J].中国表面工程,2018,31(4):88-95. 被引量:4

9孟亮,李雄,黄永俊,万强,李明震,李善军,张衍林.激光淬火及熔覆技术提高柑橘枝粉碎机65Mn钢锤片耐磨性[J].农业工程学报,2018,34(17):54-60. 被引量:9

10牛锐锋,魏荣祥,杨伦.T10/Q235复合钢板激光表面淬火特性研究[J].应用激光,2018,38(4):618-622. 被引量:1

1专利技术[J].热加工工艺,2007,36(4):81-81.

2李刚,邱玲,邱星武.40Cr激光熔凝硬化组织形态及硬度研究[J].热处理技术与装备,2008,29(3):25-28. 被引量:6

3邱玲,李刚,邱星武.40Cr激光熔凝硬化组织形态及硬度研究[J].材料导报:网络版,2008,3(2):39-41.

4邱玲,李刚,邱星武.40Cr激光熔凝硬化组织形态及性能研究[J].热加工工艺,2008,37(6):34-37. 被引量:5

5李刚,王存山,夏元良,王彦芳,董闯.灰口铸铁的激光表面熔凝硬化[J].金属热处理,2002,27(1):16-18. 被引量:3

6刘书华,葛继平,陈美玲,李桂敏.Fe-C 合金激光熔凝硬化研究[J].大连交通大学学报,1997,0(4):63-66.

7焊接科学和技术的发展及前景[J].机械制造文摘:焊接分册,2003,0(3):1-1.

8段艳丽,何欢,符跃春,王云云.合金激光表面改性的研究进展[J].材料导报:纳米与新材料专辑,2010,24(2):205-207. 被引量:7

9应小东,李午申,冯灵芝.激光表面改性技术及国内外发展现状[J].焊接,2003(1):5-8. 被引量:64

10孔德军,张永康,冯爱新.H13热作模具钢激光表面改性处理技术[J].材料导报,2005,19(8):63-65. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TG156.99[金属学及工艺—热处理]

Citation Information:

Description is made of the characteristics of laser hardening technology, including the processes of laser phase transformation hardening, laser melting hardening and laser impact hardening. And the present application of laser hardening technology is reviewed.

quote

GB/T 7714-2015 [1] LIU Chun-ge, QIU Xing-wu. Laser Hardening Surface Treatment Technology and its Present Application[J]. Rare Metals and Cemented Carbides, 2012(1): 62-64.
MLA [1] LIU Chun-ge, and QIU Xing-wu. "Laser Hardening Surface Treatment Technology and its Present Application." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 62-64.
APA [1] LIU Chun-ge, & QIU Xing-wu. (2012). Laser Hardening Surface Treatment Technology and its Present Application. Rare Metals and Cemented Carbides(1), 62-64.
IEEE [1] LIU Chun-ge and QIU Xing-wu, "Laser Hardening Surface Treatment Technology and its Present Application," Rare Metals and Cemented Carbides, no. 1, pp. 62-64, 2012. keywords: {laser hardening;surface treatment;technical characteristic;present application}