daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Accordion-like-Ti3C2 MXene-Based Gas Sensors with Sub-ppm Level Detection of Acetone at Room Temperature Accordion-like-Ti3C2 MXene-Based Gas Sensors with Sub-ppm Level Detection of Acetone at Room Temperature AITranslate

United Arab Emirates University; United Arab Emirates University; United Arab Emirates University; United Arab Emirates University; United Arab Emirates University; United Arab Emirates University; United Arab Emirates University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Compared to traditional-metal oxide-based gas sensors (MOS), the progress of high-performance room-temperature (RT) gas-sensing materials has captivated a lot of interest in recent years. MXenes, two-dimensional (2D) transition-metal carbides/nitrides, have recently been discovered and gained tremendous consideration for gas sensing applications due to their superior chemical and physical properties. Herein, we successfully synthesized accordion-like Ti3C2Tx MXene multilayers by a selective HF-etching method at 60 °C to be used as a chemiresistive sensor for acetone vapor. The fabricated sensor successfully detected acetone vapor at the parts per billion (ppb) level and showed a p-type sensing behavior. The limit of detection (LOD) of acetone vapor was about 250 ppb with a fast response time of 53 s. The sensor exhibited good repeatability, high selectivity toward acetone among other test gases, and excellent stability even after 4 months. The sensing mechanism was proposed in terms of the interaction between the charge carriers of accordion-like Ti3C2Tx, multiple hydrogen bonding between different functional groups on the MXene surface, and acetone vapor species. The prepared sensor also showed high sensitivity toward acetone vapor at RT (23 °C); hence, it lends itself high potential as a breath sensor for diabetic patients.

KeyWords AITranslate

MXene 2D nanomaterials Ti3C2Tx acetone roomtemperature gas sensor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00717

Chinese Library Classification Number:

Citation Information:

Compared to traditional-metal oxide-based gas sensors (MOS), the progress of high-performance room-temperature (RT) gas-sensing materials has captivated a lot of interest in recent years. MXenes, two-dimensional (2D) transition-metal carbides/nitrides, have recently been discovered and gained tremendous consideration for gas sensing applications due to their superior chemical and physical properties. Herein, we successfully synthesized accordion-like Ti3C2Tx MXene multilayers by a selective HF-etching method at 60 °C to be used as a chemiresistive sensor for acetone vapor. The fabricated sensor successfully detected acetone vapor at the parts per billion (ppb) level and showed a p-type sensing behavior. The limit of detection (LOD) of acetone vapor was about 250 ppb with a fast response time of 53 s. The sensor exhibited good repeatability, high selectivity toward acetone among other test gases, and excellent stability even after 4 months. The sensing mechanism was proposed in terms of the interaction between the charge carriers of accordion-like Ti3C2Tx, multiple hydrogen bonding between different functional groups on the MXene surface, and acetone vapor species. The prepared sensor also showed high sensitivity toward acetone vapor at RT (23 °C); hence, it lends itself high potential as a breath sensor for diabetic patients.

quote

GB/T 7714-2015 [1] Sanjit Manohar Majhi, Ashraf Ali, Yaser E. Greish, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00717.
MLA [1] Sanjit Manohar Majhi, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00717.
APA [1] Sanjit Manohar Majhi, Ashraf Ali, Yaser E. Greish, Hesham F. ElMaghraby, Naser N. Qamhieh, Abdul Razack Hajamohideen, & Saleh T. Mahmoud. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00717
IEEE [1] Sanjit Manohar Majhi, Ashraf Ali, Yaser E. Greish, Hesham F. ElMaghraby, Naser N. Qamhieh, Abdul Razack Hajamohideen, and Saleh T. Mahmoud, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00717. keywords: {MXene 2D nanomaterials Ti3C2Tx acetone roomtemperature gas sensor}