Multidimensionality of the Contact Potential Difference at the Nanoscale in Inorganic Oxides AITranslate

University of Quebec; University of Quebec
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Inorganic-oxide-based sample systems are popular for applications in catalysis, sensing, renewable energy, and fuel cells, in which electronic properties play important roles. Environmental conditions, e.g., temperature, can greatly impact the electronic properties and thereby the performance. The lack of basic knowledge of the local variation of electronic properties as a function of temperature limits the fundamental understanding of systems and hampers their robustness. Here, we present temperature-dependent scanning probe microscopy experiments to reveal the variation of contact potential difference (CPD) across different length scales. Our measurements demonstrate that the CPD of inorganic perovskites (e.g., SrTiO3) and metal-oxide semiconductors (e.g., TiO2) evolves significantly with temperature. We show that CPD variation depends on the locality of the measurement and originates from a thermodynamically driven intrinsic doping state. These results will facilitate a fundamental understanding of the electronic properties of oxides and thus ease emerging technologies, rationalized by engineering temperature-dependent electronic properties.

KeyWords AITranslate

inorganic oxides perovskites metaloxide semiconductors temperaturedependent electronic properties strontium titanate (SrTiO3) titanium dioxide (TiO2) contact potential difference scanning probe microscopy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00713

Chinese Library Classification Number:

Citation Information:

Inorganic-oxide-based sample systems are popular for applications in catalysis, sensing, renewable energy, and fuel cells, in which electronic properties play important roles. Environmental conditions, e.g., temperature, can greatly impact the electronic properties and thereby the performance. The lack of basic knowledge of the local variation of electronic properties as a function of temperature limits the fundamental understanding of systems and hampers their robustness. Here, we present temperature-dependent scanning probe microscopy experiments to reveal the variation of contact potential difference (CPD) across different length scales. Our measurements demonstrate that the CPD of inorganic perovskites (e.g., SrTiO3) and metal-oxide semiconductors (e.g., TiO2) evolves significantly with temperature. We show that CPD variation depends on the locality of the measurement and originates from a thermodynamically driven intrinsic doping state. These results will facilitate a fundamental understanding of the electronic properties of oxides and thus ease emerging technologies, rationalized by engineering temperature-dependent electronic properties.

quote

GB/T 7714-2015 [1] Bugrahan Guner, Omur E. Dagdeviren. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00713.
MLA [1] Bugrahan Guner, and Omur E. Dagdeviren. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00713.
APA [1] Bugrahan Guner, & Omur E. Dagdeviren. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00713
IEEE [1] Bugrahan Guner and Omur E. Dagdeviren, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00713. keywords: {inorganic oxides perovskites metaloxide semiconductors temperaturedependent electronic properties strontium titanate (SrTiO3) titanium dioxide (TiO2) contact potential difference scanning probe microscopy}