daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Uniaxial Alignment of Spin Coated Polymer Films for High-Performance Field Effect Transistors AITranslate

Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University; Beijing Jiaotong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Chain alignment has been a major method for improving the performance of polymer field effect transistors (PFETs). A nanogrooved substrate is a promising media for fabricating high-performance polymer transistors due to its effectiveness. However, the application of nanogrooved substrates in polymer spin coating suffers from the liquid repelling nature of the substrate. This work demonstrates that with the help of an α-chloronaphthalene (α-CN) additive in the chloroform solution, the highly aligned poly[4-(4,4-dihexadecyl-4H-cyclopenta[1,2-b:5,4-b′]-dithiophen-2-yl)-alt-[1,2,5]thiadiazolo-[3,4-c]pyridine] (PCDTPT) polymer films can be fabricated by spin coating onto the nanogrooved substrates. The chloroform matrix ensures the uniform film formation, and the incorporation of α-CN significantly improves the polymer chain orientation. The resulting PCDTPT thin films show an absorbance dichroic ratio as high as 16, which is among the highest ones ever reported. The polymer field effect transistors based on the aligned PCDTPT films show an average mobility of 4.42 cm2 V–1 s–1 (the highest as 5.03 cm2 V–1 s–1), which is about 6 times that of the control devices with a mean mobility of 0.77 cm2 V–1 s–1. Despite the simplicity of this method, the resulting devices show comparable and even better performances than the aligned polymer film-based devices reported in the literature. The uniaxially aligned spin coated polymer film provides a simple but effective approach to fabricating high-performance PFETs.

KeyWords AITranslate

aligned polymers polymer transistors nanogrooves solvent additive spin coating
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01136

Chinese Library Classification Number:

Citation Information:

Chain alignment has been a major method for improving the performance of polymer field effect transistors (PFETs). A nanogrooved substrate is a promising media for fabricating high-performance polymer transistors due to its effectiveness. However, the application of nanogrooved substrates in polymer spin coating suffers from the liquid repelling nature of the substrate. This work demonstrates that with the help of an α-chloronaphthalene (α-CN) additive in the chloroform solution, the highly aligned poly[4-(4,4-dihexadecyl-4H-cyclopenta[1,2-b:5,4-b′]-dithiophen-2-yl)-alt-[1,2,5]thiadiazolo-[3,4-c]pyridine] (PCDTPT) polymer films can be fabricated by spin coating onto the nanogrooved substrates. The chloroform matrix ensures the uniform film formation, and the incorporation of α-CN significantly improves the polymer chain orientation. The resulting PCDTPT thin films show an absorbance dichroic ratio as high as 16, which is among the highest ones ever reported. The polymer field effect transistors based on the aligned PCDTPT films show an average mobility of 4.42 cm2 V–1 s–1 (the highest as 5.03 cm2 V–1 s–1), which is about 6 times that of the control devices with a mean mobility of 0.77 cm2 V–1 s–1. Despite the simplicity of this method, the resulting devices show comparable and even better performances than the aligned polymer film-based devices reported in the literature. The uniaxially aligned spin coated polymer film provides a simple but effective approach to fabricating high-performance PFETs.

quote

GB/T 7714-2015 [1] Jingzan Jiang, Yadan Deng, Jun Sun, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01136.
MLA [1] Jingzan Jiang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01136.
APA [1] Jingzan Jiang, Yadan Deng, Jun Sun, Qiuhong Cui, Zhidong Lou, Yanbing Hou, Yufeng Hu, & Feng Teng. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01136
IEEE [1] Jingzan Jiang, Yadan Deng, Jun Sun, Qiuhong Cui, Zhidong Lou, Yanbing Hou, Yufeng Hu, and Feng Teng, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01136. keywords: {aligned polymers polymer transistors nanogrooves solvent additive spin coating}